Concrete Q&A

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Q&A

Author(s):

Publication: Concrete International

Volume: 37

Issue: 11

Appears on pages(s): 68

Keywords:

DOI: 10.14359/51688531

Date: 11/1/2015

Abstract:
Designing Anchors and Their Attachments for Tensile Loading

Related References:

1. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-11) and Commentary,” American Concrete Institute, Farmington Hills, MI, 2011, 503 pp.

2. “Minimum Design Loads for Buildings and Other Structures (ASCE/SEI 7-10),” American Society of Civil Engineers, Reston, VA, 2013, 636 pp.