Discussion from the March/April 2014 ACI Materials Journal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Discussion from the March/April 2014 ACI Materials Journal

Author(s): José R. Martí-Vargas

Publication: Materials Journal

Volume: 112

Issue: 1

Appears on pages(s): 173-176

Keywords:

DOI: 10.14359/51687690

Date: 1/1/2015

Abstract:
Disc. 111-M11/From the March-April 2014 ACI Materials Journal, p. 123 Practical Approach for Assessing Lightweight Aggregate Potential for Concrete Performance. Paper by Daniel Moreno, Patricia Martinez, and Mauricio Lopez; Disc. 111-M14/From the March-April 2014 ACI Materials Journal, p. 153 Effect of Misalignment on Pulloff Test Results: Numerical and Experimental Assessments. Paper by L. Courard, B. Bissonnette, A. Garbacz, A. Vaysburd, K. von Fay, G. Moczulski, and M. Morency;


ALSO AVAILABLE IN:

Electronic Materials Journal