SP-300: Fracture Mechanics Applications in Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: SP-300: Fracture Mechanics Applications in Concrete

Author(s):

Publication: Symposium Paper

Volume: 300

Issue:

Appears on pages(s): 246

Keywords:

DOI: 10.14359/51687812

Date: 3/11/2015

Abstract:

Editor: Christian Gaedicke

This CD contains 10 papers that were presented during a session sponsored by ACI technical committee 446 at the Spring Convention in 2012 in Phoenix, AZ. The papers focus on the implementation of fracture mechanics techniques in fiber-reinforced concrete, fiber-reinforced polymers, bonding, large structures, beam shear, pavements, and concrete deterioration. Where applicable, the papers compare modeling results with experimental tests.

Note: The individual papers are also available. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP-300