Effect of Admixtures on Pumpability for High-Strength Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Admixtures on Pumpability for High-Strength Concrete

Author(s): Jae Hong Jeong, Kyong Pil Jang, Chan Kyu Park, Seung Hoon Lee, and Seung Hee Kwon

Publication: Materials Journal

Volume: 113

Issue: 3

Appears on pages(s): 323-333

Keywords: admixtures; high-strength concrete; lubricating layer; pumpability; rheological properties

DOI: 10.14359/51688644

Date: 5/1/2016

Abstract:
In this study, the effects of mineral and chemical admixtures on pumpability of high-strength concrete were investigated through measuring rheological properties of concrete and the lubricating layer. A total of 32 concrete mixtures were manufactured and tested according to different types and dosages of silica fume, zirconia silica fume, fly ash, and high-range water-reducing admixtures (HRWRAs). From the experiments, it was found that zirconia silica fume is very effective in enhancing pumpability, and the increase of HRWRA dosage leads to the decrease of the viscosity of the lubricating layer and the increase of pumpability.

Related References:

1. Jacobsen, S.; Haugan, L.; Hammer, T. A.; and Kalogiannidis, E., “Flow Conditions of Fresh Mortar and Concrete in Different Pipes,” Cement and Concrete Research, V. 39, No. 11, 2009, pp. 997-1006. doi: 10.1016/j.cemconres.2009.07.005

2. Kaplan, D.; de Larrard, F.; and Sedran, T., “Design of Concrete Pumping Circuit,” ACI Materials Journal, V. 102, No. 2, Mar.-Apr. 2005, pp. 110-117.

3. Rio, O.; Rodriguez, A.; Nabulsi, S.; and Alvarez, M., “Pumping Quality Control Method Based on Online Concrete Pumping Assessment,” ACI Materials Journal, V. 108, No. 4, July-Aug. 2011, pp. 423-431.

4. Kwon, S. H.; Park, C. K.; Jeong, J. H.; Jo, S. D.; and Lee, S. H., “Prediction of Concrete Pumping—Part I: Development of New Tribometer for Analysis of Lubricating Layer,” ACI Materials Journal, V. 110, No. 6, Nov.-Dec. 2013, pp. 647-655.

5. Kwon, S. H.; Park, C. K.; Jeong, J. H.; Jo, S. D.; and Lee, S. H., “Prediction of Concrete Pumping—Part II: Analytical Prediction and Experimental Verification,” ACI Materials Journal, V. 110, No. 6, Nov.-Dec. 2013, pp. 657-667.

6. Choi, M. S.; Kim, Y. J.; Jang, K. P.; and Kwon, S. H., “Effect of the Coarse Aggregate Size on Pipe Flow of Pumped Concrete,” Construction and Building Materials, V. 66, 2014, pp. 723-730. doi: 10.1016/j.conbuildmat.2014.06.027

7. Jo, S. D.; Park, C. K.; Jeong, J. H.; Lee, S. H.; and Kwon, S. H., “A Computational Approach to Estimating a Lubricating Layer in Concrete Pumping,” Computers, Materials and Continua, V. 27, No. 3, 2011, pp. 189-210.

8. Tattersall, G. H., and Banfill, P. F., The Rheology of Fresh Concrete, Pitman Advanced Publishing Program, London, UK, 1983, p. 53.

9. Ngo, T. T.; Kadri, E. H.; Bennacer, R.; and Cussigh, F., “Use of Tribometer to Estimate Interface Friction and Concrete Boundary Layer Composition during the Fluid Concrete Pumping,” Construction and Building Materials, V. 24, No. 7, 2010, pp. 1253-1261. doi: 10.1016/j.conbuildmat.2009.12.010

10. Koehler, E. P.; Fowler, D. W.; Ferraris, C. F.; and Amziane, S., “A New Portable Rheometer for Fresh Self-Consolidating Concrete,” Workability of SCC: Roles of Its Constituents and Measurement Techniques, SP-233, C. Shi and K. H. Khayat, eds., American Concrete Institute, Farmington Hills, MI, 2006, pp. 97-116.

11. Wallevik, J. E., “Minimizing End-Effects in the Coaxial Cylinders Viscometer: Viscoplastic Flow inside the ConTec BML Viscometer 3,” Journal of Non-Newtonian Fluid Mechanics, V. 155, No. 3, 2008, pp. 116-123. doi: 10.1016/j.jnnfm.2008.05.006

12. Phillips, R. J.; Armstrong, R. C.; Brown, R. A.; Graham, A. L.; and Abbott, J. R., “A Constitutive Equation for Concentrated Suspensions that Accounts for Shear-Induced Particle Migration,” Physics of Fluids, V. 4, No. 1, 1992, pp. 30-40. doi: 10.1063/1.858498

13. Chapdelain, F., “Etude Fondamentale et Pratique sur le Pompage du Beton,” doctoral thesis, Laval University, Quebec, QC, Canada, 2007, 153 pp.

14. Ferraris, C. F.; Obla, K. H.; and Hill, R., “The Influence of Mineral Admixtures on the Rheology of Cement Paste and Concrete,” Cement and Concrete Research, V. 31, No. 2, 2001, pp. 245-255. doi: 10.1016/S0008-8846(00)00454-3

15. Park, C. K.; Noh, M. H.; and Park, T. H., “Rheological Properties of Cementitious Materials Containing Mineral Admixtures,” Cement and Concrete Research, V. 35, No. 5, 2005, pp. 842-849. doi: 10.1016/j.cemconres.2004.11.002

16. Şahmaran, M.; Christianto, H. A.; and Yaman, İ. Ö., “The Effect of Chemical Admixtures and Mineral Additives on the Properties of Self-Compacting Mortars,” Cement and Concrete Composites, V. 28, No. 5, 2006, pp. 432-440. doi: 10.1016/j.cemconcomp.2005.12.003

17. Koehler, E. P., and Fowler, D. W., “Development of a Portable Rheometer for Fresh Portland Cement Concrete,” Research Report, International Center for Aggregates Research, Austin, TX, 2004, 321 pp.

18. Choi, M. S.; Roussel, N.; Kim, Y. J.; and Kim, J. K., “Lubrication Layer Properties during Concrete Pumping,” Cement and Concrete Research, V. 45, 2013, pp. 69-78. doi: 10.1016/j.cemconres.2012.11.001


ALSO AVAILABLE IN:

Electronic Materials Journal