211.7R-15: Guide for Proportioning Concrete Mixtures with Ground Limestone and Other Mineral Fillers

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 211.7R-15: Guide for Proportioning Concrete Mixtures with Ground Limestone and Other Mineral Fillers

Author(s): ACI Committee 211

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 14

Keywords: dust-of-fracture; ground limestone; mineral fillers; mixture proportioning; paste volume; powder content; proportioning.

DOI:

Date: 4/29/2015

Abstract:
The use of ground limestone and other mineral fillers can enhance the performance, economy, and sustainability of concrete mixtures. Modifications to the conventional proportioning method in ACI 211.1 are needed to incorporate these materials. This document describes ground limestone and other mineral fillers, including their properties, characterization, and qualification, and effects on concrete properties and sustainability. Recommendations are provided for proportioning concrete mixtures with these materials.