Construction of Undulating Walls Using Dry-Mix Shotcrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Construction of Undulating Walls Using Dry-Mix Shotcrete

Author(s): Jasiczak, J.; Majchrzak, W.; and Czajka, W.,

Publication: Concrete International

Volume: 37

Issue: 6

Appears on pages(s): 31-35

Keywords: shell, anchorage, concrete, joint

DOI: 10.14359/51687879

Date: 6/1/2015

Abstract:
The undulating walls at the entry hall of the Museum of History of Polish Jews in Warsaw, Poland, were constructed using a stay-in-place form and the dry-mix shotcrete process. To avoid cracking of the walls, a support system was designed to distribute and disperse stresses from the anchorage points into the wall sections. To maintain a uniform thickness of shotcrete and delineate the outer surface, specially designed polymers strips were embedded in expansion and control joints. The strips also enabled installation of plastic sheets to prevent moisture loss and provided protection against shotcrete overspray during construction of adjacent elements.

Related References:

1. Czajka, W., “The Museum of the History of Polish Jews,” Shotcrete, V. 15, No. 1, Winter 2013, pp. 12-17.