Microspheres-Based Admixture for Free-Thaw Durability of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Microspheres-Based Admixture for Free-Thaw Durability of Concrete

Author(s): Frank Shaode Ong, Charles K. Nmai, James Curtis Smith, and John Luciano

Publication: Symposium Paper

Volume: 303

Issue:

Appears on pages(s): 255-268

Keywords: admixture; air entrainment; durability; freeze-thaw; high carbon fly ash; loss-on-ignition; microspheres; recovery test; sustainability

DOI: 10.14359/51688138

Date: 6/1/2015

Abstract:
The focus of this paper is a new liquid microspheres-based admixture that has been developed to provide freezing and thawing protection of cementitious-based materials under cyclic, saturated conditions, while addressing and eliminating issues typically associated with the use of surfactant-based admixtures for air entrainment. Consequently, this microspheres-based admixture provides unique opportunities and flexibility in reproportioning or optimizing current air-entrained concrete mixtures with respect to using increased levels of supplementary cementitious materials. It is also shown in the paper that the microspheres-based admixture will facilitate the use of materials that typically hinder air entrainment. A microspheres recovery test method that has been developed to measure the microspheres content of fresh content for quality assurance purposes is also presented and discussed.