Title: Laboratory Characterization and Field Application of Novel Ultra-High-Performance Glass Concrete

Author(s): Nancy A. Soliman, Ahmed F. Omran, and Arezki Tagnit-Hamou

Publication: Materials Journal

Volume: 113

Issue: 3

Appears on pages(s): 307-316

Keywords: field validation; footbridges; glass powder; large-scale production; sustainability; ultra-high-performance concrete (UHPC); ultra-highperformance glass concrete characterization (UHPGC)

DOI: 10.14359/51688827

Date: 5/1/2016

Abstract:
A new type of ecological ultra-high-performance concrete (UHPC) was developed at the University of Sherbrooke using waste glass of varying particle size distributions, named ultra-high-performance glass concrete (UHPGC). The current research presents laboratory characterization of various UHPGC mixtures in comparison to traditional UHPC mixtures. The research focuses on largescale application through a scaling-up by using a concrete pilot plant. The research also presents field validation of the optimized UHPGC mixture by erection of two footbridges as a case study. The UHPGC provides high workability and enhanced rheological properties, given the zero absorption of glass particles and optimized packing density of the entire material matrix. The UHPGC greatly improves the concrete microstructure, resulting in higher mechanical and durability properties, which are greater than the traditional UHPC. A compressive strength greater than 200 MPa (29,007 psi) can be obtained for the UHPGC. The higher mechanical properties allowed the footbridges’ design with approximately 60% reduced sections compared to normal concrete. The UHPGC improves durability, resulting in reduction of maintenance cost. Compared to traditional UHPC, the UHPGC reduces carbon footprint and production cost of UHPC by employing more than 400 kg/m3 of glass materials, and also saves money spent for the treatment and landfilling of glass cullets.

Related References:

1. Gupta, P. R., and Shiu, K. N., “Effective Repair and Maintenance Strategies for Parking Structures,” Concrete Repair Bulletin, July/August 2014, V. 27, No. 4, pp. 30-34.

2. U.S. Department of Homeland Security (DHS) Science and Technology, (S&T) Directorate’s Infrastructure Protection and Disaster Management Division (IDD) “UHPC Ultra-High Performance Concrete,” Technical Report, 23 pp., http://www.dhs.gov.

3. Richard, P., and Cheyrezy, M., “Reactive Powder Concretes with High Ductility and 200-800 MPa Compressive Strength,” Concrete Technology Past, Present, and Future—Proceedings of V. Mohan Malhotra Symposium, SP-144, P. K. Mehta, ed., American Concrete Institute, Farmington Hills, MI, 1994, pp. 507-518.

4. Richard, P., and Cheyrezy, M., “Composition of Reactive Powder Concretes,” Cement and Concrete Research, V. 25, No. 7, 1995, pp. 1501-1511. doi: 10.1016/0008-8846(95)00144-2

5. Dugat, J.; Roux, N.; and Bernier, G., “Mechanical Properties of Reactive Powder Concretes,” Materials and Structures, V. 29, May 1996, pp. 233-240. doi: 10.1007/BF02485945

6. Roux, N.; Andrade, C.; and Sanjuan, M., “Experimental Study of Durability of Reactive Powder Concretes,” Journal of Materials in Civil Engineering, ASCE, V. 8, No. 1, 1996, pp. 1-6. doi: 10.1061/(ASCE)0899-1561(1996)8:1(1)

7. Schmidt, M., and Fehling, E., “Ultra-High-Performance Concrete: Research, Development and Application in Europe,” Serviceability of Concrete—A Symposium Honoring Dr. Edward G. Nawy, SP-225, F. Barth, R. Frosch, H. Nassif, and A. Scanlon, eds., American Concrete Institute, Farmington Hills, MI, 2005, pp. 51-77.

8. Klemens, T., “Flexible Concrete Offers New Solutions,” Concrete Construction, V. 49, No. 12, Dec. 2004, p. 72

9. Racky, P., “Cost-Effectiveness and Sustainability of UHPC,” Proceedings of the International Symposium on Ultra-High Performance Concrete, V. 13, No. 15, Kassel, Germany, Sept. 2004, pp. 797-805.

10. Aïtcin, P.-C., “Cements of Yesterday and Today—Concrete of Tomorrow,” Cement and Concrete Research, V. 30, No. 9, 2000, pp. 1349-1359. doi: 10.1016/S0008-8846(00)00365-3

11. World Health Organization (WHO), “Health Systems: Improving Performance,” World Health Organization Report, 2000, 215 pp.

12. Shayan, A., and Xu, A., “Value-Added Utilisation of Waste Glass in Concrete,” Cement and Concrete Research, V. 34, No. 1, 2004, pp. 81-89. doi: 10.1016/S0008-8846(03)00251-5

13. FEVE, Collection for Recycling Rate in Europe, The European Container Glass Federation, 2013, http://www.feve.org/FEVE-STATIS-2013/Recycling-2011-Glass-coll.html. (last accessed Sept. 11, 2013)

14. Recyc-Québec, “Le Verre Fiches Informatives,” 2010. (in French)

15. USEPA, Wastes-Resource Conservation-Common Wastes & Materials, “Glass,” http://www.epa.gov/osw/conserve/materials/glass.htm. (last accessed Sept. 10, 2013).

16. Zidol, A.; Tohoue Tognonvi, M.; and Tagnit-Hamou, A., “Effect of Glass Powder on Concrete Sustainability,” 1st International Conference on Concrete Sustainability (ICCS13), Tokyo, Japan, May 27-29, 2012.

17. Zidol, A.; Pavoine, A.; and Tagnit-Hamou, A., “Effect of Glass Powder on Concrete Durability,” International Congress on Durability of Concrete, ICDC2012-D-11-00153, Trondheim, Norway, 2012.

18. Terro, M. J., “Properties of Concrete Made with Recycled Crushed Glass at Elevated Temperatures,” Building and Environment, V. 41, No. 5, 2006, pp. 633-639. doi: 10.1016/j.buildenv.2005.02.018

19. Idir, R.; Cyr, M.; and Tagnit-Hamou, A., “Use of Waste Glass as Powder and Aggregate in Cement-Based Materials,” SBEIDCO—1st International Conference on Sustainable Built Environment Infrastructures in Developing Countries ENSET Oran (Algeria), October 12-14, 2009, pp. 109-116.

20. Shi, C.; Wu, Y.; Riefler, C.; and Wang, H., “Characteristic and Pozzolanic Reactivity of Glass Powders,” Cement and Concrete Research, V. 35, No. 5, 2005, pp. 987-993. doi: 10.1016/j.cemconres.2004.05.015

21. Shayan, A., and Xu, A., “Performance of Glass Powder as a Pozzolanic Material in Concrete: a Field Trial on Concrete Slabs,” Cement and Concrete Research, V. 36, No. 3, 2006, pp. 457-468. doi: 10.1016/j.cemconres.2005.12.012

22. Roz-Ud-Din, N., and Parviz, S., “Strength and Durability of Recycled Aggregate Concrete Containing Milled Glass as Partial Replacement for Cement,” Construction and Building Materials, V. 29, 2012, pp. 368-377. doi: 10.1016/j.conbuildmat.2011.10.061

23. Shao, Y.; Lefort, T.; Moras, S.; and Rodriguez, D., “Studies on Concrete Containing Ground Waste Glass,” Cement and Concrete Research, V. 30, No. 1, 2000, pp. 91-100. doi: 10.1016/S0008-8846(99)00213-6

24. Khmiri, A.; Samet, B.; and Chaabouni, M., “A Cross Mixture Design to Optimise the Formulation of a Ground Waste Glass Blended Cement,” Construction and Building Materials, V. 28, No. 1, 2012, pp. 680-686. doi: 10.1016/j.conbuildmat.2011.10.032

25. Cong, K. S., and Feng, X., “The Effect of Recycled Glass Powder and Reject Fly Ash on the Mechanical Properties of Fiber-Reinforced Ultra-High Performance Concrete,” Advanced Material Science Engineering, Article ID, V. 263243, 2012, p. 8

26. Vaitkevicius, V.; Serelis, E.; and Hilbig, H., “The Effect of Glass Powder on the Microstructure of Ultra-High Performance Concrete,” Construction and Building Materials, V. 68, 2014, pp. 102-109. doi: 10.1016/j.conbuildmat.2014.05.101

27. Tagnit-Hamou, A., and Soliman, N., “Ultra-High Performance Glass Concrete and Method for Producing Same,” U.S. Patent Application. No. 61/806,083, filed March 28, 2013, accepted March 2014.

28. Soliman, N.; Aϊtcin; P.- C.; and Tagnit-Hamou, A., “New Generation of Ultra-High Performance Glass Concrete,” Advanced Concrete and Technologies. Lightweight and Foam Concretes. Education and Training, RILEM and CEB-fib, V. 5, Chapter 24, May 12-16, 2014, pp. 218-227.

29. Zerbino, R.; Giaccio, G.; Batic, O. R.; and Isaia, G. C., “Alkali-Silica Reaction in Mortars and Concretes Incorporating Natural Rice Husk Ash,” Construction and Building Materials, V. 36, 2012, pp. 796-806. doi: 10.1016/j.conbuildmat.2012.04.049

30. Juengera, M. C. G., and Ostertag, C. P., “Alkali-Silica Reactivity of Large Silica Fume-Derived Particles,” Cement and Concrete Research, V. 34, No. 8, 2004, pp. 1389-1402. doi: 10.1016/j.cemconres.2004.01.001

31. Andrea, S., and Chiara, B. M., “ASR Expansion Behavior of Recycled Glass Fine Aggregates in Concrete,” Cement and Concrete Research, V. 40, No. 4, 2010, pp. 531-536. doi: 10.1016/j.cemconres.2009.09.003

32. de Larrard, F., Concrete Mixture Proportioning: A Scientific Approach, E&FN Spon, London, UK, 1999.

33. Bonneau, O.; Lachemi, M.; Dallaire, E.; Dugat, J.; and Aïtcin, P.-C., “Mechanical Properties and Durability of Two Industrial Reactive Powder Concretes,” ACI Materials Journal, V. 94, No. 4, July-Aug. 1997, pp. 286-290.

34. Nielsen, C. V., “Triaxial Behavior of High-Strength Concrete and Mortar,” ACI Materials Journal, V. 95, No. 2, Mar.-Apr. 1998, pp. 144-151.

35. Rossi, P., “Development of New Cement Composite Materials for Construction,” Proceedings of the Institution of Mechanical Engineers, Part L: Journal of Materials: Design and Applications, V. 219, No. 1, 2005, pp. 67-74. doi: 10.1243/146442005X10193

36. Brameshuber, W., and Uebachs, S., “Practical Experience with the Application of Self-Compacting Concrete in Germany,” Proceedings of the Second International Symposium on Self-Compacting Concrete, Tokyo, Japan, 2001, pp. 687-696.

37. EFNARC, “Specification and Guidelines for Self-Compacting Concrete,” Surrey, UK, Feb. 2002, 32 pp.

38. Wuest, J., “Etude exploratoire des propriétés mécaniques de bétons de fibres ultra performants de structures,” diploma thesis, Swiss Federal Institute of Technology (EPFL), Lausanne, Switzerland, 2004.

39. Perry, V., and Zakariasen, D., “First Use of Ultra-High Performance Concrete for an Innovative Train Station Canopy,” Concrete Technology Today, V. 25, No. 2, Aug. 2004, pp. 1-2.

40. Habel, K.; Viviani, M.; Denarié, E.; and Brühwiler, E., “Development of the Mechanical Properties of an Ultra-High Performance Fiber Reinforced Concrete (UHPFRC),” Cement and Concrete Research, V. 36, No. 7, 2006, pp. 1362-1370. doi: 10.1016/j.cemconres.2006.03.009

41. Graybeal, B., “Characterization of the Behavior of Ultra-High Performance Concrete,” PhD dissertation, University of Maryland, College Park, MD.

42. Federal Highway Administration (FHWA), “Achieving the Promise of Ultra-High-Performance Concrete,” Focus, Nov. 2004, http://www.tfhrc.gove/focus/nov04/01.htm.

43. Gao, R., “Liu, Z.-M.; Zhang, L.-Q.; and Stroeven, P., “Static Properties of Reactive Powder Concrete Beams,” Key Engineering Materials, V. 302-303, 2006, pp. 521-527. doi: 10.4028/www.scientific.net/KEM.302-303.521

44. Lee, M.-G.; Chiu, C.-T.; and Wang, Y.-C., “Chiu, C.-T.; and Wang; Y.-C, “The Study of Bond Strength and Bond Durability of Reactive Powder Concrete,” Journal of ASTM International, V. 2, No. 7, 2005, pp. 104-113. doi: 10.1520/JAI12960

45. Shaheen, E., and Shrive, N. G., “Optimization of Mechanical Properties and Durability of Reactive Powder Concrete,” ACI Materials Journal, V. 103, No. 6, Nov.-Dec. 2006, pp. 444-451.

46. Tagnit-Hamou, A.; Soliman, N.; Omran, A. F.; Mousa, M. T.; Gauvreau, N.; and Provencher, M. F., “Novel Ultra-High Performance Glass Concrete,” Concrete International, V. 39, No. 3, Mar. 2015, pp. 53-59.


ALSO AVAILABLE IN:

Electronic Materials Journal