Modeling and Forming the Turkish American Community Center

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Modeling and Forming the Turkish American Community Center

Author(s): Kenneth Graff and Scott Hover

Publication: Concrete International

Volume: 37

Issue: 6

Appears on pages(s): 26-30

Keywords: concrete, mockup, shoring, reinforcing

DOI: 10.14359/51687878

Date: 6/1/2015

Abstract:
The Turkish American Community Center (TACC) in Lanham, MD, is a reinforced concrete structure comprising a mosque, Turkish bath, parking structure, and additional assembly spaces. A three -dimensional model of the structure was prepared to allow for detailed coordination of the concrete work on the project as well as resolution of potential constructibility issues. The model was provided to the general contractor and the formwork vendors. The five forming systems that were ultimately required to construct the project are briefly described.