Simplified Approach for Assessing Shear Resistance of Reinforced Concrete Beams under Impact Loads

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Simplified Approach for Assessing Shear Resistance of Reinforced Concrete Beams under Impact Loads

Author(s): De-Bo Zhao, Wei-Jian Yi, and Sashi K. Kunnath

Publication: Structural Journal

Volume: 113

Issue: 4

Appears on pages(s): 747-756

Keywords: beam; impact behavior; impact loading; reinforced concrete; shear

DOI: 10.14359/51688617

Date: 7/1/2016

Abstract:
To assess the shear resistance of reinforced concrete (RC) beams under impact loads, a two-mass model is proposed to simulate the dynamic response of RC beams wherein the impact process is divided into two phases: local response phase, and overall response phase. Stress wave propagation effects are taken into account in the local response phase. Using a dynamic failure criterion based on the Modified Compression Field Theory (MCFT), the proposed model evaluates the dynamic moment and shear demand in an RC beam and is capable of assessing the likelihood of shear failure. A comparison between the numerical simulations and experimental results indicates that the proposed model can predict the occurrence of shear failure with reasonable accuracy.

Related References:

1. Bentur, A.; Mindess, S.; and Banthia, N., “The Behaviour of Concrete under Impact Loading: Experimental Procedures and Method of Analysis,” Materials and Structures, V. 19, No. 5, 1986, pp. 371-378. doi: 10.1007/BF02472127

2. Banthia, N.; Mindess, S.; Bentur, A.; and Pigeon, M., “Impact Testing of Concrete Using a Drop-Weight Impact Machine,” Experimental Mechanics, V. 29, No. 1, 1989, pp. 63-69. doi: 10.1007/BF02327783

3. Kishi, N.; Nakano, O.; Matsuoka, K. G.; and Ando, T., “Experimental Study on Ultimate Strength of Flexural-Failure-Type RC Beams under Impact Loading,” Transactions of 16th International Conference on Structural Mechanics in Reactor Techonology, Washington, DC, 2001, 7 pp.

4. Kishi, N.; Mikami, H.; Matsuoka, K.; and Ando, T., “Impact Behavior of Shear-Failure-Type RC Beams without Shear Rebar,” International Journal of Impact Engineering, V. 27, No. 9, 2002, pp. 955-968. doi: 10.1016/S0734-743X(01)00149-X

5. Fujikake, K.; Li, B.; and Soeun, S., “Impact Response of Reinforced Concrete Beam and Its Analytical Evaluation,” Journal of Structural Engineering, ASCE, V. 135, No. 8, 2009, pp. 938-950. doi: 10.1061/(ASCE)ST.1943-541X.0000039

6. Bischoff, P., and Perry, S., “Compressive Behaviour of Concrete at High Strain Rates,” Materials and Structures, V. 24, No. 6, 1991, pp. 425-450. doi: 10.1007/BF02472016

7. Malvar, L. J., and Ross, C. A., “Review of Strain Rate Effects for Concrete in Tension,” ACI Materials Journal, V. 95, No. 6, Nov.-Dec. 1998, pp. 735-739.

8. Soroushian, P., and Choi, K.-B., “Steel Mechanical Properties at Different Strain Rates,” Journal of Structural Engineering, ASCE, V. 113, No. 4, 1987, pp. 663-672. doi: 10.1061/(ASCE)0733-9445(1987)113:4(663)

9. Malvar, L. J., “Review of Static and Dynamic Properties of Steel Reinforcing Bars,” ACI Materials Journal, V. 95, No. 5, Sept.-Oct. 1998, pp. 609-614.

10. Saatci, S., and Vecchio, F. J., “Effects of Shear Mechanisms on Impact Behavior of Reinforced Concrete Beams,” ACI Structural Journal, V. 106, No. 1, Jan.-Feb. 2009, pp. 78-86.

11. Kishi, N., and Mikami, H., “Empirical Formulas for Designing Reinforced Concrete Beams under Impact Loading,” ACI Structural Journal, V. 109, No. 4, July-Aug. 2012, pp. 510-519.

12. Tachibana, S.; Masuya, H.; and Nakamura, S., “Performance Based Design of Reinforced Concrete Beams under Impact,” Natural Hazards and Earth System Sciences, V. 10, No. 6, 2010, pp. 1069-1078. doi: 10.5194/nhess-10-1069-2010

13. Kishi, N., and Bhatti, A. Q., “An Equivalent Fracture Energy Concept for Nonlinear Dynamic Response Analysis of Prototype RC Girders Subjected to Falling-Weight Impact Loading,” International Journal of Impact Engineering, V. 37, No. 1, 2010, pp. 103-113. doi: 10.1016/j.ijimpeng.2009.07.007

14. Saatci, S., and Vecchio, F. J., “Nonlinear Finite Element Modeling of Reinforced Concrete Structures under Impact Loads,” ACI Structural Journal, V. 106, No. 5, Sept.-Oct. 2009, pp. 717-725.

15. Bhatti, A. Q.; Kishi, N.; Mikami, H.; and Ando, T., “Elasto-Plastic Impact Response Analysis of Shear-Failure-Type RC Beams with Shear Rebars,” Materials & Design, V. 30, No. 3, 2009, pp. 502-510. doi: 10.1016/j.matdes.2008.05.068

16. Ožbolt, J., and Sharma, A., “Numerical Simulation of Reinforced Concrete Beams with Different Shear Reinforcements under Dynamic Impact Loads,” International Journal of Impact Engineering, V. 38, No. 12, 2011, pp. 940-950. doi: 10.1016/j.ijimpeng.2011.08.003

17. Cotsovos, D. M., and Pavlovic, M. N., “Modelling of RC Beams under Impact Loading,” Proceedings of the Institution of Civil Engineers: Structures and Buildings, V. 165, No. 2, 2012, pp. 77-94. doi: 10.1680/stbu.2012.165.2.77

18. Cotsovos, D.; Stathopoulos, N.; and Zeris, C., “Behavior of RC Beams Subjected to High Rates of Concentrated Loading,” Journal of Structural Engineering, ASCE, V. 134, No. 12, 2008, pp. 1839-1851. doi: 10.1061/(ASCE)0733-9445(2008)134:12(1839)

19. Cotsovos, D. M., “A Simplified Approach for Assessing the Load-Carrying Capacity of Reinforced Concrete Beams under Concentrated Load Applied at High Rates,” International Journal of Impact Engineering, V. 37, No. 8, 2010, pp. 907-917. doi: 10.1016/j.ijimpeng.2010.01.005

20. Delhomme, F.; Mommessin, M.; Mougin, J. P.; and Perrotin, P., “Simulation of a Block Impacting a Reinforced Concrete Slab with a Finite Element Model and a Mass-Spring System,” Engineering Structures, V. 29, No. 11, 2007, pp. 2844-2852. doi: 10.1016/j.engstruct.2007.01.017

21. Micallef, K.; Sagaseta, J.; Fernández Ruiz, M.; and Muttoni, A., “Assessing Punching Shear Failure in Reinforced Concrete Flat Slabs Subjected to Localised Impact Loading,” International Journal of Impact Engineering, V. 71, 2014, pp. 17-33. doi: 10.1016/j.ijimpeng.2014.04.003

22. Bentz, E. C., “Sectional Analysis of Reinforced Concrete Members,” PhD thesis, Graduate Department of Civil Engineering, University of Toronto, Toronto, ON, Canada, 2000, 184 pp.

23. Vecchio, F. J., and Collins, M. P., “The Modified Compression-Field Theory for Reinforced Concrete Elements Subjected to Shear,” ACI Journal Proceedings, V. 83, No. 2, Mar.-Apr. 1986, pp. 219-231.

24. CEB-FIP, “CEB-FIP Model Code 1990: Design Code,” Comité Euro-International, Thomas Telford, London, UK, 1993, 437 pp.

25. Adhikary, S. D.; Li, B.; and Fujikake, K., “Dynamic Behavior of Reinforced Concrete Beams under Varying Rates of Concentrated Loading,” International Journal of Impact Engineering, V. 47, 2012, pp. 24-38. doi: 10.1016/j.ijimpeng.2012.02.001

26. Xu, B., and Zeng, X., “Experimental Study on the Behaviors of Reinforced Concrete Beams under Impact Loadings,” China Civil Engineering Journal, V. 47, No. 2, 2014, pp. 41-51. (in Chinese)

27. LS-DYNA v971, Livermore Software Technology Corporation, 2011.

28. Ahmed, T.; Ramachandra, L.; and Bhattacharyya, S., “Elasto-Plastic Response of Free–Free Beams Subjected to Impact Loads,” International Journal of Impact Engineering, V. 25, No. 7, 2001, pp. 661-681. doi: 10.1016/S0734-743X(01)00002-1

29. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318M-08) and Commentary,” American Concrete Institute, Farmington Hills, MI., 2008, 503 pp.

30. Saatci, S., “Behaviour and Modelling of Reinforced Concrete Structures Subjected to Impact Loads,” PhD thesis, Department of Civil Engineering, University of Toronto, Toronto, ON, Canada, 2007, 288 pp.

31. Fujikake, K.; Senga, T.; Ueda, N.; Ohno, T.; and Katagiri, M., “Study on Impact Response of Reactive Powder Concrete Beam and Its Analytical Model,” Journal of Advanced Concrete Technology, V. 4, No. 1, 2006, pp. 99-108. doi: 10.3151/jact.4.99

32. Miyamoto, A.; King, M. E.; and Fujii, M., “Non-Linear Dynamic Analysis and Design Concepts for RC Beams under Impulsive Loads,” Bulletin of the New Zealand National Society for Earthquake Engineering, V. 22, No. 2, 1989, pp. 98-111.

33. Zeng, X., and Xu, B., “Experimental Study on Impact-Resistant Behavior of RC Beams without Shear-Resistant Rebars,” China Civil Engineering Journal, V. 45, No. 9, 2012, pp. 63-72. (in Chinese)


ALSO AVAILABLE IN:

Electronic Structural Journal