Title: 364.3T-15 Treatment of Exposed Epoxy-Coated Reinforcement in Repair

Author(s): ACI Committee 364

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s):

Keywords: coating; corrosion; corrosion inhibitor; electrical resistance; epoxy-coated; reinforcing bars; reinforcing steel; repair; ring anode effect; sacrificial anode

DOI:

Date: 6/1/2015

Abstract:
This document outlines the treatment and repair of concrete areas containing epoxy-coated reinforcing steel when epoxy-coated reinforcing steel is exposed in a repair area.