Greener Concrete Using Post-Consumer Products

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Greener Concrete Using Post-Consumer Products

Author(s): Tarun R. Naik; Rakesh Kumar; and Giacomo Moriconi

Publication: Symposium Paper

Volume: 305

Issue:

Appears on pages(s): 42.1-42.10

Keywords: alkali-silica reaction; durability; glass; greener concrete; plastics; post-consumer products; used tires

DOI: 10.14359/51688606

Date: 9/1/2015

Abstract:
The need to develop greener concrete is increasing day-by-day with the desire to develop sustainable infrastructures, resource conservation, and contribution to the reduction in the causes of global climate change by reducing carbon footprint of concrete and concrete-making materials, through environmentally-friendly techniques of concrete manufacturing by using recyclable materials, for example post-consumer products. This paper describes the possible roles of post-consumer products namely: used tires, plastics, and glass in the manufacture of greener concrete. Extensive research findings from the studies carried out at University of Wisconsin-Milwaukee Center for By-Products Utilization (UWM-CBU) and elsewhere describing the technology for beneficial use of recycled materials obtained from post-consumer materials in the manufacturing of greener concrete has been presented in this paper. The goal is to not waste such materials because waste is wasted if you waste it; otherwise, it is a resource for a society to be beneficially recycled.