327R-14: Guide to Roller-Compacted Concrete Pavements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 327R-14: Guide to Roller-Compacted Concrete Pavements

Author(s): ACI Committee 327

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 51

Keywords: industrial pavement; inspection and testing; joints; pavement; pavement design; roller-compacted concrete (RCC); RCC mixture proportioning; RCC pavement construction; RCC production

DOI:

Date: 3/2/2015

Abstract:
This guide provides owner-agencies, contractors, materials suppliers, and others with a thorough introduction to roller-compacted concrete (RCC) and its many paving applications. This guide describes RCC and how it works as a paving material, how it compares to concrete pavement, its common uses and benefits, and potential limitations compared to other paving materials. Troubleshooting guidelines are provided, as well as detailed overviews of RCC properties and materials, mixture proportioning, structural design issues, production and construction considerations, and quality control.