Out-of-Plane Behavior and Failure of Full-Scale RC Bearing

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Out-of-Plane Behavior and Failure of Full-Scale RC Bearing

Author(s): Kevin Mueller

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 4/12/2015

Abstract:
This session provides an opportunity for researchers, architectural/civil/structural engineers, and students to exchange recent advances in applied research and to share information, experiences, and knowledge in the implementation of rational design approaches for determining the fire resistance of a range of concrete structures.