Record Attendance at The ACI Concrete Convention and Exposition – Fall 2015

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Record Attendance at The ACI Concrete Convention and Exposition – Fall 2015

Author(s):

Publication: Concrete International

Volume: 38

Issue: 4

Appears on pages(s): 22-25

Keywords:

DOI: 10.14359/51688906

Date: 4/1/2016

Abstract:
Convention theme of “Constructability” exemplified in the inaugural ACI Excellence Awards.