Use of Damage Rating Index to Quantify Alkali-Silica Reaction Damage in Concrete: Fine versus Coarse Aggregate

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Use of Damage Rating Index to Quantify Alkali-Silica Reaction Damage in Concrete: Fine versus Coarse Aggregate

Author(s): L. F. M. Sanchez, B. Fournier, M. Jolin, M. A. B. Bedoya, J. Bastien, and J. Duchesne

Publication: Materials Journal

Volume: 113

Issue: 4

Appears on pages(s): 395-407

Keywords: alkali-aggregate reaction; crack detection; Damage Rating Index; degradation; durability; expansion

DOI: 10.14359/51688983

Date: 7/1/2016

Abstract:
The Damage Rating Index (DRI), a microscopic and semi-quantitative petrographic tool, is a method that has increasingly been used in North America and Europe because it can answer questions regarding the nature and the degree of damage in concrete affected by deleterious mechanisms such as alkali-aggregate reaction (AAR). This paper presents the results of the condition assessment, using the DRI, of concrete mixtures of different strengths and incorporating different reactive aggregate types (fine versus coarse aggregate) with the aim of verifying both how alkali-silica reaction (ASR) develops against its expansion levels and how the DRI could be used to better quantify damage in concrete due to ASR.

Related References:

1. Fournier, B., and Bérubé, A., “Alkali-Aggregate Reaction in Concrete: A Review of Basic Concepts and Engineering Implications,” Canadian Journal of Civil Engineering, V. 27, No. 2, 2000, pp. 167-191. doi: 10.1139/l99-072

2. Villeneuve, V.; Fournier, B.; and Duchesne, J., “Determination of the Damage in Concrete Affected by ASR—The Damage Rating Index (DRI),” 14th International Conference on Alkali-Aggregate Reaction (ICAAR), Austin, TX, May 2012, 100 pp.

3. Dunbar, P. A., and Grattan-Bellew, P. E., “Results of Damage Rating Evaluation of Condition of Concrete from a Number of Structures Affected by ASR,” CANMET/ACI International Workshop on Alkali-Aggregate Reactions in Concrete, Dartmouth, NS, Canada, Oct. 1995, pp. 257-266.

4. Grattan-Bellew, P. E., and Mitchell, L. D., “Quantitative Petrographic Analysis of Concrete—The Damage Rating Index (DRI) Method, A Review,” Proceedings of the Marc-André Bérubé Symposium on AAR in Concrete, CANMET/ACI Advances in Concrete Technology Seminar, Montréal, QC, Canada, 2006, pp. 321-334.

5. Shrimer, F. H., “Application and Use of Damage Rating Index in Assessment of AAR-Affected Concrete-Selected Case Studies,” 11th International Conference on Alkali-Aggregate Reaction (ICAAR), Québec, QC, Canada, June 2000, pp. 899-907.

6. Rivard, P.; Fournier, B.; and Ballivy, G., “The DRI Method for ASR Affected Concrete—A Critical Review of Petrographic Features of Deterioration and Evaluation Criteria,” Cement, Concrete and Aggregates, V. 24, No. 2, 2002, pp. 1-10.

7. Rivard, P., and Ballivy, G., “Assessment of the Expansion Related to Alkali-Silica Reaction by the Damage Rating Index Method,” Construction and Building Materials, V. 19, No. 2, 2005, pp. 83-90. doi: 10.1016/j.conbuildmat.2004.06.001

8. Bérubé, M.-A.; Smaoui, N.; Fournier, B.; Bissonnette, B.; and Durand, B., “Evaluation of the Expansion Attained to Date by Concrete Affected by Alkali-Silica Reaction. Part III: Application to Existing Structures,” Canadian Journal of Civil Engineering, V. 32, 2005, pp. 463-479. doi: 10.1139/l04-104

9. Shrimer, F. H., “Development of the Damage Rating Index Method as a Tool in the Assessment of Alkali-Aggregate Reaction in Concrete: A Critical Review,” Proceedings of the Marc-André Bérubé Symposium on AAR in Concrete, CANMET/ACI Advances in Concrete Technology Seminar, Montréal, QC, Canada, 2006, pp. 391-411.

10. Powers, L., and Shrimer, F. H., “Quantification of ASR in Concrete: An Introduction to the Damage Rating Index,” ICMA Conference: International Cement Microscopy Association/Society of Concrete Petrographers Joint Meeting, Quebec City, QC, Canada, 2009, 9 pp.

11. Blight, G. E.; McIver, J. R.; Schutte, W. K.; and Rimmer, R., “The Effects of Alkali-Aggregate Reaction on Reinforced Concrete Structures made with Witwatersrand Quartzite Aggregate,” 5th International Conference on AAR in Concrete (ICAAR), Cape Town, South Africa, 1981.

12. Sims, I.; Hunt, B.; and Miglio, B., “Quantifying Microscopical Examinations of Concrete for AAR and Other Durability Aspects,” Durability of Concrete, G. M. Idorn International Symposium, SP-131, J. Holm and M. Geiker, eds., American Concrete Institute, Farmington Hills, MI, 1992, pp. 267-287. doi: 10.14359/1213

13. Salomon, M., and Panetier, J. L., “Quantification du degré d’avancement de l’alcali-réaction dans les bétons et de la néofissuration associée,” 3rd CANMET/ACI International Conference on Durability of Concrete,” Nice, France, 1994, pp. 383-401.

14. Rivard, P.; Fournier, B.; and Ballivy, G., “Quantitative Petrographic Technique for Concrete Damage due to ASR: Experimental and Application,” Cement, Concrete and Aggregates, V. 22, No. 1, 2000, pp. 63-72. doi: 10.1520/CCA10465J

15. Broekmans, M. A. T. M., “The Alkali-Silica Reaction: Mineralogical and Geochemical Aspects of Some Dutch Concretes and Norwegian Mylonites,” PhD thesis, Utrecht University, Utrecht, the Netherlands, 2002, 144 pp.

16. Lindgård, J.; Skjolsvold, O.; Haugen, M.; Hagelia, P.; and Wigum, B. J., “Experience from Evaluation of Degree of Damage in Fluorescent Impregnated Plan Polished Sections of Half-Cores Based on the ‘Crack Index Method’,” 12th International Conference on AAR in Concrete, Beijing, China, 2004, pp. 939-947.

17. British Cement Association, “The Diagnosis of Alkali Silica Reaction—Report of a Working Party,” UK, 1992, 44 pp.

18. St. John, D. A.; Poole, A. W.; and Sims, I., Concrete Petrography: A Handbook of Investigative Techniques, Taylor & Francis, London, UK, 1998, 488 pp.

19. Reinhardt, H. W., and Mielich, O., “A Fracture Mechanics Approach to the Crack Formation in Alkali Sensitive Grains,” Cement and Concrete Research, V. 41, No. 3, 2011, pp. 255-262. doi: 10.1016/j.cemconres.2010.11.008

20. Wood, G. M.; Norris, P.; and Leek, D., “Physical Behavior of AAR Damaged Concrete in Structures and in Test Conditions,” 8th ICAAR—International Conference on Alkali-Aggregate Reaction in Concrete, Kyoto, Japan, 1989, pp. 765-770.

21. Wood, G. M., and Johnson, R. A., “An Engineer’s Perspective on UK. Experience with Alkali-Aggregate Reaction,” 8th ICAAR—International Conference on Alkali-Aggregate Reaction in Concrete, Kyoto, Japan, 1989, pp. 785-790.

22. Smaoui, N.; Bérubé, M. A.; Fournier, B.; Bissonnette, B.; and Durand, B., “Evaluation of the Expansion Attained to Date by Concrete Affected by Alkali-Silica Reaction—Part I: Experimental Study,” Canadian Journal of Civil Engineering, V. 31, 2004, pp. 826-845. doi: 10.1139/l04-051

23. Walker, H. N.; Lane, D. S.; and Stutzman, P. E., Petrographic Methods of Examining Hardened Concrete: A Petrographic Manual, FHWA-HRT-04-150, Federal Highway Administration, McLean, VA, 2006, 333 pp.

24. Fournier, B.; Tremblay, S.; and Frenette, J., “Results of the Petrographic and Stiffness Damage Testing of Concrete Cores from the Princess Margaret Bridge, Fredericton, NB, Canada, Report Submitted to GEMTEC-Consulting Engineers and Scientists,” Apr. 2009, 71 pp.

25. Grattan-Bellew, P. E., and Danay, A., “Comparison of Laboratory and Field Evaluation of AAR in Large Dams,” Proceedings of the International Conference on Concrete AAR in Hydroelectric Plants and Dams, Fredericton, NB, Canada, 1992, 23 pp.

26. Thomas, M. D. A.; Folliard, K. J.; Fournier, B.; Rivard, P.; and Drimalas, T., “Methods for Evaluating and Treating ASR-Affected Structures: Results of Field Application and Demonstration Projects—Volume II: Details of Field Applications and Analysis,” FHWA-HIF-14-003, Federal Highway Administration, U.S. Department of Transportation, Washington, DC, Nov. 2013, 342 pp.

27. Bérubé, M. A.; Fournier, B.; and Côté, T., “Using the Damage Rating Index for Assessing the Expansion of Concrete Affected by Freeze-Thaw, Sulphate attack, or ASR,” 14th ICAAR—International Conference on Alkali-Aggregate Reaction in Concrete, TX, 2012, 10 pp.

28. Lindgard, J., “Alkali-Silica Reaction (ASR)—Performance Testing,” PhD thesis, Norwegian University of Science and Technology, Trondheim, Norway, 2013, 271 pp.

29. Fournier, B.; Bérubé, M. A.; Folliard, K. J.; and Thomas, M. D. A., “Report on the Diagnosis, Prognosis and Mitigation of ASR in Transportation Structures,” FHWA-HIF-09-004, Federal Highway Administration, McLean, VA, 2010, 147 pp.

30. ASTM C1074-11, “Standard Practice for Estimating Concrete Strength by the Maturity Method,” ASTM International, West Conshohocken, PA, 2011, 10 pp.

31. Sanchez, L. F. M.; Fournier, B.; Jolin, M.; and Duchesne, J., “Reliable Quantification of AAR Damage through Assessment of the Damage Rating Index (DRI),” Cement and Concrete Research, V. 67, 2015, pp. 74-92. doi: 10.1016/j.cemconres.2014.08.002

32. Alexander, M., and Mindess, S., Aggregates in Concrete, Taylor & Francis, London, UK, 2005, 448 pp.

33. Sanchez, L. F. M.; Fournier, B.; Jolin, M.; and Bastien, J., “Evaluation of the Stiffness Damage Test (SDT) as a Tool for Assessing Damage in Concrete due to Alkali-Silica Reaction (ASR): Input Parameters and Variability of the Test Responses,” Construction and Building Materials, V. 77, 2015, pp. 20-32. doi: 10.1016/j.conbuildmat.2014.11.071


ALSO AVAILABLE IN:

Electronic Materials Journal