Title: Reliability of Temperature-Dependent Models for Analysis of Reinforced Concrete Members Subjected to Fire

Author(s): Fady ElMohandes and Frank J. Vecchio

Publication: Structural Journal

Volume: 113

Issue: 3

Appears on pages(s): 481-490

Keywords: ASCE; cooling; Eurocode; fire; heat; structures; thermal

DOI: 10.14359/51688605

Date: 5/1/2016

Abstract:
A computational modeling procedure has been developed for better estimating the behavior of reinforced concrete members subjected to fire. The highly nonlinear procedure of combined thermal and structural analysis integrates the transient conductive, boundaryconvective, and boundary-radiative heat transfer analysis with the structural analysis of reinforced concrete members. The effect of the models selected for the various temperature-dependent properties of concrete and steel reinforcement on the overall response of reinforced concrete members with various loading and fire scenarios was studied. For concrete materials, the temperaturedependent properties investigated and included the density, thermal conductivity, specific heat capacity, thermal expansion strain, peak compressive stress and the corresponding strain, initial modulus of elasticity, tensile strength, and the shape of the stress-strain curve. For steel reinforcing bars, they included the thermal expansion strain, yield stress, ultimate stress, and Young’s modulus. In addition to the heat development phase, the cooling phase was also considered as a fire scenario, where the residual capacity of concrete columns subjected to fire was investigated.

Related References:

1. Lie, T. T., “Structural Fire Protection,” ASCE Manuals and Reports on Engineering Practice No. 78, American Society of Civil Engineers, Reston, VA, 1992, 241 pp.

2. CEN, “ENV 1992-1-2:1995—Eurocode 2: Design of Concrete Structures—Part 1-2: General Rules. Structural Fire Design,” European Committee for Standardization (CEN), Brussels, Belgium, 1996, 63 pp.

3. CEN, “EN 1992-1-2:2004—Eurocode 2: Design of Concrete Structures—Part 1-2: General Rules. Structural Fire Design,” European Committee for Standardization (CEN), Brussels, Belgium, 2005, 97 pp.

4. ElMohandes, F., “Advanced Three-Dimensional Nonlinear Analysis of Reinforced Concrete Structures Subjected to Fire and Extreme Loads,” PhD thesis, University of Toronto, Toronto, ON, Canada, 2013, 407 pp.

5. ElMohandes, F., and Vecchio, F. J., “Vector3: A. User’s Manual,” Department of Civil Engineering, University of Toronto, Toronto, ON, Canada, 2013, 81 pp.

6. ElMohandes, F., and Vecchio, F. J., “Vector3: B. Sample Coupled Thermal and Structural Analysis,” Department of Civil Engineering, University of Toronto, Toronto, ON, Canada, 2013, 68 pp.

7. Vecchio, F. J., and Collins, M. P., “The Modified Compression Field Theory for Reinforced Concrete Elements Subjected to Shear,” ACI Journal Proceedings, V. 83, No. 2, Mar.-Apr. 1986, pp. 219-231.

8. Lie, T. T., and Lin, T. D., “Fire Tests on Reinforced Concrete Columns, Specimens No. 1-12,” 12 NRC Publications—DBR Internal Reports No. 478-489, Division of Building Research, National Research Council of Canada (NRC), Ottawa, ON, Canada, 1983.

9. Mostafaei, H.; Leroux, P.; and Lafrance, P.-S., “Fire Endurance of a Reinforced Concrete Column under Both Axial and Lateral Loads,” NRC Report IRC-RR-327, National Research Council Canada (NRC), Ottawa, ON, Canada, 2012, 31 pp.

10. Lie, T. T.; Rowe, T. J.; and Lin, T. D., “Residual Strength of Fire-Exposed Reinforced Concrete Columns,” Evaluation and Repair of Fire Damage to Concrete, SP-92, American Concrete Institute, Farmington Hills, MI, 1986, pp. 153-174.

11. CAN/ULC S101-07, “Standard Methods of Fire Endurance Tests of Building Construction and Materials,” Underwriters Laboratories of Canada, Toronto, ON, Canada, 2007, 85 pp.

12. ASTM E119-12a, “Standard Test Methods for Fire Tests of Building Construction and Materials,” ASTM International, West Conshohocken, PA, 2012, 34 pp.

13. ISO, “ISO 834-1:1999: Fire-Resistance Tests—Elements of Building Construction—Part 1: General Requirements,” ISO, Geneva, Switzerland, 1999, 25 pp.

14. Franssen, J.-M., “SAFIR: A Thermal/Structural Program Modelling Structures under Fire,” North American Steel Construction Conference (NASCC), American Institute of Steel Construction, Chicago, IL, 2003.

15. Lie, T. T., and Allen, D. E., “Calculations of the Fire Resistance of Reinforced Concrete Columns,” NRCC 12797, Division of Building Research, National Research Council of Canada, Ottawa, ON, Canada, 1972.

16. Lie, T. T.; Lin, T. D.; Allen, D. E.; and Abrams, M. S., “Fire Resistance of Reinforced Concrete Columns,” DBR Paper No. 1167, Division of Building Research, National Research Council of Canada (NRC), Ottawa, ON, Canada, 1984, 20 pp.

17. Chang, Y. F.; Chen, Y. H.; Sheu, M. S.; and Yao, G. C., “Residual Stress-Strain Relationship for Concrete after Exposure to High Temperatures,” Cement and Concrete Research, V. 36, No. 10, 2006, pp. 1999-2005. doi: 10.1016/j.cemconres.2006.05.029


ALSO AVAILABLE IN:

Electronic Structural Journal