Title:
Reinforced Concrete in Motion: A Retrospective of Developments on Knowledge Related to Flexural Response of Reinforced Concrete
Author(s):
Mete A. Sozen
Publication:
Web Session
Volume:
Issue:
Appears on pages(s):
Keywords:
DOI:
Date:
10/27/2014
Abstract:
This session is aimed at disseminating information related to past and current research on behavior of reinforced concrete flexural members and walls, as well as on structural collapse.