Recommendations for Casting Inclined Columns

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Recommendations for Casting Inclined Columns

Author(s): Britez, C.: Pacheco, J.; Bueno, S.; and Helene, P.

Publication: Concrete International

Volume: 38

Issue: 3

Appears on pages(s): 43-48

Keywords: finish, bughole, mockup, SCC

DOI: 10.14359/51688841

Date: 3/1/2016

Abstract:
The new Museu da Imagem e do Som (Museum of Image and Sound) headquarters is being built in Rio de Janeiro, Brazil. In this bold design, the structure incorporates a vertical boulevard, with seven stories, a continuous external promenade, and a display of sequential ramps and floors. With architectural concrete finishes specified for its unique forms and oblique lines, this building’s superstructure presented some special challenges—especially for the construction of inclined columns with high-performance concrete.

Related References:

1. ABNT NBR 6118, “Projeto de Estruturas de Concreto—Procedimento (Design of Structural Concrete—Procedure),” Associação Brasileira de Normas Técnicas (Brazilian National Standards Organization), Rio de Janeiro, Brazil, 2007, 221 pp.

2. ABNT NBR 12655, “Concreto de Cimento Portland—Preparo, Controle e Recebimento—Procedimento (Portland Cement Concrete—Preparation, Control and Acceptance—Procedure),” Associação Brasileira de Normas Técnicas (Brazilian National Standards Organization), Rio de Janeiro, Brazil, 2006, 18 pp.

3. ABNT NBR 14931, “Execução de Estruturas de Concreto—Procedimento (Execution of Concrete Structures—Procedure),” Associação Brasileira de Normas Técnicas (Brazilian National Standards Organization), Rio de Janeiro, Brazil, 2004, 53 pp.

4. ABNT NBR 15823, “Concreto Auto-Adensável (Self-Compacting Concrete),” Associação Brasileira de Normas Técnicas (Brazilian National Standards Organization), Rio de Janeiro, Brazil, 2010, 15 pp.

5. Neville, A.M., and Brooks, J.J., Concrete Technology, Longman Scientific & Technical, New York, 1987, 438 pp.

6. Kosmatka, S.H., and Wilson, M.L., Design and Control of Concrete Mixtures, 15th edition, Portland Cement Association, Skokie, IL, 2011, 444 pp.

7. The Contractor’s Guide to Quality Concrete Construction, third edition, L.K. Kennedy, ed., American Society of Concrete Contractors, St. Louis, MO, 2005, 147 pp.

8. Significance of Tests and Properties of Concrete & Concrete-Making Materials, J.F. Lamond and J.H. Pielert, eds., ASTM International, West Conshohocken, PA, 2006, 645 pp.

9. da Fonseca, A.A., and Nunes, Â., “Betão Branco: Fabrico, Características e Utilização Estrutural,” Secil, 1998, 20 pp.

10. Nero, J.M.G., and Nunes, A., “Betão Branco: Prescrição e Utilização,” Secil, 2000, 19 pp.

11. Kirchheim, A.P., “Concreto Branco,” Concreto - Ciência e Tecnologia, G.C. Isaia, ed., IBRACON, São Paulo, Brazil, 2011, pp. 1683-1730.

12. Thompson, M.S., “Blowholes in Concrete Surfaces,” Concrete, V. 3, No. 2, Feb. 1969, pp. 64-66.

13. Reading, T.J., “The Bughole Problem,” ACI Journal Proceedings, V. 69, No. 3, Mar. 1972, pp. 165-171.

14. CCANZ IB 33, “Specification and Production of Concrete Surface Finishes,” Cement & Concrete Association of New Zealand, Wellington, New Zealand, 1989, 28 pp.

15. CIB Working Commission W 29, “Tolerances on Blemishes of Concrete,” CIB Report No. 24, International Council for Building Research Studies and Documentation, 1974, 16 pp.

16. ABNT NBR 5735, “Cimento Portland de Alto-Forno (Blast-Furnace Slag Portland Cement—Specification),” Associação Brasileira de Normas Técnicas (Brazilian National Standards Organization), Rio de Janeiro, Brazil, 1991, 6 pp.

17. ABNT NBR 12653, “Materiais Pozolânicos—Requisitos (Pozzolanic Materials—Requirements),” Associação Brasileira de Normas Técnicas (Brazilian National Standards Organization), Rio de Janeiro, Brazil, 2014, 6 pp.

18. ABNT NBR 15900, “Água para Amassamento do Concreto (Mixing Water for Concrete),” Associação Brasileira de Normas Técnicas (Brazilian National Standards Organization), Rio de Janeiro, Brazil, 2009, 11 pp.

19. ABNT NBR 7211, “Agregados para Concreto—Especificação (Aggregates for Concrete—Specification),” Associação Brasileira de Normas Técnicas (Brazilian National Standards Organization), Rio de Janeiro, Brazil, 2009, 9 pp.

20. ABNT NBR 11768, “Aditivos Químicos para Concreto de Cimento Portland—Requisitos (Chemical Admixtures for Portland Cement Concrete—Requirements),” Associação Brasileira de Normas Técnicas (Brazilian National Standards Organization), Rio de Janeiro, Brazil, 2011, 19 pp.