Fast-Track Precast Concrete Pavements for High-Volume Roadways

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Fast-Track Precast Concrete Pavements for High-Volume Roadways

Author(s): Shiraz D. Tayabji

Publication: Web Session

Volume: Tayabji-Shiraz.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 4/13/2015

Abstract:
Heavy-duty pavements span a wide variety of uses, from truck distribution facilities, to intermodal yards, to military equipment hardstands, to high-volume interstates. These pavements can be subjected to extremely high axle loadings, millions of heavy vehicle load repetitions, high-speed truck traffic, or all of these. Designers and contractors must understand the unique requirements of these pavements, and use appropriate design tools, specification provisions, and construction techniques to properly design and build the pavements for their expected service lives. Concrete pavements are ideally suited for these applications because of their rigidity, strength, and durability. However, different types of concrete pavements, including conventional jointed pavements, roller-compacted concrete (RCC), and precast, may be optimal choices depending on the circumstances.