Title: Experimental Investigation of Prestress Losses in Full-Scale Bridge Girders

Author(s): David B. Garber, José M. Gallardo, Dean J. Deschenes, and Oguzhan Bayrak

Publication: Structural Journal

Volume: 112

Issue: 5

Appears on pages(s): 553-564

Keywords: prestress loss; prestressed bridge girder; pretensioned concrete

DOI: 10.14359/51687909

Date: 9/1/2015

Abstract:
An experimental study was conducted in which 30 full-scale, precast, pretensioned bridge girders were constructed and instrumented with the intention of investigating prestress loss. Several different precast beam fabrication plants were used to investigate the influence of different concrete materials and construction techniques. The constructed girders were conditioned in several different climates for up to 3 years. During this period, prestress loss was measured by using vibrating wire gauges (VWG) embedded in test specimens. Following the conditioning period, the girders were flexural service load-tested to quantify the prestress loss at the time of testing and in turn verify the losses measured using VWGs. Prestress losses were found to be heavily influenced by concrete stiffness, which was dependent on coarse aggregate type and quantity. The measured short- and long-term prestress losses were compared to those determined using several different estimation procedures, suggested by ACI Committee 423.

Related References:

1. Gallardo Méndez, J. M., “Model of Strain-Related Prestress Loss in Pretensioned Simply Supported Bridge Girders,” PhD dissertation, the University of Texas at Austin, Austin, TX, 2013, 330 pp.

2. Garber, D.; Gallardo, J.; Deschenes, D.; Dunkman, D.; and Bayrak, O., “Effect of New Prestress Loss Estimates on Pretensioned Concrete Bridge Girder Design,” Report No. FHWA/TX-12/0-6374-2, Center for Transportation Research, the University of Texas at Austin, Austin, TX, 2013, 300 pp.

3. Neville, A. M.; Dilger, W. H.; and Brooks, J. J., Creep of Plain and Structural Concrete, Construction Press, 1983, 380 pp.

4. Tadros, M. K.; Al-Omaishi, N.; Seguirant, S. J.; and Gallt, J. G., “Prestress Losses in Pretensioned High-Strength Concrete Bridge Girders,” NCHRP Report 496, Transportation Research Board, Washington, DC, 2003, 73 pp.

5. Bažant, Z. P., and Wittmann, F. H., Creep and Shrinkage in Concrete Structures, Wiley & Sons, New York, 1982.

6. Juenger, M. C. G., and Jennings, H. M., “Examining the Relationship between the Microstructure of Calcium Silicate Hydrate and Drying Shrinkage of Cement Pastes,” Cement and Concrete Research, V. 32, No. 2, 2002, pp. 289-296. doi: 10.1016/S0008-8846(01)00673-1

7. Mindess, S.; Young, J.; and Darwin, D., Concrete, Prentice Hall, Upper Saddle River, NJ, 2002, 644 pp.

8. Powers, T., “The Thermodynamics of Volume Change and Creep,” Matériaux et Construction, V. 1, No. 6, 1968, pp. 487-507. doi: 10.1007/BF02473638

9. Tazawa, E. I.; Sato, R.; Sakai, E.; and Miyazawa, S., “Work of JCI Committee on Autogenous Shrinkage,” International RILEM Workshop on Shrinkage of Concrete (Shrinkage 2000), V. Baroghel-Bouny and P.-C. Aïtcin, eds., RILEM, Bagneux, France, 2000, pp. 21-40.

10. Bažant, Z. P.; Hauggaard, A. B.; Baweja, S.; and Ulm, F.-J., “Microprestress-Solidification Theory for Concrete Creep. I: Aging and Drying Effects,” Journal of Engineering Mechanics, V. 123, No. 11, 1997, pp. 1188-1194. doi: 10.1061/(ASCE)0733-9399(1997)123:11(1188)

11. Hansen, T. C.; Radjy, F.; and Sellevold, E. J., “Cement Paste and Concrete,” Annual Review of Materials Science, V. 3, No. 1, 1973, pp. 233-268. doi: 10.1146/annurev.ms.03.080173.001313

12. Ulm, F.; Le Maou, F.; and Boulay, C., “Creep and Shrinkage of Concrete—Kinetics Approach,” The Adam Neville Symposium: Creep and Shrinkage—Structural Design Effects, SP-194, A. Al-Manaseer, ed., American Concrete Institute, Farmington Hills, MI, 2000, pp. 135-154.

13. Vandamme, M., and Ulm, F.-J., “Nanogranular Origin of Concrete Creep,” Proceedings of the National Academy of Sciences of the United States of America, V. 106, No. 26, 2009, pp. 10552-10557. doi: 10.1073/pnas.0901033106

14. Magura, D. D.; Sozen, M. A.; and Siess, C. P., “A Study of Stress Relaxation in Prestressing Reinforcement,” Civil Engineering Studies SRS-237, University of Illinois, Urbana, IL, 1962, 116 pp.

15. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary,” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

16. Birrcher, D. B.; Bayrak, O.; and Kreger, M. E., “Effects of Increasing Allowable Compressive Stress at Prestress Transfer,” ACI Structural Journal, V. 107, No. 1, Jan.-Feb. 2010, pp. 21-31.

17. TxDOT, “Standard Specification for Construction and Maintenance of Highways, Streets, and Bridges,” Texas Department of Transportation, Austin, TX, 2012.

18. AASHTO, “AASHTO LRFD Bridge Design Specification, Customary U.S. Units, 6th Edition,” American Association of State Highway and Transportation Officials, Washington, DC, 2012, 1925 pp.

19. Brooks, J., “30-Year Creep and Shrinkage of Concrete,” Magazine of Concrete Research, V. 57, No. 9, 2005, pp. 545-556. doi: 10.1680/macr.2005.57.9.545

20. Mokhtarzadeh, A., and French, C., “Time-Dependent Properties of High-Strength Concrete with Consideration for Precast Applications,” ACI Materials Journal, V. 97, No. 3, May-June 2000, pp. 263-271.

21. PCI, PCI Design Handbook, seventh edition, Precast and Prestressed Concrete Institute, Chicago, IL, 2010, 804 pp.


ALSO AVAILABLE IN:

Electronic Structural Journal