Title: An Overview of ACI Report on High-Volume Fly Ash Concrete

Author(s): Harvey H. Haynes

Publication: Symposium Paper

Volume: 303

Issue:

Appears on pages(s): 301-310

Keywords: compressive strength; corrosion resistance; fly ash; heat of hydration; permeability; sustainability

DOI: 10.14359/51688142

Date: 6/1/2015

Abstract:
This paper summarizes a new ACI publication titled Report on High-Volume Fly Ash Concrete for Structural Applications. High-volume fly ash (HVFA) concrete is a sustainable concrete that is currently available for wide-scale usage. Technical knowledge on the material from over two decades of research and field experience are presented to provide the design and construction industry with confidence in using HVFA concrete.