BEHAVIOR AND SIMPLIFIED MODELING OF MECHANICAL REINFORCING BAR SPLICES

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: BEHAVIOR AND SIMPLIFIED MODELING OF MECHANICAL REINFORCING BAR SPLICES

Author(s): Zachary B. Haber, M. Saiid Saiidi, and David H. Sanders

Publication: Structural Journal

Volume: 112

Issue: 2

Appears on pages(s): 179-188

Keywords: accelerated bridge construction; acceptance criteria; coupler; ductility; mechanical splice; repair; seismic; shape-memory alloy

DOI: 10.14359/51687455

Date: 3/1/2015

Abstract:
Bridge seismic design codes do not allow mechanical reinforcing bar splices in regions expected to undergo significant inelastic deformations during earthquakes, thus severely limiting precast and innovative bridge column construction that uses such splices. The uniaxial behavior of two commercially available mechanical splices under different loading conditions was investigated experimentally in this study with emphasis on deformation response. Tests were performed with static, dynamic, and cyclic loading. The performance of the splices was satisfactory under all loading conditions in that bar fracture occurred outside the splice. Furthermore, the results revealed the effect of the relatively high stiffness of mechanical couplers. The responses of individual splices were used to interpret data from a series of cyclic tests on half-scale bridge columns employing mechanical splices in plastic hinge zones. Lastly, a simple method was proposed and validated for modeling these devices in reinforced concrete members.

Related References:

1. ACI Committee 439, “Types of Mechanical Splices for Reinforcing Bars (ACI 439.3R-07),” American Concrete Institute, Farmington Hills, MI, 2007, 20 pp.

2. ICC-ES AC133, “Acceptance Criteria for Mechanical Connector Systems for Steel Reinforcing Bars,” International Code Council Evaluation Service, Whittier, CA, 2010, 9 pp.

3. ASTM A1034/A1034M-10, “Standard Test Methods for Testing Mechanical Splices for Steel Reinforcing Bars,” ASTM International, West Conshohocken, PA, 2010, 5 pp.

4. CT670, “Method of Tests for Mechanical and Welded Reinforcing Steel Splices,” California Department of Transportation, Division of Engineering Services, Sacramento, CA, 2011, 11 pp.

5. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-02) and Commentary,” American Concrete Institute, Farmington Hills, MI, 2002, 443 pp.

6. American Assiciation of State Highway and Transportation Officials (AASHTO), “AASHTO Guide Specifications for LRFD Seismic Bridge Design,” second edition, Washington, DC, 2011, 301 pp.

7. California Department of Transportation, “Seismic Design Criteria (SDC) Version 1.7,” Division of Engineering Services, Sacramento, CA, 2013, 180 pp.

8. Haber, Z. B.; Saiidi, M.; and Sanders, D. H., “Seismic Performance of Precast Columns with Mechanically Spliced Column-Footing Connection,” ACI Structural Journal, Vol. 111, No. 3, May-June 2014, pp. 639-650.

9. Paulson, C., and Hanson, J. M., “Fatigue Behavior of Welded and Mechanical Splices in Reinforcing Steel,” NCHRP Report 10-35, Dec. 1991, 158 pp.

10. Rowell, S. P.; Grey, C. E.; Woodson, S. C.; and Hager, K. P., “High Strain-Rate Testing of Mechanical Couplers,” Report ERDC TR-09-8, U.S. Army Corps of Engineers, Washington, DC, Sept. 2009, 74 pp.

11. Aida, H.; Tanimura, Y.; Tadokoro, T.; and Takimoto, K., “Cyclic Loading Experiment of Precast Columns of Railway Rigid-Frame Viaduct Installed with NMB Splice Sleeves,” Proceedings of the Japan Concrete Institute, V. 27, No. 2, 2005, pp. 613-618.

12. Culmo, M. P., “Connection Details for Prefabricated Bridge Elements and Systems,” Report FHWA-IF-09-010, Federal Highway Administration, Washington, DC, Mar. 2009, 568 pp.

13. ASTM A370-03a, “Standard Test Methods and Definitions for Mechanical Testing of Steel Products,” ASTM International, West Conshohocken, PA, 2003, 49 pp.

14. Motaref, S.; Saiidi, M. S.; and Sanders, D. H., “Seismic Response of Precast Bridge Columns with Energy Dissipating Joints,” Report No. CCEER-11-01, Center for Civil Engineering Earthquake Research, Department of Civil Engineering. University of Nevada, Reno, Reno, NV, 2011.

15. Sadrossadat-Zadeh, M., and Saiid Saiidi, M., “Effect of Strain Rate on Stress-Strain Properties and Yield Propagation in Steel Reinforcing Bars,” Report No. CCEER-07-02, Center for Civil Engineering Earthquake Research, Department of Civil Engineering. University of Nevada, Reno, Reno, NV, 2007.

16. Otani, S., and Sozen, M. A., “Behavior of Multistory Reinforced Concrete Frames during Earthquakes,” Structural Research Series No. 392, University of Illinois, Urbana, IL, 1972, 551 pp.

17. Haber, Z. B.; Saiidi, M.; Ou, Y. C.; and Sanders, D. H., “A Method for Calculating the Seismic Response of Bridge Columns with Grouted Sleeve Column-Footing Connections,” Proceedings, Seventh National Seismic Conference on Bridges & Highways, Oakland, CA., May 20-22, 2013.

18. Malvar, L. J, “Review of Static and Dynamic Properties of Steel Reinforcing Bars” ACI Materials Journal, V. 95, No. 5, Sept.-Oct.1998, pp. 609-614.

19. Fu, H. C.; Erki, M. A.; and Seckin, M., “Review of Effects of Loading Rate on Reinforced Concrete,” Journal of Structural Engineering, ASCE, V. 117, No. 12, Dec. 1991, pp. 3660-3679.

20. Mander, J. B.; Panthaki, F. D.; Kasalanati, A. “Low-Cycle Fatigue Behavior of Reinforcing Steel,” Journal of Materials in Civil Engineering, ASCE, V. 6, No. 4, 1994, pp. 453-468.

21. Mander, J. B.; Priestley, M. J. N.; and Park, R., “Theoretical Stress-Strain Model for Confined Concrete,” Journal of Structural Engineering, ASCE, V. 114, No. 8, 1988, pp. 1808-1826.


ALSO AVAILABLE IN:

Electronic Structural Journal