Mixture Proportioning Approach for Low-CO2 Concrete Using Supplementary Cementitious Materials

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Mixture Proportioning Approach for Low-CO2 Concrete Using Supplementary Cementitious Materials

Author(s): Keun-Hyeok Yang, Sung-Ho Tae, and Dong-Uk Choi

Publication: Materials Journal

Volume: 113

Issue: 4

Appears on pages(s): 533-542

Keywords: life-cycle assessment; low-CO2 concrete; mixture proportions; supplementary cementitious materials

DOI: 10.14359/51688992

Date: 7/1/2016

Abstract:
This study developed a simple and rational mixture proportioning procedure for low-CO2 concrete using supplementary cementitious materials (SCMs) such as fly ash (FA), ground-granulated blast-furnace slag (GGBS), and condensed silica fumes (SF). Lifecycle CO2 reduction ratio was critically considered as one of the targeted requirements. The effect of SCMs on CO2 reduction and the compressive strength of concrete was examined by a nonlinear multiple regression analysis using a total of 12,537 datasets, which produced schematized data allowing for the straightforward design of SCMs for satisfying the targeted requirements. Considering the determined substitution level of SCMs for a targeted CO2 reduction ratio, unit binder content and water-binder ratio (W/B) were formulated for the designed compressive strength and entrained air content of concrete. The fine aggregate-to-total aggregate ratio (S/a) was determined from the quadratic formula of a parametrized value for a targeted initial slump of concrete. Overall, the developed procedure is expected to encourage the practical production and application of low-CO2 concrete in the ready mixed concrete field.

Related References:

1. ISO 14040, “Environmental Management—Life-cycle Assessment—Principles and Framework,” International Standardization Organization, Geneva, Switzerland, 2006.

2. IgCC Public Comment Hearing Committee, International Green Construction Code, International Code Council, Washington, DC, 2010.

3. Yang, K. H.; Seo, E. A.; Jung, Y. B.; and Tae, S. H., “Effect of Ground Granulated Blast-Furnace Slag on Life-Cycle Environmental Impact of Concrete,” Journal of the Korea Concrete Institute, V. 26, No. 1, 2013, pp. 13-21. doi: (in Korean)10.4334/JKCI.2014.26.1.013

4. Malhotra, V. M., “Introduction: Sustainable Development and Concrete Technology,” Concrete International, V. 24, No. 7, July 2002, 22 pp.

5. Yang, K. H.; Song, J. K.; and Song, K. I., “Assessment of CO2 Reduction of Alkali-Activated Concrete,” Journal of Cleaner Production, V. 39, No. 1, 2013, pp. 265-272. doi: 10.1016/j.jclepro.2012.08.001

6. Yang, K. H.; Jung, Y. B.; Cho, M. S.; and Tae, S. H., “Effect of Supplementary Cementitious Materials on Reduction of CO2 Emissions from Concrete,” Journal of Cleaner Production, V. 103, 2015, pp. 774-783. doi: 10.1016/j.jclepro.2014.03.018

7. ACI Committee 226, “Use of Fly Ash in Concrete (ACI 226.3R-87),” American Concrete Institute, Farmington Hills, MI, 1987, 29 pp.

8. Malhotra, V. M., and Mehta, P. K., Pozzolanic and Cementitious Materials, Gordon and Breach Publishers, Amsterdam, the Netherlands, 1996, 191 pp.

9. ISO 13315-2, “Environmental Management for Concrete and Concrete Structures—Part 2: System Boundary and Inventory Data,” International Organization for Standardization, Geneva, Switzerland, 2014.

10. Korea LCI Database Information Network. http://www.edp.or.kr/lci., Oct. 2015.

11. Damineli, B. L.; Kemeid, F. M.; Aguiar, P. S.; and John, V. M., “Measuring the Eco-Efficiency of Cement Use,” Cement and Concrete Composites, V. 32, No. 8, 2010, pp. 555-562. doi: 10.1016/j.cemconcomp.2010.07.009

12. Neville, A. M., Properties of Concrete, Addison Wesley Longman, Edingurgh, UK, 1995, 844 pp.

13. AIJ, “Standard Specification and Commentary for Building Construction JASS 5: Reinforced Concrete Work,” Architectural Institute of Japan, Tokyo, Japan, 2003. (in Japanese)

14. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-08) and Commentary,” American Concrete Institute, Farmington Hills, MI, 2008, 473 pp.


ALSO AVAILABLE IN:

Electronic Materials Journal