Concrete Made with Recycled Glass Aggregates: Mechanical Performance

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Made with Recycled Glass Aggregates: Mechanical Performance

Author(s): Diogo Serpa, Jorge de Brito, and Jorge Pontes

Publication: Materials Journal

Volume: 112

Issue: 1

Appears on pages(s): 29-38

Keywords: mechanical performance; recycled glass aggregates; sustainability

DOI: 10.14359/51687366

Date: 1/1/2015

Abstract:
This study aims at characterizing the mechanical performance of concrete made with varying glass content (5, 10, and 20% of the overall volume of aggregates) and analyzing the influence of the size of these aggregates (fine, coarse, or both) on that performance. The use of glass aggregates as an environmentally friendly alternative to dumping it as waste reduces the consumption of natural resources and requires the space needed for dumping grounds. The aggregates were studied in terms of density and abrasion. Fresh concrete was tested for workability and density. Hardened concrete was tested for compressive, splitting tensile, and flexural strength; modulus of elasticity; and abrasion wear. It was found that the incorporation of glass aggregates in concrete leads to a loss of its mechanical performance, though this is not significant for ratios of up to 10% of the volume of natural aggregates, except for abrasion resistance, where there is an improvement. A better performance was seen in concrete with coarse glass aggregates, followed by concrete with fine glass aggregates, and finally, concrete with the simultaneous incorporation of coarse and fine glass aggregates.

Related References:

1. Topçu, I. B., and Canbaz, M., “Properties of Concrete Containing Waste Glass,” Cement and Concrete Research, V. 34, No. 2, 2004, pp. 267-274. doi: 10.1016/j.cemconres.2003.07.003

2. National Institute of Statistics, “Management of Waste in Portugal, 2004-2009, Information to the medial,” INE, Aug. 4, 2010. (in Portuguese)

3. Oliveira, L.; Gomes, J.; and Santos, P., “Evaluation of the Performance of the Replacement of Natural Sand by Glass Waste Sand in Structural Concrete,” National Meeting of Structural Concrete 2008, Guimarães, Portugal, 2008. (in Portuguese)

4. Al-Sibahy, A., and Edwards, R., “Mechanical and Thermal Properties of Novel Lightweight Concrete Mixtures Containing Recycled Glass and Metakaolin,” Construction and Building Materials, V. 31, 2012, pp. 157-167. doi: 10.1016/j.conbuildmat.2011.12.095

5. Wang, H. Y., and Huang, W. L., “A Study on the Properties of Fresh Self-Consolidating Glass Concrete (SCGC),” Construction and Building Materials, V. 24, No. 4, 2010, pp. 619-624. doi: 10.1016/j.conbuildmat.2009.08.047

6. Wang, H. Y., “A Study on the Effects of LCD Glass Sand on the Properties of Concrete,” Waste Management (New York, N.Y.), V. 29, No. 1, 2009, pp. 335-341. doi: 10.1016/j.wasman.2008.03.005

7. Su, N., and Chen, J. S., “Engineering Properties of Asphalt Concrete Made with Recycled Glass,” Resources, Conservation and Recycling, V. 35, No. 4, 2002, pp. 259-274. doi: 10.1016/S0921-3449(02)00007-1

8. Ferreira, L.; de Brito, J.; and Saikia, N., “Influence of Curing Conditions on the Mechanical Performance of Concrete Containing Recycled Plastic Aggregate,” Construction and Building Materials, V. 36, 2012, pp. 196-204. doi: 10.1016/j.conbuildmat.2012.02.098

9. Silva, R.; de Brito, J.; and Saikia, N., “Influence of Curing Conditions on the Durability-Related Performance of Concrete Made with Selected Plastic Waste Aggregates,” Cement and Concrete Composites, V. 35, No. 1, 2013, pp. 23-31. doi: 10.1016/j.cemconcomp.2012.08.017

10. Bravo, M., and de Brito, J., “Concrete Made with Used Tyre Aggregates: Durability-Related Performance,” Journal of Cleaner Production, V. 25, No. 4, 2012, pp. 42-50. doi: 10.1016/j.jclepro.2011.11.066

11. Valadares, F.; Bravo, M.; and de Brito, J., “Concrete with Used Tire Rubber Aggregates: Mechanical Performance,” ACI Materials Journal, V. 109, No. 3, May-June 2012, pp. 283-292.

12. Evangelista, L., and de Brito, J., “Mechanical Behavior of Concrete Made with Fine Recycled Concrete Aggregates,” Cement and Concrete Composites, V. 29, No. 5, 2007, pp. 397-401. doi: 10.1016/j.cemconcomp.2006.12.004

13. Evangelista, L., and de Brito, J., “Durability Performance of Concrete Made with Fine Recycled Concrete Aggregates,” Cement and Concrete Composites, V. 32, No. 1, 2010, pp. 9-14. doi: 10.1016/j.cemconcomp.2009.09.005

14. de Brito, J.; Pereira, A. S.; and Correia, J., “Mechanical Behavior of Non-Structural Concrete Made with Recycled Ceramic Aggregates,” Cement and Concrete Composites, V. 27, No. 4, 2005, pp. 429-433. doi: 10.1016/j.cemconcomp.2004.07.005

15. Correia, J.; de Brito, J.; and Pereira, A. S., “Effects on Concrete Durability of Using Recycled Ceramic Aggregates,” Materials and Structures, V. 39, No. 2, 2006, pp. 169-177. doi: 10.1617/s11527-005-9014-7

16. Serpa, D.; Santos Silva, A.; de Brito, J.; Pontes, J.; and Soares, D., “ASR of Mortars Containing Glass,” Construction and Building Materials, V. 47, 2013, pp. 489-495. doi: 10.1016/j.conbuildmat.2013.05.058

17. de Castro, S., and de Brito, J., “Evaluation of the Durability of Concrete Made with Crushed Glass Aggregates,” Journal of Cleaner Production, V. 41, 2013, pp. 7-14. doi: 10.1016/j.jclepro.2012.09.021

18. Chen, S. H.; Chang, C. S.; Wang, H. Y.; and Huang, W. L., “Mixture Design of High Performance Recycled Liquid Crystal Glass Concrete (HPGC),” Construction and Building Materials, V. 25, No. 10, 2011, pp. 3886-3892. doi: 10.1016/j.conbuildmat.2011.04.012

19. Kou, S. C., and Poon, C. S., “Properties of Self-Compacting Concrete Prepared with Recycled Glass Aggregates,” Cement and Concrete Composites, V. 31, No. 2, 2009, pp. 107-113. doi: 10.1016/j.cemconcomp.2008.12.002

20. Ismail, Z. Z., and Al-Hashmi, E. A., “Recycling of Waste Glass as a Partial Replacement for Fine Aggregate in Concrete,” Waste Management (New York, N.Y.), V. 29, No. 2, 2009, pp. 655-659. doi: 10.1016/j.wasman.2008.08.012

21. Limbachiya, M. C., “Bulk Engineering and Durability Properties of Washed Glass Sand Concrete,” Construction and Building Materials, V. 23, No. 2, 2009, pp. 1078-1083. doi: 10.1016/j.conbuildmat.2008.05.022

22. Alhumoud, J. M.; Al-Mutairi, N. Z.; and Terro, M. J., “Recycling Crushed Glass in Concrete Mixtures,” International Journal of Environment and Waste Management, V. 2, No. 1/2, 2008, pp. 111-124. doi: 10.1504/IJEWM.2008.016996

23. Terro, M. J., “Properties of Concrete Made with Recycled Crushed Glass at Elevated Temperatures,” Building and Environment, V. 41, No. 5, 2006, pp. 633-639. doi: 10.1016/j.buildenv.2005.02.018

24. Park, S. B.; Lee, B. C.; and Kim, J. H., “Studies on Mechanical Properties of Concrete Containing Waste Glass Aggregate,” Cement and Concrete Research, V. 34, No. 12, 2004, pp. 2181-2189. doi: 10.1016/j.cemconres.2004.02.006

25. EN 1992-1-1:2004, “Eurocode 2: Design of Concrete Structures - Part 1-1: General Rules and Rules for Buildings,” European Committee for Standardization, Brussels, Belgium, 2004, 225 pp.

26. EN 206-1:2000, “Concrete—Part 1: Specification, Performance, Production and Conformity,” European Committee for Standardization, Brussels, Belgium, 2000, 72 pp.

27. NP EN 933-1:2000, “Tests for Geometrical Properties of Aggregates, Part 1: Determination of Particle Size Distribution—Sieving Method,” Instituto Português da Qualidade, Lisbon, Portugal, 2000. (in Portuguese)

28. NP EN 933-2:1999, “Tests for Geometrical Properties of Aggregates, Part 2: Determination of Particle Size Distribution—Test Sieves, Nominal Size of Apertures,” Instituto Português da Qualidade, Lisbon, Portugal, 1999. (in Portuguese)

29. NP EN 1097-6:2003, “Tests for Mechanical and Physical Properties of Aggregates, Part 6: Determination of Particle Density and Water Absorption,” Instituto Português da Qualidade, Lisbon, Portugal, 2003. (in Portuguese)

30. NP EN 1097-3:2008, “Tests for Mechanical and Physical Properties of Aggregates, Part 3: Determination of Loose Bulk Density and Voids,” Instituto Português da Qualidade, Lisbon, Portugal, 2008. (in Portuguese)

31. NP EN 933-4:2008, “Tests for Geometrical Properties of Aggregates, Part 4: Determination of Particle Shape—Shape Index,” Instituto Português da Qualidade, Lisbon, Portugal, 2008. (in Portuguese)

32. LNEC E237:1970, “Determination of the Water Absorption by Capillarity,” Instituto Português da Qualidade, Lisbon, Portugal, 1970. (in Portuguese)

33. NP EN 12350-2:2009, “Testing Fresh Concrete, Part 2: Slump-Test,” Instituto Português da Qualidade, Lisbon, Portugal, 2009. (in Portuguese)

34. NP EN 12350-6:2009, “Testing Fresh Concrete, Part 6: Density” Instituto Português da Qualidade, Lisbon, Portugal, 2009. (in Portuguese)

35. NP EN 12390-3:2009, “Testing Hardened Concrete, Part 3: Compressive Strength of Test Specimens,” Instituto Português da Qualidade, Lisbon, Portugal, 2009. (in Portuguese)

36. NP EN 12390-6:2003, “Testing Hardened Concrete, Part 6: Tensile Splitting Strength of Test Specimens,” Instituto Português da Qualidade, Lisbon, Portugal, 2003. (in Portuguese)

37. NP EN 12390-5:2009, “Testing Hardened Concrete, Part 5: Flexural Strength of Test Specimens,” Instituto Português da Qualidade, Lisbon, Portugal, 2009. (in Portuguese)

38. LNEC E 397:1993, “Hardened Concrete: Determination of the Modulus of Elasticity in Compression,” Instituto Português da Qualidade, Lisbon, Portugal, 1993. (in Portuguese)

39. DIN 52108:2002, “Testing of Inorganic Non-Metallic Materials—Wear Test Using the Grinding Wheel according to Boehme—Grinding Wheel Method,” Deutsches Institut für Normung, Berlin, Germany 2002. (in German)

40. de Brito, J., “Abrasion Resistance of Concrete Made with Recycled Aggregates,” International Journal of Sustainable Engineering, V. 3, No. 1, 2010, pp. 58-64. doi: 10.1080/19397030903254710


ALSO AVAILABLE IN:

Electronic Materials Journal