Modeling of Near-Surface-Mounted Carbon Fiber-Reinforced Polymer for Strengthening Reinforced Concrete Beams in Sustained Load

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Modeling of Near-Surface-Mounted Carbon Fiber-Reinforced Polymer for Strengthening Reinforced Concrete Beams in Sustained Load

Author(s): Yail J. Kim

Publication: Structural Journal

Volume: 112

Issue: 6

Appears on pages(s): 805-813

Keywords: carbon fiber-reinforced polymer (CFRP); long-term; modeling; near-surface-mounted (NSM); strengthening; sustained load

DOI: 10.14359/51687659

Date: 11/1/2015

Abstract:
This paper presents a theoretical model for predicting the longterm behavior of near-surface-mounted (NSM) carbon fiber reinforced polymer (CFRP) strips embedded in a reinforced concrete beam subjected to creep-induced distress. The concept of age-adjusted effective properties is employed, including timedependent material characteristics. Upon validation of the modeling approach using a previously conducted test program, a parametric investigation is performed to examine the effect of various material parameters such as concrete strength, CFRP modulus, and reinforcement ratio. A design proposal is made to facilitate NSM CFRP technologies for practical strengthening application. Four design categories are suggested depending on the level of sustained load. The proposed long-term design factors are in conformance with the time-dependent multipliers of ACI 318-11.

Related References:

1. Hollaway, L. C., “A Review of the Present and Future Utilisation of FRP Composites in the Civil Infrastructure with Reference to Their Important In-Service Properties,” Construction and Building Materials, V. 24, No. 12, 2010, pp. 2419-2445. doi: 10.1016/j.conbuildmat.2010.04.062

2. ACI Committee 440, “Guide for the Design and Construction of Externally Bonded FRP Systems for Strengthening Concrete Structures (ACI 440.2R-08),” American Concrete Institute, Farmington Hills, MI, 2008, 76 pp.

3. Plevris, N., and Triantafillou, T. C., “Time-Dependent Behavior of RC Members Strengthened with FRP Laminates,” Journal of Structural Engineering, ASCE, V. 120, No. 3, 1994, pp. 1016-1042. doi: 10.1061/(ASCE)0733-9445(1994)120:3(1016)

4. Tan, K. H., and Saha, M. K., “Long-Term Deflections of Reinforced Concrete Beams Externally Bonded with FRP System,” Journal of Composites for Construction, ASCE, V. 10, No. 6, 2006, pp. 474-482. doi: 10.1061/(ASCE)1090-0268(2006)10:6(474)

5. Sobuz, H. R.; Ahmed, E.; Sutan, N. M.; Hasan, N. M. S.; Uddin, M. A.; and Uddin, M. J., “Bending and Time-Dependent Responses of RC Beams Strengthened with Bonded Carbon Fiber Composite Laminates,” Construction and Building Materials, V. 29, 2012, pp. 597-611. doi: 10.1016/j.conbuildmat.2011.11.006

6. Gilbert, R. I., “Time-Dependent Analysis of Composite Steel-Concrete Sections,” Journal of Structural Engineering, ASCE, V. 115, No. 11, 1989, pp. 2687-2705. doi: 10.1061/(ASCE)0733-9445(1989)115:11(2687)

7. Elbadry, M. M.; Youkim, S. A.; and Ghali, A., “Model Analysis of Time-Dependent Stresses and Deformations of Structural Concrete,” Progress in Structural Engineering and Materials, V. 5, No. 3, 2003, pp. 153-166. doi: 10.1002/pse.148

8. Kim, Y. J., and Khan, F., “Creep-Induced Distress on Flexural Behavior of Reinforced Concrete Beams Retrofitted with Near-Surface-Mounted Carbon Fiber-Reinforced Polymer,” ACI Structural Journal, V. 112, No. 4, July-Aug. 2015, pp. 493-503.

9. Hughes Brothers, “Carbon Fiber Reinforced Polymer Tape Aslan 500,” Hughes Brothers, Seward, NE, 2009.

10. Naguib, W., and Mirmiran, A., “Flexural Creep Tests and Modeling of Concrete-Filled Fiber Reinforced Polymer Tubes,” Journal of Composites for Construction, ASCE, V. 6, No. 4, 2002, pp. 272-279. doi: 10.1061/(ASCE)1090-0268(2002)6:4(272)

11. Wu, Z., and Diab, H., “Constitutive Model for Time-Dependent Behavior of FRP-Concrete Interface,” Journal of Composites for Construction, ASCE, V. 11, No. 5, 2007, pp. 477-486. doi: 10.1061/(ASCE)1090-0268(2007)11:5(477)

12. Ferrier, E.; Michel, L.; Jurkiewiez, B.; and Hamelin, P., “Creep Behavior of Adhesives Used for External FRP Strengthening of RC Structures,” Construction and Building Materials, V. 25, No. 2, 2011, pp. 461-467. doi: 10.1016/j.conbuildmat.2010.01.002

13. Meaud, C.; Jurkiewiez, B.; and Ferrier, E., “Investigation of Creep Effects in Strengthened RC Structures through Double Lap Shear Testing,” Composites. Part B, Engineering, V. 42, No. 3, 2011, pp. 359-366. doi: 10.1016/j.compositesb.2010.12.024

14. ACI Committee 209, “Guide for Modeling and Calculating Shrinkage and Creep in Hardened Concrete (ACI 209.2R-08),” Farmington Hills, MI, 2008, 44 pp.

15. Findley, W. N., “Mechanism and Mechanics of Creep of Plastics,” SPE Journal, V. 16, 1960, pp. 57-65.

16. Scott, D. W.; Lai, J. S.; and Zureick, A.-H., “Creep Behavior of Fiber-Reinforced Polymer Composites: A Review of the Technical Literature,” Journal of Reinforced Plastics and Composites, V. 14, 1995, pp. 588-617.

17. Hamed, E., and Chang, Z.-T., “Effect of Creep on the Edge Debonding Failure of FRP Strengthened RC Beams—A Theoretical and Experimental Study,” Composites Science and Technology, V. 74, 2013, pp. 186-193. doi: 10.1016/j.compscitech.2012.11.011

18. Razak, H. A., “Time Dependent Effects in Reinforced Concrete Sections Subjected to Flexure,” PhD thesis, University of Surrey, Surrey, UK, 1986, 219 pp.

19. Khan, A. A.; Cook, W. D.; and Mitchell, D., “Creep, Shrinkage, and Thermal Strains in Mormal, Medium, and High-Strength Concretes during Hydration,” ACI Materials Journal, V. 94, No. 2, Mar.-Apr. 1997, pp. 156-163.

20. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-11) and Commentary,” American Concrete Institute, Farmington Hills, MI, 2011, 503 pp.

21. Corotis, R. B., and Tsay, W.-Y., “Probabilistic Load Duration Model for Live Loads,” Journal of Structural Engineering, ASCE, V. 109, No. 4, 1983, pp. 859-874. doi: 10.1061/(ASCE)0733-9445(1983)109:4(859)

22. MacGregor, J. G., Reinforced Concrete: Mechanics and Design, Prentice Hall, Upper Saddle River, NJ, 1997, 939 pp.

23. USGS, “Climate of North Dakota: Relative Humidity,” Northern Prairie Wildlife Research Center, Jamestown, ND, 2013.


ALSO AVAILABLE IN:

Electronic Structural Journal