Mechanism of Nucleation and Growth of Passive Film on Steel Reinforcing Bar at Different Durations of its Exposure in Concrete Pore Solution at Nanoscale

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Mechanism of Nucleation and Growth of Passive Film on Steel Reinforcing Bar at Different Durations of its Exposure in Concrete Pore Solution at Nanoscale

Author(s): R. R. Hussain, A. Alhozaimy, A. Al Negheimish, R. Al-Zaid, and D. D. N. Singh

Publication: Materials Journal

Volume: 112

Issue: 4

Appears on pages(s): 523-534

Keywords: corrosion; nanotechnology; passive layer; reinforcing bars

DOI: 10.14359/51687662

Date: 7/1/2015

Abstract:
The nanoscale passive film formation on steel reinforcing bars at different stages of their exposure in concrete pore solution is characterized by the application of atomic force microscopy, Raman spectroscopy, electrochemical impedance spectroscopy, electrochemical noise, and cyclic voltametry studies. Based on this, a new description of the sequence of reactions during the formation of passive film on steel reinforcing bars is suggested in this paper. The results generated during this investigation revealed that the surface of the steel reinforcing bars prior to their embedding in a concrete pore solution remain covered with a film of ferric hydroxide (Fe(OH)3). The passive film on the reinforcing bars is formed by the dissolution of this oxide film followed by a series of chemical reactions. The nanotechnological investigations conducted in this paper indicated that a protective passive film on a reinforcing bar’s surface develops within 24 hours of its exposure to the concrete pore solution. Further exposure helps growth of the film over a period of up to 7 days. Beyond this period of exposure, no significant changes in either the structure or the protective property of the film are recorded. In solid concrete, however, the film formation and its growth is slow compared with the concrete pore solution, and a minimum period of 20 days is needed to form a complete protective film on the reinforcing bars embedded in concrete.

Related References:

1. Neville, A. M., Properties of Concrete, fifth edition, Prentice Hall, Upper Saddle River, NJ, 2012, 872 pp.

2. Bensted, J., “Hydration of Portland Cement,” Chemistry of Cement, second edition, S. Sakethraman, ed., Publishing Tech Book International, New Delhi, 2002, pp. 31-86.

3. Röβler, M., and Odler, I., “Investigation on the Relationship between Porosity, Structure and Strength of Hydrated Portland Cement Pastes I. Effect of Porosity,” Cement and Concrete Research, V. 15, No. 2, 1985, pp. 320-330. doi: 10.1016/0008-8846(85)90044-4

4. Diamond, S., and Gomez-Toledo, C., “Consistency, Setting, and Strength Gain Characteristics of a ‘Low Porosity’ Portland Cement Paste,” Cement and Concrete Research, V. 8, No. 5, 1978, pp. 613-621. doi: 10.1016/0008-8846(78)90044-3

5. Nieuwoudt, M. K.; Comins, J. D.; and Cukrowski, I., “The Growth of the Passive Film on Iron in 0.05M NaOH Studied In Situ by Raman Micro Spectroscopy and Electrochemical Polarization. Part II: In Situ Raman Spectra of the Passive Film Surface during Growth by Electrochemical Polarization,” Journal of Raman Spectroscopy, V. 42, No. 6, 2011, pp. 1353-1365. doi: 10.1002/jrs.2842

6. Godech, R. F.; Petek, A.; and Dolecek, V., “Nucleation and Growth of Passive Film on AISI 420 Martensitic Stainless Steel under Potentiostatic Conditions,” Acta Chimica Slovenica, V. 49, 2002, pp. 139-148.

7. Marcotte, T. D., and Hansson, C. M., “The Interface of Silica Fume on the Corrosion Resistance of Steel in High Performance Concrete Exposed to Simulated Sea Water,” Journal of Materials Science, V. 38, No. 23, 2003, pp. 4765-4776. doi: 10.1023/A:1027431203746

8. Deng, H.; Ishikawa, I.; Yoneya, M.; and Nanjo, H., “Reconstruction in Air of an Iron Passive Film Formed at –0.4V in a Borate Buffer Solution,” The Journal of Physical Chemistry B, V. 108, No. 26, 2004, pp. 9138-9146. doi: 10.1021/jp0376673

9. Diez-Perez, I.; Sanz, F.; and Gorostiza, P., “In Situ Studies of Metal Passive Films,” Current Opinion in Solid State and Materials Science, V. 10, No. 3-4, 2006, pp. 144-152. doi: 10.1016/j.cossms.2007.01.002

10. Nieuwoudt, M. K.; Comins, J. D.; and Cukrowski, I., “The Growth of the Passive Film on Iron in 0.05 M NaOH Studied In Situ by Raman Micro-spectroscopy and Electrochemical Polarization. Part II: Near Resonance Enhancement of the Raman Spectra of Iron Oxide and Hydroxide Compounds,” Journal of Raman Spectroscopy, V. 42, No. 6, 2011, pp. 1335-1339. doi: 10.1002/jrs.2837

11. Stramann, M., and Müller, J., “Mechanism of the Oxygen Reduction on Rust-Covered Metal Substrate,” Corrosion Science, V. 36, No. 2, 1994, pp. 327-359. doi: 10.1016/0010-938X(94)90161-9

12. Ramirez, C. W.; Borgard, B.; Jones, D.; and Heidersbach, R., Dec. “Laboratory Simulation of Corrosion in Reinforced Concrete,” Materials Performance, V. 29, No. 12, 1990, pp. 33-42.

13. Valdez, B.; Rosas, N.; and Sempedro, J. A., “Chapter 1: Case and Laboratory Studies,” Corrosion of Steel Reinforcement in Concrete Water, P. Castro, O. Trocnois, and C. Andrade, eds., NACE International Book Publications, 1998, pp. 51-54.

14. Al-Negheimish, A.; Alhozaimy, A.; Hussain, R. R.; Al-Zaid, R.; Singh, J. K.; and Singh, D. D. N., “The Role of Manganese Sulfide Inclusions in Steel Rebar in the Formation and Breakdown of Passive Films in Concrete Pore Solutions,” Corrosion Journal, V. 70, No. 1, 2014, pp. 74-86. doi: 10.5006/0941

15. Alhozaimy, A.; Hussain, R. R.; Al-Negheimish, A.; Al-Zaid, R.; and Singh, D. D. N., “Effect of Simulated Concrete Pore Solution Chemistry, Chloride Ions, and Temperature on the Passive Layer Formed on Steel Reinforcement,” ACI Materials Journal, V. 111, No. 4, July-Aug. 2014, pp. 411-421.

16. Li, Y.; Wu, J.; Zhang, D.; Wang, Y.; and Hou, B., “The Electrochemical Reduction Reaction of Dissolved Oxygen on Q235 Carbon Steel in Alkaline Solution Containing Chloride Ions,” Journal of Solid State Electrochemistry, V. 14, No. 9, 2010, pp. 1667-1673. doi: 10.1007/s10008-009-0997-9

17. Veleva, L.; Alpuche-Aviles, M. A.; Graves-Brook, M. K.; and Wipf, D. O., “Comparative Cyclic Voltammetry and Surface Analysis of Passive Films Grown on Stainless Steel 316 in Concrete Pore Model Solutions,” Journal of Electroanalytical Chemistry, V. 537, No. 1-2, 2002, pp. 85-93. doi: 10.1016/S0022-0728(02)01253-6

18. Kuroda, K.; Cahan, B. D.; Nazri, G. H.; Yeager, E.; and Mitchel, T. E., “Electron Diffraction Study of the Passive Film on Iron,” Journal of the Electrochemical Society, V. 129, No. 10, 1982, pp. 2163-2169. doi: 10.1149/1.2123468

19. Cox, B., and Wong, Y. M., “Simulating Porous Oxide Films on Zirconium Alloys,” Journal of Nuclear Materials, V. 218, No. 3, 1995, pp. 324-334. doi: 10.1016/0022-3115(94)00653-9

20. ASTM C876-09, “Standard Test Method for Corrosion Potentials of Uncoated Reinforcing Steel in Concrete,” ASTM International, West Conshohocken, PA, 2009, 7 pp.

21. Gan, W. Z.; Jin, W. L.; and Shao, J. P., “The Electrochemical Characterization of Rebar Passivation Film in Simulated Concrete Media,” Advanced Material Research, V. 255, 2011, pp. 539-545. doi: 10.4028/www.scientific.net/AMR.255-260.539

22. Tamura, H., “The Role of Rusts in Corrosion and Corrosion Protection of Iron and Steel,” http://eprints.lib.hokudai.ac.jp/dspace/bitstream/2115/34142/1/tamura.pdf. (last accessed June 8, 2015)