STRUCTURAL BEHAVIOUR OF THE CONNECTIONS BETWEEN PRE FABRICATED CONCRETE SEGMENTS FOR TUNNELS.

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: STRUCTURAL BEHAVIOUR OF THE CONNECTIONS BETWEEN PRE FABRICATED CONCRETE SEGMENTS FOR TUNNELS.

Author(s): Fernando Peña, Arturo Galván Chávez y Roberto Meli.

Publication: IMCYC

Volume: 3

Issue: 2

Appears on pages(s): 2-18

Keywords: Tunnel; dowels; joints; moment–rotation relation.

DOI:

Date: 1/1/2012

Abstract:
The aim of this paper is to study the mechanical behavior of typical planar joints, similar to those used in segmented tunnels, by means of experimental tests performed in scaled down models. In addition, a theoretical moment–rotation relation that represents the mechanical behavior of joints between segments of tunnels is proposed. The proposed curve consists of an initial linear part and a plastic branch.