Behavior of Deep Beams Containing High-Strength Longitudinal Reinforcement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior of Deep Beams Containing High-Strength Longitudinal Reinforcement

Author(s): Juan de Dios Garay-Moran and Adam S. Lubell

Publication: Structural Journal

Volume: 113

Issue: 1

Appears on pages(s): 17-28

Keywords: deep beams; high-strength reinforcement; one-way shear; reinforced concrete; safety; shear reinforcement; strut-and-tie

DOI: 10.14359/51687910

Date: 1/1/2016

Abstract:
Steel reinforcing bars conforming to ASTM A1035 have enhanced corrosion resistance and significantly higher tensile strength compared to conventional reinforcing steel grades. However, the impact of the unique stress-strain characteristics of this steel on the failure modes and strength prediction models is not yet fully understood. This paper reports on the laboratory testing to failure of eight large-scale specimens having small shear span to effective depth ratios and containing or omitting web reinforcement. All specimens were longitudinally reinforced with deformed A1035 steel bars with measured stresses at the peak load from 695 to 988 MPa (100 to 143 ksi)—significantly higher than the design stress limits defined in current codes of practice. Members without web reinforcement failed in a brittle manner after the formation of diagonal cracks joining the loads and supports. For members containing web reinforcement, the shear span to effective depth ratio and the longitudinal reinforcement ratio were both found to influence the failure mode and post-peak ductility. It was possible to develop designs that could exploit the high reinforcement strength while exhibiting acceptable serviceability characteristics and adequate ductility at failure. The safety of capacity predictions using ACI ITG-6R-10 provisions is presented.

Related References:

1. ASTM A1035-11, “Standard Specification for Deformed and Plain, Low Carbon, Chromium, Steel Bars for Concrete Reinforcement,” ASTM International, West Conshohocken, PA, 2011, 5 pp.

2. El-Hacha, R., and Rizkalla, S. H., “Fundamental Material Properties of MMFX Steel Bars,” Research Report RD-02/04, Constructed Facilities Lab, North Carolina State University, Raleigh, NC, July 2002, 62 pp.

3. Darwin, D.; Browning, J.; Nguyen, T. V.; and Locke, C., “Mechanical and Corrosion Properties of a High-Strength, High Chromium Reinforcing Steel for Concrete,” SM Report No. 66, University of Kansas, Lawrence, KS, 2002, 106 pp.

4. ASTM A615-06, “Standard Specification for Deformed and Plain Carbon-Steel Bars for Concrete Reinforcement,” ASTM International, West Conshohocken, PA, 2006, 6 pp.

5. ASTM A706, “Standard Specification for Low-Alloy Steel Deformed and Plain Bars for Concrete Reinforcement,” ASTM International, West Conshohocken, PA, 2008, 6 pp.

6. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-11) and Commentary,” American Concrete Institute, Farmington Hills, MI, 2011, 465 pp.

7. CSA A23.3-04, “Design of Concrete Structures (CAN/CSA A23.3-04),” Canadian Standards Association, Mississauga, ON, Canada, 2004.

8. AASHTO, “AASHTO LRFD Bridge Design Specifications and Commentary,” third ddition, American Association of State Highway Transportation Officials, Washington, DC, 2004, 1264 pp.

9. ACI Innovation Task Group 6, “Design Guide for the Use of ASTM A1035/A1035M Grade 100 (690) Steel Bars for Structural Concrete (ACI ITG-6R-10),” American Concrete Institute, Farmington Hills, MI, 2010, 90 pp.

10. Kani, M. W.; Huggins, M. W.; and Witkopp, R. R., Kani on Shear in Reinforced Concrete, University of Toronto Press, Toronto, ON, Canada, 1979, 224 pp.

11. Leonhardt, F., and Walther, R., “The Stuttgart Shear Tests 1961,” Translation No. 111, Cement and Concrete Association, London, UK, 1964, 134 pp.

12. MacGregor, J. G., and Wight, J. K., Reinforced Concrete Mechanics and Design, fourth edition, Prentice Hall, Upper Saddle River, NJ, 2004, 1132 pp.

13. Malhas, A.F., “Preliminary Experimental Investigation of the Flexural Behaviour of Reinforced Concrete Beams Using MMFX Steel,” MMFX Steel Corporation: Technical Resources, July 2002, 55 pp.

14. Vijay, P. V.; Gangarao, V. S.; and Parchasaree, W., “Bending Behaviour of Concrete Beams Reinforced with MMFX Steel bars,” MMFX Steel Corporation: Technical Resources, July 2002, 33 pp.

15. Desalegne, A. S., and Lubell, A. S., “Shear Behavior of Concrete Slabs Longitudinally Reinforced with High-Performance Steel,” ACI Structural Journal, V. 107, No. 2, Mar.-Apr. 2010, pp. 228-236.

16. Lubell, A. S.; Bentz, E. C.; and Collins, M. P., “Influence of Longitudinal Reinforcement on One-Way Shear in Slabs and Wide Beams,” Journal of Structural Engineering, ASCE, V. 135, No. 1, 2009, pp. 78-87. doi: 10.1061/(ASCE)0733-9445(2009)135:1(78)

17. Hassan, T. K.; Seliem, H. M.; Dwairi, H.; Rizkalla, S. H.; and Zia, P., “Shear Behavior of Large Concrete Beams Reinforced with High-Strength Steel,” ACI Structural Journal, V. 105, No. 2, Mar.-Apr. 2008, pp. 173-179.

18. Sumpter, M.; Rizkalla, S. H.; and Zia, P., “Behavior of High Performance Steel as Shear Reinforcement for Concrete Beams,” ACI Structural Journal, V. 106, No. 2, Mar.-Apr. 2009, pp. 171-177.

19. Collins, M. P., and Kuchma, D., “How Safe Are Our Large, Lightly Reinforced, Concrete Beams, Slabs and Footings?” ACI Structural Journal, V. 96, No. 4, July-Aug. 1999, pp. 482-490.

20. Adebar, P., and Zhou, Z., “Bearing Strength of Compressive Struts Confined by Plain Concrete,” ACI Structural Journal, V. 90, No. 5, Sept.-Oct. 1993, pp. 534-541.

21. Tan, K. H., and Cheng, G. H., “Size Effect on Shear Strength of Deep Beams: Investigating with Strut-and-Tie Models,” Journal of Structural Engineering, ASCE, V. 132, No. 5, 2006, pp. 673-685. doi: 10.1061/(ASCE)0733-9445(2006)132:5(673)

22. Garay-Moran, J.-D., and Lubell, A. S., “Behaviour of Concrete Deep Beams with High Strength Reinforcement,” SER No. 277, Department of Civil and Environmental Engineering, University of Alberta, Edmonton, AB, Canada, 2008, 283 pp.

23. Desalegne, A. S., and Lubell, A. S., “Shear in Concrete Beams Reinforced with High-Performance Steel,” ACI Structural Journal, V. 112, No. 6, Nov.-Dec. 2015, pp. 783-792. doi: 10.14359/51687798

24. Walraven, J., and Lehwalter, N., “Size Effects in Short Beams Loaded in Shear,” ACI Structural Journal, V. 91, No. 5, Sept.-Oct. 1994, pp. 585-593.

25. CSA G30.18-09. “Carbon Steel Bars for Concrete Reinforcement (CAN/CSA G30.18),” Canadian Standards Association, Mississauga, ON, Canada, 2009, 28 pp.

26. Aguilar, G.; Matamoros, A. B.; Parra-Montesinos, G. J.; Ramirez, J. A.; and Wight, J. K., “Experimental Evaluation of Design Procedures for Shear Strength of Deep Reinforced Concrete Beams,” ACI Structural Journal, V. 99, No. 4, July-Aug. 2002, pp. 539-548.

27. Oh, J. K., and Shin, S. W., “Shear Strength of Reinforced High-Strength Concrete Deep Beams,” ACI Structural Journal, V. 98, No. 2, Mar.-Apr. 2001, pp. 164-173.

28. Tan, K. H., and Lu, H. Y., “Shear Behavior of Large Reinforced Concrete Deep Beams and Code Comparisons,” ACI Structural Journal, V. 96, No. 5, Sept.-Oct. 1999, pp. 836-845.

29. ACI Committee 440, “Guide for the Design and Construction of Structural Concrete Reinforced with FRP Bars (ACI 440.1R-06),” American Concrete Institute, Farmington Hills, MI, 2006, 44 pp.


ALSO AVAILABLE IN:

Electronic Structural Journal