Database with Shear Tests on Non-Slender Reinforced Concrete Beams with Vertical Stirrups

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Database with Shear Tests on Non-Slender Reinforced Concrete Beams with Vertical Stirrups

Author(s): Leonardo Todisco, Karl-Heinz Reineck, and Oguzhan Bayrak

Publication: Structural Journal

Volume: 112

Issue: 6

Appears on pages(s): 761-769

Keywords: beams; database; reinforced concrete; shear reinforcement; shear slenderness; shear strength; shear tests; strut-and-tie models

DOI: 10.14359/51688055

Date: 11/1/2015

Abstract:
A database is presented with 278 tests on non-slender reinforced concrete beams with vertical stirrups. These beams are commonly referred to as non-slender beams because they have shear spandepth ratios (a/d) less than 2.4. In keeping with European terminology, the term “deep beams” is not used for these beams, because in Europe, deep beams are often defined only for ratios of a/d < 1 and always contain vertical as well as horizontal reinforcement in their web. After having applied several control/filtering criteria, 178 beams remained in the evaluation database that can be used to check conservativeness and accuracy of relevant design provisions. For example, the application of strut-and-tie models of ACI 318-14 to non-slender beams with stirrups (and without any horizontal skin reinforcement) was unconservative—that is, it yielded database analysis results that were above the desired 5% fractile. Almost all unconservative estimations were obtained for test specimens with very low amounts of stirrups. This problem can be solved either by increasing the required amount of minimum reinforcement in the vertical direction or by placing a minimum amount of reinforcement in both the horizontal and vertical direction. It is also important to note that a comparison with Kani’s shear valley showed that for a/d < 1, the valley was not filled up to the full flexural capacity, despite the presence of vertical stirrups in test specimens.

Related References:

ACI Committee 318, 2014, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (318R-14),” American Concrete Institute, Farmington Hills, MI, 519 pp.

Birrcher, D. B.; Tuchscherer, R. G.; Huizinga, M. R.; and Bayrak, O., 2013, “Minimum Web Reinforcement in Deep Beams,” ACI Structural Journal, V. 110, No. 2, Mar.-Apr., pp. 297-306.

Birrcher, D. B.; Tuchscherer, R. G.; Huizinga, M. R.; and Bayrak, O., 2014, “Depth Effect in Deep Beams,” ACI Structural Journal, V. 111, No. 4, July-Aug., pp. 731-740. doi: 10.14359/51687002

Birrcher, D. B.; Tuchscherer, R. G.; Huizinga, M. R.; Bayrak, O.; Wood, S. L.; and Jirsa, J. O., 2009, “Strength and Serviceability Design of Reinforced Concrete Deep Beams,” Report No. 0-5253-1, Center for Transportation Research, University of Texas at Austin, Austin, TX, Apr., 376 pp.

Brown, M. D.; Sankovich, C. L.; Bayrak, O.; Jirsa, J. O.; Breen, J. E.; and Wood, S. L., 2006, “Design for Shear in Reinforced Concrete Using Strut-and-Tie Models,” CTR Research Report 0-4371-2, Center for Transportation Research, The University of Texas at Austin, Austin, TX, Mar. 2006, 348 pp.

CEB-FIP MC 90, 1993, “Design of Concrete Structures (CEB-FIP-Model-Code 1990),” 
Thomas Telford.

EC 2, Part 1-1, 2005, “Eurocode 2: Design of Concrete Structures. Part 1.1: General Rules and Rules for Buildings,” German Version EN 1992-1-1.

fib MC, 2010, “fib Model Code for Concrete Structures 2010,” fib, Wilhelm Ernst & Sohn, Verlag für Architektur und technische Wissenschaften GmbH&Co KG, Berlin, 402 pp.

Kani, G. N. J., 1964, “The Riddle of Shear Failure and its Solution,” ACI Journal Proceedings, V. 61, No. 4, Apr., pp. 441-467.

Kani, G. N. J., 1966, “Basic Facts Concerning Shear Failure,” ACI Journal Proceedings, V. 63, No. 6, June, pp. 675-692.

Matsuo, M.; Lertsrisakulrat, T.; Yanagawa, A.; and Niwa, J., 2001, “Shear Behavior of RC Deep Beams with Stirrups,” Transactions of the Japan Concrete Institute, V. 23, pp. 385-390.

Quintero-Febres, C. G.; Parra-Montesinos, G.; and Wight, J. K., 2006, “Strength of Struts in Deep Concrete Members Designed Using Strut-and-Tie Method,” ACI Structural Journal, V. 103, No. 4, July-Aug., pp. 577-586.

FIP Recommendations, 1999, “Practical Design of Structural Concrete,” FIP-Commission 3 – Practical Design, (Distributed by: fib, Lausanne. http://www.fib-international.org).

Reineck, K.-H., ed., 2002, “Examples for the Design of Structural Concrete with Strut-and-Tie Models,” Strut-and-Tie Models, SP-208, American Concrete Institute, Farmington Hills, MI, 242 pp.

Reineck, K.-H.; Bentz, E.; Fitik, B.; Kuchma, D. A.; and Bayrak, O., 2014, “The ACI-DAfStb Database with Shear Tests on Slender Reinforced Concrete Beams with Stirrups,” ACI Structural Journal, V. 111, No. 5, Sept.-Oct., pp. 1147-1156. doi: 10.14359/51686819

Reineck, K.-H.; Kuchma, D. A.; and Fitik, B., 2010, “Extended Databases with Shear Tests on Structural Concrete Beams without and with Stirrups for the Assessment of Shear Design Procedures,” Research Report, ILEK, University of Stuttgart, Germany, and University of Illinois, Urbana, IL, July.

Reineck, K.-H.; Kuchma, D. A.; and Fitik, B., 2012, “Erweiterte Datenbanken zur Überprüfung der Querkraftbemessung von Konstruktionsbetonbauteilen ohne und mit Bügel (Extended Databases with Shear Tests on Structural Concrete Beams without and with Stirrups for Assessing Shear Design Procedures),” DAfStb H. 597. Beuth Verl. Berlin. (in German)

Reineck, K.-H.; Kuchma, D. A.; Kim, K. S.; and Marx, S., 2003, “Shear Database for Reinforced Concrete Members without Shear Reinforcement,” ACI Structural Journal, V. 100, No. 2, Mar.-Apr., pp. 240-249. (discussion in ACI Structural Journal, V. 101, No. 1, pp. 139-144).

Reineck, K.-H., and Novak, L. C., eds., 2011, Further Examples for the Design of Structural Concrete with Strut-and-Tie Models, SP-273, American Concrete Institute, Farmington Hills, MI, 288 pp.

Reineck, K.-H., and Todisco, L., 2014, “Database of Shear Tests for Non-Slender Reinforced Concrete Beams without Stirrups,” ACI Structural Journal, V. 111, No. 6, Nov.-Dec., pp. 1363-1371. doi: 10.14359/51686820

Russo, G.; Venir, R.; and Pauletta, M., 2005, “Reinforced Concrete Deep Beams—Shear Strength Model and Design Formula,” ACI Structural Journal, V. 102, No. 3, May-June, pp. 429-437.

Albajar, J. S., 2008, “The Influence of Aggregate Fracture on the Shear Strength of Reinforced Concrete Beams,” thesis, Department of Civil & Environmental Engineering of the University of London, Imperial College, London, UK, 409 pp.

Todisco, L., 2011, “Test Evidence for Applying Strut-and-Tie Models to Deep Beams and D-Regions of Beams,” master’s degree thesis, Technical University of Bari, Bari, Italy, Oct.

Todisco, L.; Reineck, K.-H.; and Bayrak, O., 2015, “Report Part 6.2 – ACI-DAfStb Shear Database with Shear Tests on Non-Slender R.-C. Beams with Stirrups Subjected to Point Loads,” ACI-DAfStb Databases 2015 on Shear Tests for Evaluating Relationships for the Shear Design of Structural Concrete Members without and with Stirrups, K.-H. Reineck and D. Dunkelberg, eds.

Tuchscherer, R. G.; Birrcher, D. B.; Huizinga, M. R.; and Bayrak, O., 2010, “Confinement of Deep Beam Nodal Regions,” ACI Structural Journal, V. 107, No. 6, Nov.-Dec., pp. 709-717.

Tuchscherer, R. G.; Birrcher, D. B.; Huizinga, M. R.; and Bayrak, O., 2011, “Distribution of Stirrups across Web of Deep Beams,” ACI Structural Journal, V. 108, No. 1, Jan.-Feb., pp. 108-115.

Wight, J. K., and Parra-Montesinos, G., 2003, “Use of Strut and Tie Model for Deep Beam Design as Per ACI 318 Code,” Concrete International, V. 25, No. 5, May, pp. 63-70.

Zhang, N., and Tan, K.-H., 2007, “Size Effect in RC Deep Beams: Experimental Investigation and STM Verification,” Engineering Structures, V. 29, No. 12, pp. 3241-3254. doi: 10.1016/j.engstruct.2007.10.005