Discussion from the Jan/Feb 2015 ACI Materials Journal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Discussion from the Jan/Feb 2015 ACI Materials Journal

Author(s): Zdenek P. Bažant, Roman Wendner, Giannis Boumakis, and Mija Hubler

Publication: Materials Journal

Volume: 112

Issue: 6

Appears on pages(s): 829-832

Keywords:

DOI:

Date: 11/1/2015

Abstract:
Disc. 112-M14/From the January-February 2015 ACI Materials Journal, p. 125 Statistical Comparisons of Creep and Shrinkage Prediction Models Using RILEM and NU-ITI Databases. Paper by Akthem Al-Manaseer and Armando Prado


ALSO AVAILABLE IN:

Electronic Materials Journal