Title: SCC Under Pressure Research Program

Author(s):

Publication: Concrete International

Volume: 37

Issue: 1

Appears on pages(s): 27-29

Keywords: model, form, test, transducer

DOI: 10.14359/51687458

Date: 1/1/2015

Abstract:
Various pressure models for self-consolidating concrete have been developed independently by researchers from Europe, the United States, and Canada. To help reconcile these models, RILEM Technical Committee 233-FPC, Form Pressure Generated by Fresh Concrete, was formed 5 years ago. The committee conducted full-scale wall tests two years ago in Stockholm, Sweden. As a continuation of this research, another testing program was carried out on tall column forms in Toronto, Canada, in 2014. This article provides a brief summary of the event.