Barcelona Test as an Alternative Method to Control and Design Fiber-Reinforced Concrete Pipes

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Barcelona Test as an Alternative Method to Control and Design Fiber-Reinforced Concrete Pipes

Author(s): Renata Monte, Albert de la Fuente, Antonio Domingues de Figueiredo, and Antonio Aguado

Publication: Structural Journal

Volume: 113

Issue: 6

Appears on pages(s): 1175-1184

Keywords: Barcelona test; concrete pipes; cracking; design; fibers; numerical simulation

DOI: 10.14359/51689018

Date: 11/1/2016

Abstract:
The use of fibers as primary reinforcement for concrete pipes (CPs) is known by both industrial and scientific researchers as an attractive alternative to steel. However, the use of fibers in CPs has not yet been well established in this industry because of, among other reasons, the lack of systematic quality control of fiber-reinforced concrete pipes (FRCPs). Therefore, an experimental program involving the production and testing of 600 mm (23.6 in.) internal-diameter FRCPs was performed using low contents of steel (10 and 20 kg/m3 [0.62 and 1.25 lb/ft3]) and polypropylene (2.3 and 4.6 kg/m3 [0.14 and 0.29 lb/ft3]) fibers. These FRCPs were expected to be viable alternatives to those unreinforced and steel bar-reinforced concrete pipes corresponding to low- to moderate-strength classes. A numerical simulation of the tests using the constitutive equation derived from the Barcelona test was carried out, aimed at confirming that both can be an innovative combination to deal with both the characterization of the FRC tensile behavior and the direct design of these pipes. In this regard, those pipes containing 20 kg/m3 (1.25 lb/ft3)of steel fibers reached the C60 strength class in the TEBT (equivalent to ASTM C76 Class I). Consequently, the steel bars could be completely replaced by fibers. This fact led to an effective reduction of 20% of steel as well as to the elimination of those operations related to the reinforcement preparation. Simultaneously, these FRCPs represent a challenge at a numerical level because the model could be insensitive to this low amount of fibers. The comparisons between the experimental and numerical results have confirmed the suitability of both the model and the constitutive equation to simulate the pipe response when subjected to the TEBT.

Related References:

1. Viñolas, B., “Applications and Advances of the MIVES Methodology in Multicriteria Decision Analysis,” PhD thesis, Universitat Politècnica de Catalunya, Barcelona, Spain, 2011, 314 pp.

2. Peyvandi, A.; Soroushian, P.; Balachandra, A. M.; and Sobolev, K., “Enhancement of the Durability Characteristics of Concrete Nanocomposite Pipes with Modified Graphite Nanoplatelets,” Construction and Building Materials, V. 47, 2013, pp. 111-117. doi: 10.1016/j.conbuildmat.2013.05.002

3. Pedersen, C., “New Production Processes, Materials and Calculation Techniques for Fiber Reinforced Concrete Pipes,” PhD thesis, Technical University of Denmark, Lyngby, Denmark, 1996, 128 pp.

4. Haktanir, T.; Ari, K.; Altun, F.; and Karahan, O., “A Comparative Experimental Investigation of Concrete, Reinforced-Concrete and Steel-Fibre Concrete Pipes under Three-Edge-Bearing Test,” Construction and Building Materials, V. 21, No. 8, 2007, pp. 1702-1708. doi: 10.1016/j.conbuildmat.2006.05.031

5. Figueiredo, A., “Evaluation of the Test Method for Crushing Strength of Steel Fiber Reinforced Concrete Pipes,” Proceedings of the 7th International RILEM Symposium on Fiber Reinforced Concrete (BEFIB 2008), Chennai, India, 2008, pp. 989-1000.

6. Abolmaali, A.; Mikhaylova, A.; Wilson, A.; and Lundy, J., “Performance of Steel Fiber-Reinforced Concrete Pipes,” Transportation Research Record: Journal of the Transportation Research Board, V. 2313, No. 1, 2012, pp. 168-177. doi: 10.3141/2313-18

7. de la Fuente, A.; Figueiredo, A. D.; Aguado, A.; Molins, C.; and Chama Neto, P. J., “Experimentation and Numerical Simulation of Steel Fiber Reinforced Concrete Pipes,” Materiales de Construcción, V. 61, No. 302, 2011, pp. 239-256.

8. Figueiredo, A. D.; de la Fuente, A.; Molins, C.; and Aguado, A., “A New Approach on Crushing Strength Test for Fiber Reinforced Concrete Pipes” Proceedings of the 8th RILEM International Symposium on Fiber Reinforced Concrete, Guimarães, Portugal, 2012, 13 pp.

9. Mohamed, N.; Soliman, A.; and Nehdi, M., “Optimum Fiber Content for Precast Steel Fiber Reinforced Concrete Pipes,” FRC 2014 Joint ACI-fib International Workshop: Fiber Reinforced Concrete Applications, Montreal, QC, Canada, 2014, pp. 500-510.

10. Peyvandi, A.; Soroushian, P.; and Jahangirnejad, S., “Enhancement of the Structural Efficiency and Performance of Concrete Pipes through Fiber Reinforcement,” Construction and Building Materials, V. 45, 2013, pp. 36-44. doi: 10.1016/j.conbuildmat.2013.03.084

11. UNE-EN 127916:2008, “Concrete Pipes and Fittings, Unreinforced, Steel Fiber and Reinforced,” National Complement to the Standard UNE-EN 1916:2002, 2008, 2 pp.

12. AS 4139:2003, “Fiber-Reinforced Concrete Pipes and Fittings,” Australian Standards, 2003, 54 pp.

13. EN 1916:2002, “Concrete Pipes and Fittings, Unreinforced, Steel Fiber and Reinforced,” British Standards Institution, London, UK, 2002, 96 pp.

14. ASTM C76-14, “Standard Specification for Reinforced Concrete Culvert, Storm Drain, and Sewer Pipe,” ASTM International, West Conshohocken, PA, 2014, 11 pp.

15. Heger, F. J., “A Theory for the Structural Behavior of Reinforced Concrete Pipes,” PhD thesis, Massachusetts Institute of Technology, Cambridge, MA, 1962, 300 pp.

16. Heger, F. J., “Structural Behavior of Circular Reinforced Concrete Pipe—Development of Theory,” ACI Journal Proceedings, V. 60, No. 11, Nov. 1963, pp. 1567-1614.

17. Peyvandi, A.; Soroushian, P.; and Jahangirnejad, S., “Structural Design Methodologies for Concrete Pipes with Steel and Synthetic Fiber Reinforcement,” ACI Structural Journal, V. 111, No. 1, Jan.-Feb. 2014, pp. 83-91.

18. de la Fuente, A.; Escariz, R. C.; de Figueiredo, A. D.; Molins, C.; and Aguado, A., “A New Design Method for Steel Fiber Reinforced Concrete Pipes,” Construction and Building Materials, V. 30, 2012, pp. 547-555. doi: 10.1016/j.conbuildmat.2011.12.015

19. de la Fuente, A.; Escariz, R. C.; de Figueiredo, A. D.; and Aguado, A., “Design of Macrosynthetic Fiber Reinforced Concrete Pipes,” Construction and Building Materials, V. 43, 2013, pp. 523-532. doi: 10.1016/j.conbuildmat.2013.02.036

20. EN 14651, “Test Method for Metallic Fibered Concrete—Measuring the Flexural Tensile Strength (Limit of Proportionality (LOP), Residual),” European Committee for Standardization, Brussels, Belgium, 2007, 20 pp.

21. RILEM TC 162-TDF, “Test and Design Methods for Steel Fibre Reinforced Concrete. σ-ε Design Method,” Materials and Structures, V. 36, No. 262, 2003, pp. 560-567. doi: 10.1617/14007

22. fib Bulletins 65 and 66, “Model Code 2010 Final Draft,” Fédération Internationale du Béton (fib), Lausanne, Switzerland, 2010, 720 pp.

23. Blanco, A.; Pujadas, P.; de la Fuente, A.; Cavalaro, S.; and Aguado, A., “Application of Constitutive Models in European Codes to RC-FRC,” Construction and Building Materials, V. 40, 2013, pp. 246-259. doi: 10.1016/j.conbuildmat.2012.09.096

24. Molins, C.; Aguado, A.; and Saludes, S., “Double Punch Test to Control the Energy Dissipation in Tension of FRC (Barcelona Test),” Materials and Structures, V. 42, No. 4, 2009, pp. 415-425. doi: 10.1617/s11527-008-9391-9

25. UNE 83515:2010, “Hormigones con fibras. Determinación de la resistencia a fisuración, tenacidad y resistencia residual a tracción. Método Barcelona,” Asociación Española de Normalización y Certificación Madrid, Spain, 2010, 10 pp.

26. Pujadas, P.; Blanco, A.; Cavalaro, S.; de la Fuente, A.; and Aguado, A., “New Analytical Model to Generalize the Barcelona Test Using Axial Displacement,” Journal of Civil Engineering and Management, V. 19, No. 2, 2013, pp. 259-271. doi: 10.3846/13923730.2012.756425

27. Blanco, A.; Pujadas, P.; Cavalaro, S. H. P.; de la Fuente, A.; and Aguado, A., “Constitutive Model for Fiber Reinforced Concrete Based on the Barcelona Test,” Cement and Concrete Composites, V. 53, 2014, pp. 327-340. doi: 10.1016/j.cemconcomp.2014.07.017

28. Pedersen, C., “The Moment-Rotation Relationship with Implementation of Stress-Crack Width Relationships,” Technical University of Denmark, Lyngby, Denmark, 1995, 17 pp.

29. Amorim, D. L. N.; Proença, S. P. B.; and Flórez-López, J., “Simplified Modeling of Cracking in Concrete: Application in Tunnel Linings,” Engineering Structures, V. 70, 2014, pp. 23-35. doi: 10.1016/j.engstruct.2014.03.031

30. de la Fuente, A.; Aguado, A.; Molins, C.; and Armengou, J., “Numerical Model for the Analysis up to Failure of Precast Concrete Sections,” Computers & Structures, V. 106-107, 2012, pp. 105-114. doi: 10.1016/j.compstruc.2012.04.007

31. Barros, J. A. O., and Figueiras, J. A., “Flexural Behavior of SFRC: Testing and Modeling,” Journal of Materials in Civil Engineering, ASCE, V. 11, No. 4, 1999, pp. 331-339. doi: 10.1061/(ASCE)0899-1561(1999)11:4(331)

32. Olesen, J. F., “Fictitious Crack Propagation in Fiber-Reinforced Concrete Beams,” Journal of Engineering Mechanics, ASCE, V. 127, No. 3, 2001, pp. 272-280. doi: 10.1061/(ASCE)0733-9399(2001)127:3(272)

33. Casanova, P., and Rossi, P., “Analysis and Design of Steel Fiber Reinforced Concrete Beams,” ACI Structural Journal, V. 94, No. 5, Sept.-Oct. 1997, pp. 595-602.

34. Pujadas, P.; Blanco, A.; Cavalaro, S. H. P.; de la Fuente, A.; and Aguado, A., “Multidirectional Double Punch Test to Assess the Post-cracking Behavior and Fiber Orientation of FRC,” Construction and Building Materials, V. 58, 2014, pp. 214-224. doi: 10.1016/j.conbuildmat.2014.02.023

35. Pujadas, P.; Blanco, A.; Cavalaro, S. H. P.; de la Fuente, A.; and Aguado, A., “Fiber Distribution in Macro- plastic Fiber Reinforced Concrete Slab—Panels,” Construction and Building Materials, V. 64, 2014, pp. 496-503. doi: 10.1016/j.conbuildmat.2014.04.067

36. Torrents, J.; Blanco, A.; Pujadas, P.; Aguado, A.; Juan-García, P.; and Sánchez-Moragues, M., “Inductive Method for Assessing the Amount and Orientation of Steel Fibers in Concrete,” Materials and Structures, V. 45, No. 10, 2012, pp. 1577-1594. doi: 10.1617/s11527-012-9858-6

37. Cavalaro, S.; López, R.; Torrents, J.; and Aguado, A., “Improved Assessment of Fiber Content and Orientation with Inductive Method in SFRC,” Materials and Structures, V. 48, No. 6, 2015, pp. 1859-1873. doi: 10.1617/s11527-014-0279-6


ALSO AVAILABLE IN:

Electronic Structural Journal