232.3R-14: Report on High-Volume Fly Ash Concrete for Structural Applications

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 232.3R-14: Report on High-Volume Fly Ash Concrete for Structural Applications

Author(s): ACI Committee 232

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 19

Keywords: alkali-silica reaction; compressive strength; corrosion of reinforcement; cracking; deicing salts; fly ash; heat of hydration; mixture proportions; modulus of elasticity; shrinkage; sulfate attack; sustainability; tensile strength.

DOI:

Date: 10/1/2014

Abstract:
This report presents technical information to support the use of high-volume fly ash concrete for structural applications. The advantages and limitations of high-volume fly ash concrete are discussed, and the characteristics of the fresh and hardened materials and the durability of the material to various aggressive environments are covered. Field applications are presented along with sustainability features.