Effect of Temperature on Chloride Diffusion in Saturated Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Temperature on Chloride Diffusion in Saturated Concrete

Author(s): B. Touil, F. Ghomari, A. Bezzar, A. Khelidj, and S. Bonnet

Publication: Materials Journal

Volume: 114

Issue: 5

Appears on pages(s): 713-721

Keywords: activation energy; coefficient of migration of chlorides; pozzolan; temperature

DOI: 10.14359/51688929

Date: 9/1/2017

Abstract:
The degradation of reinforced concrete (RC) structures exposed to marine environments is largely due to the transfer of chloride ions through the material. The prediction of the penetration of these ions in the concrete by the diffusion coefficient is a fundamental indicator for the characterization of its durability. Tests simulating chloride diffusion in saturated areas are developed at a constant temperature; however, in reality, the temperature fluctuates with the seasons and diurnal variations. To simulate the coupled temperature diffusion of chloride in RC structures in permanent contact with the Mediterranean Sea, an experimental program was developed in the laboratory to assess the migration coefficients of a pozzolanic concrete (CPZ10) and compared to ordinary concrete (OC). The tests of migration are made under an electric field, at different temperatures, from 5 to 50°C (41 to 122°F). Also, a study of the activation energy was made and compared with the Arrhenius theory. The test results showed that the migration coefficient of concrete increases with increasing temperature. The activation energy values of natural pozzolan incorporated concretes were lower than OC.

Related References:

1. Verbeck, G. J., “Mechanisms of Corrosion in Concrete,” Corrosion of Metals in Concrete, SP-49, American Concrete Institute, Farmington Hills, MI, 1975, pp. 21-38.

2. Hassain, S. E., “Al-Gahtani, A. S.; and Rasheeduzzafar, “Chloride Threshold for Corrosion of Reinforcement in Concrete,” ACI Materials Journal, V. 93, No. 6, Nov.-Dec. 1996, pp. 534-538.

3. Kondraivendhan, B., and Bhattacharjee, B., “Effect of Age and Water-Cement Ratio on Size and Dispersion of Pores in Ordinary Portland Cement Paste,” ACI Materials Journal, V. 107, No. 2, Mar.-Apr. 2010, pp. 147-154.

4. Ellis Jr., W. E.; Rigg, E. H.; and Butler, W. B., “Comparative Results of Utilization of Fly Ash, Silica Fume and GGBFS in Reducing the Chloride Permeability of Concrete,” Durability of Concrete, SP-126, V. M. Malhotra, ed., American Concrete Institute, Farmington Hills, MI, 1991, pp. 443-458.

5. Mehta, P. K., “Role of Pozzolanic and Cementitious Material in Sustainable Development of Concrete Industry,” Sixth CANMET/ACI/JCI International Conference: Fly Ash, Silica Fume, Slag & Natural Pozzolans in Concrete, SP-178, V. M. Malhotra, ed., American Concrete Institute, Farmington Hills, MI, 1998, pp. 1-20.

6. Collepardi, S.; Corinaldesi, V.; Moriconi, G.; Bonora, G.; and Collepardi, M., “Durability of High-Performance Concretes with Pozzolanic and Composite Cements,” 2000 CANMET/ACI Conference on Durability, SP-192, American Concrete Institute, Farmington Hills, MI, 2000, pp. 152-172.

7. Das, B. B., and Kondraivendhan, B., “Implication of Pore Size Distribution Parameters on Compressive Strength, Permeability and Hydraulic Diffusivity of Concrete,” Construction and Building Materials, V. 28, No. 1, 2012, pp. 382-386.

8. Hu, Y. J., and Du, Y. L., “Effect of Pore Structure on the Chloride Permeability of Concrete with Mineral Admixture,” Advanced Materials Research, V. 690-693, 2013, pp. 835-838.

9. Dhir, R. K.; Jones, M. R.; and Elghaly, A. E., “PFA Concrete: Exposure Temperature Effects on Chloride Diffusion,” Cement and Concrete Research, V. 23, No. 5, 1993, pp. 1105-1114.

10. Dousti, A.; Rashetnia, R.; Ahmadi, B.; and Shekarchi, M., “Influence of Exposure Temperature on Chloride Diffusion in Concretes Incorporating Silica Fume or Natural Zeolite,” Construction and Building Materials, V. 49, 2013, pp. 393-399.

11. Yuan, Q., and Santhanam, M., “Performance of Cement-Based Materials in Aggressive Aqueous Environments,” State-of-the-Art Report RILEM TC211-PAE, V. 10, Springer Netherlands, Dordrecht, the Netherlands, 2013, pp. 319-343.

12. Alfarabi, S.; Loughlin, K. F.; Azad, A. K.; and Navaz, C. M., “Determination of the Effective Chloride Diffusion Coefficient in Concrete via a Gas Diffusion Technique,” ACI Materials Journal, V. 94, No. 3, May-June 1997, pp. 227-233.

13. Castellote, M.; Andrade, C.; and Alonso, C., “Measurement of the Steady and Nonsteady State Chloride Diffusion Coefficients in a Migration Test by Means of Monitoring the Conductivity in the Anolyte Chamber—Comparison with Natural Diffusion Tests,” Cement and Concrete Research, V. 31, No. 10, 2001, pp. 1411-1420.

14. Stephen, L. D.; Detwiler, R. J.; and Hooton, R. D., “Testing Transport Properties of Concrete,” Concrete International, V. 32, No. 11, Nov. 2010, pp. 33-38.

15. ASTM C1202-05, “Standard Test Method for Electrical Indication of Chloride’s Ability to Resist Chloride,” ASTM International, West Conshohocken, PA, 2005, 6 pp.

16. ASTM C1556, “Standard Test Method for Determining the Apparent Chloride Diffusion Coefficient of Cementitious Mixtures by Bulk Diffusion,” ASTM International, West Conshohocken, PA, 2011, 7 pp.

17. Maage, M.; Helland, S.; Poulsen, E.; Vennesland, Ø.; and Carlsen, J. E., “Service Life Prediction of Existing Concrete Structures Exposed to Marine Environment,” ACI Materials Journal, V. 93, No. 6, Nov.-Dec. 1996, pp. 602-608.

18. Luciano, J., and Miltenberger, M., “Predicting Chloride Diffusion Coefficients from Concrete Mixture Proportions,” ACI Materials Journal, V. 96, No. 6, Nov.-Dec. 1999, pp. 698-702.

19. Thomas, M. D. A., and Bentz, E. C., “Life-365: Computer Program for Predicting the Service Life and Life-Cycle Costs of Reinforced Concrete Exposed to Chlorides,” University of Toronto, Toronto, ON, Canada, 2000, 5 pp.

20. Andrade, C., “Calculation of Chloride Diffusion Coefficient in Concrete from Ionique Diffusion Measurements,” Cement and Concrete Research, V. 23, No. 3, 1993, pp. 724-742.

21. Truc, O., “A New Way for Determining the Chloride Diffusion Coefficient in Concrete from Steady State Diffusion Test,” Cement and Concrete Research, V. 30, No. 2, 2000, pp. 217-226.

22. Luping, T., and Nilsson, L., “A Rapid Determination of Chloride Diffusivity in Concrete by Applying an Electrical Field,” ACI Materials Journal, V. 89, No. 1, Jan.-Feb. 1992, pp. 49-53.

23. Tong, L., and Gjørv, O. E., “Chloride Diffusivity Based on Migration Testing,” Cement and Concrete Research, V. 31, No. 7, 2001, pp. 973-982.

24. Detwiler, R. J.; Kjellsen, K. O.; and Gjørv, O. E., “Resistance to Chloride Intrusion of Concrete Cured at Different Temperatures,” ACI Materials Journal, V. 88, No. 1, Jan.-Feb. 1991, pp. 19-24.

25. Al-Khaja, W. A., “Influence of Temperature, Cement Type and Level of Concrete Consolidation on Chloride Ingress in Conventional and High-Strength Concretes,” Construction and Building Materials, V. 11, No. 1, 1997, pp. 9-13.

26. Yuan, Q.; Shi, C.; de Schutter, G.; and Audenaert, K., “Effect of Temperature on Transport of Chloride Ions in Concrete,” 2nd International Conference on Concrete Repair, Rehabilitation and Retrofitting, M. G. Alexander, H. D. Beushausen, F. Dehn, and P. Moyo, eds., Cape Town, South Africa, Nov. 24-26, 2008, pp. 345-351.

27. Panesar, D. K., and Chidiac, S. E., “Effect of Cold Temperature on the Chloride-Binding Capacity of Cement,” Journal of Cold Regions Engineering, V. 25, No. 4, 2011, pp. 133-144.

28. Collepardi, M.; Marcialis, A.; and Turriziani, R., “Penetration of Chloride Ions into Cement Pastes and Concretes,” Journal of the American Ceramic Society, V. 55, No. 5, 1972, pp. 534-535.

29. Goto, S., and Roy, D. M., “Diffusion of Ions through Hardened Cement Pastes,” Cement and Concrete Research, V. 11, No. 5-6, 1981, pp. 751-757.

30. Page, C. L.; Short, N. R.; and Tarras, A. E. I., “Diffusion of Chloride Ions in Hardened Cement Pastes,” Cement and Concrete Research, V. 11, No. 3, 1981, pp. 395-406.

31. Nguyen, T. S.; Lorente, S.; and Carcasses, M., “Effect of the Environment Temperature on the Chloride Diffusion through CEM-I and CEM-V Mortars: An Experimental Study,” Construction and Building Materials, V. 32, No. 2, 2009, pp. 795-803.

32. Samson, E., and Marchand, J., “Modeling the Effect of Temperature on Ionic Transport in Cementitious Materials,” Cement and Concrete Research, V. 37, No. 3, 2007, pp. 455-468.

33. Yang, C. C., and Weng, S. H., “Effect of 95°C Temperature on the Chloride-Migration of Concrete Using Electrical Field,” Materials Chemistry and Physics, V. 125, No. 3, 2011, pp. 876-882.

34. Otsuki, N.; Madlangbayan, M. S.; Nishida, T.; Saito, T.; and Baccay, M. A., “Temperature Dependency of Chloride Induced Corrosion in Concrete,” Journal of Advanced Concrete Technology, V. 7, No. 1, 2009, pp. 41-50.

35. fib, “Model Code for Service Life Design,” fib Bulletin 34, International Federation for Structural Concrete, Lausanne, Switzerland, 2006, 116 pp.

36. NA 442, “Cement: Composition, Specifications and Conformity Criteria for Common Cements,” Algerian Standard, Algeria, 2005, 21 pp.

37. ACI Committee 232, “Use of Raw or Processed Natural Pozzolans in Concrete (ACI 232.1R-00),” American Concrete Institute, Farmington Hills, MI, 2000, 24 pp.

38. ASTM C618-12a, “Standard Specification for Coal Fly Ash and Raw or Calcined Natural Pozzolan for Use in Concrete,” ASTM International, West Conshohocken, PA, 2012, 5 pp.

39. EN 197-1:2000, “Cement. Composition, Specifications and Conformity Criteria for Common Cements,” European Committee for Standarization, Brussels, Belgium, 2000, 52 pp.

40. ASTM C595-03, “Standard Specification for Blended Hydraulic Cements,” ASTM International, West Conshohocken, PA, 2003, 7 pp.

41. Kaid, N.; Cyr, M.; Julien, S.; and Khelafi, H., “Durability of Concrete Containing a Natural Pozzolan as Defined by a Performance-Based Approach,” Construction and Building Materials, V. 23, No. 12, 2009, pp. 3457-3467.

42. Boukli, S. M. A., “Contribution à l’Étude de la Résistance Caractéristique des Bétons de la Région de Tlemcen,” PhD thesis, University of Tlemcen, Tlemcen, Algeria, 2009, 234 pp. (in French)

43. EN 206-1:2000, “Concrete. Specification, Performance, Production and Conformity,” European Committee for Standarization, Brussels, Belgium, 2000, 74 pp.

44. AFPC-AFREM, “Durabilité des Bétons: Méthode Recommandée pour la Mesure des Grandeurs Associées à la Durabilité,” Report of Technical Journeys AFPC- AFREM, Toulouse, France, 1997, 283 pp. (in French)

45. Ben Fraj, A.; Bonnet, S.; and Khelidj, A., “New Approach for Coupled Chloride/Moisture Transport in Non-Saturated Concrete with and without Slag,” Construction and Building Materials, V. 35, 2012, pp. 761-771.

46. Djerbi, A.; Bonnet, S.; Khelidj, A.; and Baroghel-Bouny, V., “Influence of Traversing Crack on Chloride Diffusion into Concrete,” Cement and Concrete Research, V. 38, No. 6, 2008, pp. 877-883.

47. NF XP P18-461, “Essai sur Béton Durci: Essai Accéléré des Ions Chlorure en Régime Stationnaire, Détermination du Coefficient de Diffusion Effectif des Ions Chlorure,” French Standardization Association, Saint-Denis, France, 2012, 11 pp. (in French).

48. Mehta, P. K., and Monteiro, P. J. M., Concrete: Microstructure, Properties and Materials, third edition, the McGraw-Hill Companies, Inc., New York, 2005, 659 pp.

49. Thomas, M., Supplementary Cementing Materials in Concrete, CRC Press, Boca Raton, FL, 2013, 190 pp.

50. Kumar, R., and Bhattacharjee, B., “Study on Some Factors Affecting the Results in the Use of MIP Method in Concrete Research,” Cement and Concrete Research, V. 33, No. 3, 2003, pp. 417-424.

51. Li, L. Y., “A Pore Size Distribution-Based Chloride Transport Model in Concrete,” Magazine of Concrete Research, V. 66, No. 18, 2014, pp. 937-947.

52. AutoPore IV 9500, “Operator’s Manual V1.04 Appendix D,” Micromeritics Instrument Corporation, Norcross, GA, 2001, 6 pp.

53. Khan, M. I., and Alhozaimy, A. M., “Properties of Natural Pozzolan and its Potential Utilization in Environmental Friendly Concrete,” Canadian Journal of Civil Engineering, V. 38, No. 1, 2011, pp. 71-78.

54. Touil, B.; Ghomari, F.; Bezzar, A.; Khelidj, A.; and Bonnet, S., “Les Bétons aux Pouzzolanes en Façade Maritime,” Proceedings 1O-270, CMSS2013, Rabat, Maroc, 2013, 100 pp. (in French)

55. Yang, C. C., “On the Relationship between Pore Structure and Chloride Diffusivity from Accelerated Chloride Migration Rest in Cement-Based Materials,” Cement and Concrete Research, V. 36, No. 7, 2006, pp. 1304-1311.

56. Sun, G. W.; Sun, W.; Zhang, Y. S.; and Liu, Z. Y., “Relationship between Chloride Diffusivity and Pore Structure of Hardened Cement Paste,” Journal of Zhejiang University-Science A (Applied Physics & Engineering), V. 12, No. 5, 2011, pp. 360-367.

57. Coussy, O., and Eymard, R., “Non-Linear Binding and the Diffusion-Migration Test,” Transport in Porous Media, V. 53, No. 1, 2003, pp. 51-74.

58. Touil, B.; Ghomari, F.; Bezzar, A.; Khelidj, A.; and Bonnet, S., “Effect of Natural Pozzolan on Concrete’s Durability,” ICDS12, Lisboa, Portugal, May 31-June 1, 2012, 8 pp.

59. Djerbi, A.; Bonnet, S.; Khelidj, A.; and Baroghel-Bouny, V., “Effect of Uniaxial Compressive Loading on Gas Permeability and Chloride Diffusion Coefficient of Concrete and their Relationship,” Cement and Concrete Research, V. 52, 2013, pp. 131-139.

60. Touil, B.; Ghomari, F.; Bezzar, A.; Khelidj, A.; and Bonnet, S., “Etude des Performances de Durabilité des Bétons Locaux,” Proceedings 29th Meeting of AUGC, Civil Engineering at the Service of the Mediterranean, Tlemcen, Algeria, May 29-31, 2011, V. 2, pp. 53-64. (in French)

61. Jensen, O. M.; Korzen, M. S. H.; Jakobsen, H. J.; and Skibsted, J., “Influence of Cement Constitution and Temperature on Chloride Binding in Cement Paste,” Advances in Cement Research, V. 12, No. 2, 2000, pp. 57-64.

62. Caré, S., “Effect of Temperature on Porosity and on Chloride Diffusion in Cement Pastes,” Construction and Building Materials, V. 22, 2008, pp. 1560-1573.

63. Lin, S. H., “Chloride Diffusion in Porous Concrete under Conditions of Variable Temperature,” Wärme - und Stoffübertragung, V. 28, No. 7, 1993, pp. 41


ALSO AVAILABLE IN:

Electronic Materials Journal