Effect Of Fly Ash And Polypropylene Fiber On Early Shrinkage And Cracking Of Alkali-Activated Slag Cement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect Of Fly Ash And Polypropylene Fiber On Early Shrinkage And Cracking Of Alkali-Activated Slag Cement

Author(s): Yuanyuan Wan and Yonghao Fang

Publication: Symposium Paper

Volume: 305

Issue:

Appears on pages(s): 24.1-24.10

Keywords: alkali-activated slag cement; cracking; fly ash; polypropylene fiber; shrinkages

DOI: 10.14359/51688584

Date: 9/1/2015

Abstract:
The effects of substituting 5-20% fly ash for slag and adding 0.10~0.30% polypropylene fiber on the physical and mechanica1 properties, shrinkage and cracking behaviors, water permeability and porosity of alkali-activated ground granulated blast furnace slag cement paste and mortar are studied. The results show that replacing 5-15% fly ash for slag in the alkali-activated slag cement paste and mortar increased the flexural strength, though the compressive strength were slightly decreased. When the replacement of fly ash for slag was increased to 20%, both the flexural and compressive strengths of the paste and mortar begin to decrease. The early shrinkage and cracking were reduced by the fly ash replacement. Adding 0.10~0.30% polypropylene fiber decreased both the flexural and compressive strengths, whereas the shrinkage, especially the cracking of the alkali-activated slag cement was greatly reduced.