238.2T-14: Concrete Thixotropy (TechNote)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 238.2T-14: Concrete Thixotropy (TechNote)

Author(s): ACI Committee 238

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 6

Keywords: aggregate segregation; formwork pressure; plastic viscosity; pumpability; rheology; rheometer; static yield stress; thixotropy; yield stress.

DOI:

Date: 6/1/2014

Abstract:
Fresh concrete can exhibit different rheological behavior when at rest than when flowing. This difference is due to thixotropy, which can have important consequences for formwork pressure, multi-lift casting, slip-form paving, pumping, and segregation resistance. This TechNote defines thixotropy and distinguishes it from other changes in rheological properties; discusses the origins of, test methods for measuring, and factors affecting thixotropy; and concludes with its applications.