Bond of Reinforcement in High-Strength Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Bond of Reinforcement in High-Strength Concrete

Author(s): Joseph Jones and Julio A. Ramirez

Publication: Structural Journal

Volume: 113

Issue: 3

Appears on pages(s): 549-556

Keywords:

DOI: 10.14359/51688620

Date: 5/1/2016

Abstract:
This paper describes an examination of the development of tension lap splices in high-strength concrete and the applicability of the restriction in the ACI 318 code where the values of √fc′ used to calculate development length shall not exceed 100 psi. The focus is on the development of splices with Grade 60 epoxy-coated and uncoated bars in normal weight concrete. A summary of the behavior of bond is presented to provide context for the study. It is followed by a literature review to analyze the relevant previous experimental work in this area. Based on the analysis of those data, a modification to the current code limitation is proposed. The main conclusion of this paper is that the limit of 100 psi (0.689 MPa) on the square root of the specified compressive strength in Section 12.1.2 of ACI 318-11 (Section 25.4.1.4 of 318-14) may be extended to 120 psi (0.827 MPa) based on the analysis of available data without significant modifications to the current provisions for concrete strengths up to 16,000 psi (110 MPa).

Related References:

ACI Committee 318, 2011, “Building Code Requirements for Structural Concrete (ACI 318-11) and Commentary,” American Concrete Institute, Farmington Hills, MI, 503 pp.

ACI Committee 318, 2014, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 519 pp.

Azizinamini, A.; Pavel, R.; Hatfield, E.; and Ghosh, S. K., 1999, “Behavior of Lab-Spliced Reinforcing Bars Embedded in High-Strength Concrete,” ACI Structural Journal, V. 96, No. 5, Sept.-Oct., pp. 826-835.

Choi, O. C.; Hadje-Ghaffari, H.; Darwin, D.; and McCabe, S. L., 1991, “Bond of Epoxy-Coated Reinforcement: Bar Parameters,” ACI Materials Journal, V. 88, No. 2, Mar.-Apr., pp. 207-217.

Cleary, D. B., and Ramirez, J. A., 1991, “Bond Strength of Epoxy-Coated Reinforcement,” ACI Materials Journal, V. 88, No. 2, Mar.-Apr., pp. 146-149.

Cleary, D. B., and Ramirez, J. A., 1993, “Epoxy-Coated Reinforcement under Repeated Loading,” ACI Structural Journal, V. 90, No. 4, July-Aug., pp. 451-458.

Darwin, D.; Tholen, M. L.; Idun, E. K.; and Zuo, J., 1996, “Splice Strength of High Relative Rib Area Reinforcing Bars,” ACI Structural Journal, V. 93, No. 1, Jan.-Feb., pp. 95-107.

Hamad, B. S.; Jirsa, J. O.; and D’Abreu de Paulo, N.,1993, “Anchorage Strength of Epoxy-Coated Hooked Bars,” ACI Structural Journal, V. 90, No. 2, Mar.-Apr., pp. 210-217.

Hasan, H. O.; Cleary, D. B.; and Ramirez, J. A., 1996, “Performance of Concrete Bridge Decks and Slabs Reinforced with Epoxy-Coated Steel,” ACI Structural Journal, V. 93, No. 4, July-Aug., pp. 397-403.

Hester, C. J.; Salamizavaregh, S.; Darwin, D.; and McCabe, S. L., 1993, “Bond of Epoxy-Coated Reinforcement: Splices,” ACI Structural Journal, V. 90, No. 1, Jan.-Feb., pp. 89-102.

Joint ACI-ASCE Committee 408, 2003, “Bond and Development of Straight Reinforcing Bars in Tension (ACI 408R-03),” American Concrete Institute, Farmington Hills, MI, 49 pp.

Kadoriku, J., 1994, “Study on Behavior of Lap Splices in High-Strength Reinforced Concrete Members,” doctorate thesis, Kobe University, Kobe, Japan, 201 pp.

Ramirez, J. A., and Russell, B. W., 2008, “Transfer, Development, and Splice Length for Strand/Reinforcement in High-Strength Concrete,” Transportation Research Board, National Research Council, Washington, DC.

Treece, R. A., and Jirsa, J. O., 1989, “Bond Strength of Epoxy-Coated Reinforcing Bars,” ACI Materials Journal, V. 86, No. 2, Mar.-Apr., pp. 167-174.


ALSO AVAILABLE IN:

Electronic Structural Journal