Reliability-Based Study on Ductility Measures of Reinforced Concrete Beams in ACI 318

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Reliability-Based Study on Ductility Measures of Reinforced Concrete Beams in ACI 318

Author(s): Hassan Baji and Hamid Reza Ronagh

Publication: Structural Journal

Volume: 113

Issue: 2

Appears on pages(s): 373-382

Keywords: beams; ductility; Monte Carlo simulation; reinforced concrete; reliability; safety factor; strength

DOI: 10.14359/51688201

Date: 3/1/2016

Abstract:
This paper presents a reliability-based investigation into the ductility requirements of reinforced concrete beams designed based on the ACI Code. Results showed that the code-specified model for predicting ductility measures, such as the neutral axis depth, is considerably less reliable than it is for predicting the flexural strength. The ratio of the strain at tensile reinforcement to yield strain of steel was used to define a limit state to ensure adequate ductility in reinforced concrete beams. Due to variability in the material properties and model error, there is high variability in ductility measures, leading to a high probability of compressive failure. Based on a target probability of failure taken from the literature, it was found that modification of the current ductility requirements is desired. This research highlights the need for more reliability-based studies into the safety factors provided by the ACI Code for ensuring adequate ductility in reinforced concrete beams.

Related References:

ACI Committee 318, 1999, “Building Code Requirements for Structural Concrete (ACI 318-99) and Commentary (ACI 318R-99),” American Concrete Institute, Farmington Hills, MI, 420 pp.

ACI Committee 318, 2011, “Building Code Requirements for Structural Concrete (ACI 318-11) and Commentary,” American Concrete Institute, Farmington Hills, MI, 503 pp.

Al-Haddad, M. S., 1995, “Curvature Ductility of RC Beams under Low and High Strain Rates,” ACI Structural Journal, V. 92, No. 5, Sept.-Oct., pp. 526-534.

Alca, N.; Alexander, S. D.; and MacGregor, J. G., 1997, “Effect of Size on Flexural Behavior of High-Strength Concrete Beams,” ACI Structural Journal, V. 94, No. 1, Jan.-Feb., pp. 59-67.

Allen, D. E., 1970, “Probabilistic Study of Reinforced Concrete in Bending,” ACI Journal Proceedings, V. 67, No. 12, Dec., pp. 989-995.

Aydemir, C., and Zorbozan, M., 2012, “Uncertainty Analysis of Flexural Overstrength Ratio for RC Columns,” Journal of Structural Engineering, ASCE, V. 138, No. 8, Aug., pp. 1042-1053. doi: 10.1061/(ASCE)ST.1943-541X.0000528

Baji, H., and Ronagh, H. R., 2013, “Reliability Analysis of Moment Redistribution in Reinforced Concrete Beams,” Magazine of Concrete Research, V. 65, No. 13, pp. 769-779. doi: 10.1680/macr.12.00147

Bartlett, F. M.; Hong, H. P.; and Zhou, W., 2003, “Load Factor Calibration for the Proposed 2005 Edition of the National Building Code of Canada: Companion-Action Load Combinations,” Canadian Journal of Civil Engineering, V. 30, No. 2, pp. 440-448. doi: 10.1139/l02-086

Bengar, H. A., and Maghsoudi, A., 2007, “Ductility of HSC Members under Bending,” Iranian Journal of Science and Technology, V. 31, No. B2, pp. 209-223.

Bernardo, L. F., and Lopes, S. M. R., 2003, “Flexural Ductility of High-Strength Concrete Beams,” Structural Concrete, V. 4, No. 3, pp. 135-154. doi: 10.1680/stco.2003.4.3.135

Bournonville, M.; Dahnke, J.; and Darwin, D., 2004, “Statistical Analysis of the Mechanical Properties and Weight of Reinforcing Bars,” SL 04-1, University of Kansas, Lawrence, KS, 194 pp.

Carmo, R.; Costa, H.; Simões, T.; Lourenço, C.; and Andrade, D., 2013, “Influence of Both Concrete Strength and Transverse Confinement on Bending Behavior of Reinforced LWAC Beams,” Engineering Structures, V. 48, pp. 329-341.

Corley, W., 1966, “Rotational Capacity of Reinforced Concrete Beams,” Journal of the Structural Division, ASCE, V. 92, No. ST5, pp. 121-146.

Costello, J. F., and Chu, K.-H., 1969, “Failure Probabilities of Reinforced Concrete Beams,” Journal of the Structural Division, ASCE, V. 95, pp. 2281-2304.

Debernardi, P. G., and Taliano, M., 2002, “On Evaluation of Rotation Capacity for Reinforced Concrete Beams,” ACI Structural Journal, V. 99, No. 3, May-June, pp. 360-368.

Ellingwood, B.; Galambos, T. V.; MacGregor, J. G.; and Cornell, C., 1980, “Development of a Probability Based Load Criteria for American Standard A 58. NBS Special Publication 577, National Bureau of Standards, Washington, DC, 238 pp.

Ho, J.; Kwan, A.; and Pam, H., 2004, “Minimum Flexural Ductility Design of High-Strength Concrete Beams,” Magazine of Concrete Research, V. 56, No. 1, pp. 13-22. doi: 10.1680/macr.2004.56.1.13

Ho, J., and Peng, J., 2011, “Strain Gradient Effects on Flexural Strength Design of Normal-Strength Concrete Columns,” Engineering Structures, V. 33, No. 1, pp. 18-31.

Hognestad, E.; Hanson, N. W.; and McHenry, D., 1955, “Concrete Stress Distribution in Ultimate Strength Design,” ACI Journal Proceedings, V. 52, No. 12, Dec., pp. 455-479.

Ibrahim, H. H. H., and Macgregor, J. G., 1996, “Flexural Behavior of Laterally Reinforced High-Strength Concrete Sections,” ACI Structural Journal, V. 93, No. 6, Nov.-Dec., pp. 674-684.

Ito, K., and Sumikama, A., 1985, “Probabilistic Study of Reduction Coefficient for Balanced Steel Ratio in the ACI Code,” ACI Journal Proceedings, V. 82, No. 5, Sept.-Oct., pp. 701-709.

Joint Committee on Structural Safety (JCSS), 2015, “Probablistic Model Code,” www.jcss.byg.dtu.dk/Publications/Probabilistic_Model_Code. (last accessed Feb. 3, 2016)

Kaar, P.; Hanson, N.; and Capell, H., 1978a, “Stress-Strain Characteristics of High Strength Concrete,” Douglas McHenry International Symposium on Concrete and Concrete Structures, V. 55, pp. 161-186.

Kaar, P. H.; Fiorato, A.; Carpenter, J.; and Corley, W., 1978b, “Limiting Strains of Concrete Confined by Rectangular Hoops,” RD053.01D, Portland Cement Association, Skokie, IL, 12 pp.

Kappos, A.; Chryssanthopoulos, M.; and Dymiotis, C., 1999, “Uncertainty Analysis of Strength and Ductility of Confined Reinforced Concrete Members,” Engineering Structures, V. 21, No. 3, pp. 195-208. doi: 10.1016/S0141-0296(97)00181-8

Khadiranaikar, R. B., and Awati, M. M., 2012, “Concrete Stress Distribution Factors for High-Performance Concrete,” Journal of Structural Engineering, ASCE, V. 138, No. 3, pp. 402-415.

Kim, J. K.; Yi, S. T.; and Kim, J. H. J., 2001, “Effect of Specimen Sizes on Flexural Compressive Strength of Concrete,” ACI Structural Journal, V. 98, No. 3, May-June, pp. 416-424.

Kim, J. K.; Yi, S. T.; and Yang, E. I., 2000, “Size Effect on Flexural Compressive Strength of Concrete Specimens,” ACI Structural Journal, V. 97, No. 2, Mar.-Apr., pp. 291-296.

Ko, M.-Y.; Kim, S.-W.; and Kim, J.-K., 2001, “Experimental Study on the Plastic Rotation Capacity of Reinforced High Strength Concrete Beams,” Materials and Structures, V. 34, No. 5, pp. 302-311.

Lee, J.-H., and Son, H.-S., 2000, “Failure and Strength of High-Strength Concrete Columns Subjected to Eccentric Loads,” ACI Structural Journal, V. 97, No. 1, Jan.-Feb., pp. 75-85.

Lin, C.-H., and Lee, F.-S., 2001, “Ductility of High-Performance Concrete Beams with High-Strength Lateral Reinforcement,” ACI Structural Journal, V. 98, No. 4, July-Aug., pp. 600-608.

Maghsoudi, A., and Sharifi, Y., 2009, “Ductility of High Strength Concrete Heavily Steel Reinforced Members,” Scientia Iranica, Transaction A, V. 16, No. 4, Aug., pp. 297-307.

MathWorks, 2014, “MATLAB and Statistics Toolbox,” The MathWorks, Inc., Natick, MA.

Mattock, A. H., 1965, “Rotational Capacity of Hinging Regions in Reinforced Concrete Beams, Proceedings of the International Symposium on the Flexural Mechanics of Reinforced Concrete, Miami, FL.

Mertol, H. C.; Rizkalla, S.; Zia, P.; and Mirmiran, A., 2008, “Characteristics of Compressive Stress Distribution in High-Strength Concrete,” ACI Structural Journal, V. 105, No. 5, Sept.-Oct., pp. 626-633.

Mirza, S. A., and MacGregor, J. G., 1979, “Variability of Mechanical Properties of Reinforcing Bars,” Journal of the Structural Division, ASCE, V. 105, No. 5, pp. 921-937.

Nedderman, W. H., 1973, “Flexural Stress Distribution in Very-High Strength Concrete,” MSc thesis, University of Texas at Arlington, Arlington, TX.

Nowak, A. S., and Collins, K. R., 2012, Reliability of Structures, CRC Press, Boca Raton, FL, 407 pp.

Nowak, A. S., and Szerszen, M. M., 2003, “Calibration of Design Code for Buildings (ACI 318): Part 1—Statistical Models for Resistance,” ACI Structural Journal, V. 100, No. 3, May-June, pp. 377-382.

Park, R., and Ruitong, D., 1988, “Ductility of Doubly Reinforced Concrete Beam Sections,” ACI Structural Journal, V. 85, No. 2, Mar.-Apr., pp. 217-225.

Pastor, J. A., 1986, “High-Strength Concrete Beams,” PhD thesis, Cornell University, Ithaca, NY.

Rusch, H., 1955, “Tests on the Strength of the Flexural Compression Zone,” N9. 120, Deutscher Ausschuss Für Stahlbeton, Berlin, Germany.

Sargin, M., and Handa, V., 1969, “A General Formulation for the Stress-Strain Properties of Concrete,” University of Waterloo, Waterloo, ON, Canada, 36 pp.

Schade, J. E., 1992, “Flexural Concrete Stress in High Strength Concrete Columns,” MSc thesis, University of Calgary, Calgary, AB, Canada.

Srikanth, M.; Kumar, G. R.; and Giri, S., 2007, “Moment Curvature of Reinforced Concrete Beams Using Various Confinement Models and Experimental Validation,” Asian Journal of Civil Egineering, V. 8, No. 3, pp. 247-265.

Swartz, S.; Nikaeen, A.; Narayan Babu, H.; Periyakaruppan, N.; and Refai, T., 1985, “Structural Bending Properties of Higher Strength Concrete,” High-Strength Concrete, SP-87, H. G. Russell, ed., American Concrete Institute, Farmington Hills, MI, pp. 147-178.

Tan, T. H., and Nguyen, N. B., 2005, “Flexural Behavior of Confined High-Strength Concrete Columns,” ACI Structural Journal, V. 102, No. 2, Mar.-Apr., pp. 198-205.

Sykora, M.; Holicky, M.; Prieto, M.; and Tanner, P., 2015, “Uncertainties in Resistance Models for Sound and Corrosion-Damaged RC Structures According to EN 1992-1-1,” Materials and Structures, V. 48, No. 10, Oct., pp. 3415-3430. doi: 10.1617/s11527-014-0409-1

Szerszen, M. M., and Nowak, A. S., 2003, “Calibration of Design Code for Buildings (ACI 318): Part 2—Reliability Analysis and Resistance Factors,” ACI Structural Journal, V. 100, No. 3, May-June, pp. 383-391.

Trezos, C., 1997, “Reliability Considerations on the Confinement of RC Columns for Ductility,” Soil Dynamics and Earthquake Engineering, V. 16, No. 1, pp. 1-8. doi: 10.1016/S0267-7261(96)00033-4

Weiss, W. J.; Guler, K.; and Shah, S. P., 2001, “Localization and Size-

Dependent Response of Reinforced Concrete Beams,” ACI Structural Journal, V. 98, No. 5, Sept.-Oct., pp. 687-695.

Yang, K.-H.; Sim, J.-I.; and Kang, T. H.-K., 2013, “Generalized Equivalent Stress Block Model Considering Varying Concrete Compressive Strength and Unit Weight,” ACI Structural Journal, V. 110, No. 5, Sept.-Oct., pp. 791-800.


ALSO AVAILABLE IN:

Electronic Structural Journal