Self-Compacting Concrete With C&DW: Microstructure And Long-Term

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Self-Compacting Concrete With C&DW: Microstructure And Long-Term

Author(s): Stefania Manzi; Claudio Mazzotti and Maria Chiara Bignozzi

Publication: Symposium Paper

Volume: 305

Issue:

Appears on pages(s): 17.1-17.8

Keywords: construction and demolition waste; long-term behavior; mechanical properties; microstructure; porosity; self-consolidating concrete; sustainability

DOI: 10.14359/51688577

Date: 9/1/2015

Abstract:
Mix-design of self-consolidating concrete (SCC) with construction and demolition concrete waste (C&DW) as recycled aggregates is investigated. The novelty of this paper consists in the possibility of using both fine and coarse high-grade C&DW for the preparation of new SCC. The effects of recycled aggregates on porosity measurements and mechanical investigations combined with time-dependent properties are investigated. A reference SCC mix, with natural aggregates and the same water/powder ratio as SCC with recycled aggregates, is reported for comparison. Results are correlated in an integrated approach to study the feasibility of structural SCC with medium-high mechanical strength. Finally, this work attempts to strengthen the concept of sustainability in civil constructions.