Discussions from the May-June 2014 ACI Structural Journal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Discussions from the May-June 2014 ACI Structural Journal

Author(s): José R. Martí-Vargas; W. L. Gamble; José R. Martí-Vargas; and Bhupinder Singh

Publication: Structural Journal

Volume: 112

Issue: 2

Appears on pages(s): 233-240

Keywords:

DOI: 10.14359/51687759

Date: 3/1/2015

Abstract:
Disc. 111-S41/From the May-June 2014 ACI Structural Journal, p. 503 Bond-Slip-Strain Relationship in Transfer Zone of Pretensioned Concrete Elements. Paper by Ho Park and Jae-Yeol Cho; Disc. 111-S44/From the May-June 2014 ACI Structural Journal, p. 537 Fire Protection for Beams with Fiber-Reinforced Polymer Flexural Strengthening Systems. Paper by Nabil Grace and Mena Bebawy; Disc. 111-S45/From the May-June 2014 ACI Structural Journal, p. 549 Analysis and Prediction of Transfer Length in Pretensioned, Prestressed Concrete Members. Paper by Byung Hwan Oh, Si N. Lim, Myung K. Lee, and Sung W. Yoo; and Disc. 111-S50/From the May-June 2014 ACI Structural Journal, p. 607 Flexural Testing of Reinforced Concrete Beams with Recycled Concrete Aggregates. Paper by Thomas H.-K. Kang, Woosuk Kim, Yoon-Keun Kwak, and Sung-Gul Hong