Title: An Update on EPRI Concrete Research

Author(s): Kenneth F. Barry

Publication: Web Session

Volume: Barry.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/27/2014

Abstract:
The goal of the ACI Foundation’s Strategic Development Council (SDC) is industry-wide collaboration to address the concrete industry’s technological challenges and to create a forum for the introduction and nurturing of new technologies. This session highlights issues of importance in the concrete industry and overviews of newer technologies currently or soon to be impacting the concrete industry. The presentations are by individuals who are both well-versed in the specific issue or technology and directly involved in their implementation and further development.