Effects of Nanosilica Addition on Increased Thermal Stability of Cement-Based Composite

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effects of Nanosilica Addition on Increased Thermal Stability of Cement-Based Composite

Author(s): Seungmin Lim and Paramita Mondal

Publication: Materials Journal

Volume: 112

Issue: 2

Appears on pages(s): 305-316

Keywords: carbonation; cement paste; high temperature exposure; nanosilica; thermogravimetric analysis (TGA)

DOI: 10.14359/51687177

Date: 3/1/2015

Abstract:
Recently, nanosilica has been widely suggested as an excellent supplementary cementitious material due to its superior reactivity in comparison to other types of siliceous materials. Nanosilica is reported to increase the residual compressive strength of mortar after exposure to high temperatures. The addition of nanosilica has also been reported to cause fundamental changes in hydration products, increasing the average chain length of calcium silicate hydrate (C-S-H) and volume fraction of high-density C-S-H in cement paste in addition to decreasing calcium hydroxide content. However, it is not well understood exactly how nanosilica addition increases thermal stability of cement-based composites. In this study, the effects of replacement of a small amount of cement with nanosilica on the degradation of cement paste exposed to various heating and cooling regimes were investigated. Following heat treatment of cement paste samples with and without nanosilica up to 500°C (935°F), two different cooling regimes (cooling down to room temperature of 23 ± 2°C [73.4 ± 3.6°F] and prolonged heat treatment at 50°C [122°F] for 3 days) were followed. The residual states of each sample were analyzed by compression test, x-ray diffraction, scanning electron microscopy, and thermogravimetric analysis. The experimental results show that replacing 5% cement by weight with nanosilica leads to a 7 to 20% higher residual compressive strength after exposure to elevated temperatures. Furthermore, maintained exposure at above ambient temperature for long periods of time after exposure to high temperatures caused severe damage only to paste samples that did not contain nanosilica. This damage was not seen in samples containing nanosilica. Reduction in calcium hydroxide content due to the pozzolanic activity of nanosilica seems to be the primary reason for the minimized level of damage by reducing the degree of carbonation of hydration products immediately following heat treatment.

Related References:

1. Ulm, F. J.; Acker, P.; and Lévy, M., “The ‘Chunnel’ Fire. II: Analysis of Concrete Damage,” Journal of Engineering Mechanics, ASCE, V. 125, No. 3, 1999, pp. 283-289. doi: 10.1061/(ASCE)0733-9399(1999)125:3(283)

2. Komonen, J., and Penttala, V., “Effects of High Temperature on the Pore Structure and Strength of Plain and Polypropylene Fiber Reinforced Cement Paste,” Fire Technology, V. 39, No. 1, 2003, pp. 23-34. doi: 10.1023/A:1021723126005

3. Handoo, S. K.; Agarwal, S.; and Agarwal, S. K., “Physicochemical, Mineralogical, and Morphological Characteristics of Concrete Exposed to Elevated Temperatures,” Cement and Concrete Research, V. 32, No. 7, 2002, pp. 1009-1018. doi: 10.1016/S0008-8846(01)00736-0

4. Odelson, J. B.; Kerr, E. A.; and Vichit-Vadakan, W., “Young’s Modulus of Cement Paste at Elevated Temperatures,” Cement and Concrete Research, V. 37, No. 2, 2007, pp. 258-263. doi: 10.1016/j.cemconres.2006.11.006

5. Chan, Y. N.; Luo, X.; and Sun, W., “Compressive Strength and Pore Structure of High-Performance Concrete after Exposure to High Temperature up to 800°C,” Cement and Concrete Research, V. 30, No. 2, 2000, pp. 247-251. doi: 10.1016/S0008-8846(99)00240-9

6. Khoury, G. A., “Compressive Strength of Concrete at High Temperatures: A Reassessment,” Magazine of Concrete Research, V. 44, No. 161, 1992, pp. 291-309. doi: 10.1680/macr.1992.44.161.291

7. Vydra, V.; Vodák, F.; Kapičková, O.; and Hošková, Š., “Effect of Temperature on Porosity of Concrete for Nuclear-Safety Structures,” Cement and Concrete Research, V. 31, No. 7, 2001, pp. 1023-1026. doi: 10.1016/S0008-8846(01)00516-6

8. Peng, G.-F., and Huang, Z.-S., “Change in Microstructure of Hardened Cement Paste Subjected to Elevated Temperatures,” Construction & Building Materials, V. 22, No. 4, 2008, pp. 593-599. doi: 10.1016/j.conbuildmat.2006.11.002

9. Rostásy, F. S.; Weiß, R.; and Wiedemann, G., “Changes of Pore Structure of Cement Mortars due to Temperature,” Cement and Concrete Research, V. 10, Mar. 1980, pp. 157-164. doi: 10.1016/0008-8846(80)90072-1

10. Harmathy, T. Z., “Thermal Properties of Concrete at Elevated Temperatures,” Journal of Materials, V. 5, No. 1, 1970, pp. 47-74.

11. Harmathy, T. Z., Fire Safety Design and Concrete, Longman Group, London, UK, 1993, 272 pp.

12. Piasta, J., “Heat Deformations of Cement Paste Phases and the Microstructure of Cement Paste,” Matériaux et Constructions, V. 17, No. 6, 1984, pp. 415-420. doi: 10.1007/BF02473981

13. Zhou, Q., and Glasser, F. P., “Thermal Stability and Decomposition Mechanisms of Ettringite at <120°C,” Cement and Concrete Research, V. 31, No. 9, 2001, pp. 1333-1339. doi: 10.1016/S0008-8846(01)00558-0

14. Alarcon-Ruiz, L.; Platret, G.; Massieu, E.; and Ehrlacher, A., “The Use of Thermal Analysis in Assessing the Effect of Temperature on a Cement Paste,” Cement and Concrete Research, V. 35, No. 3, 2005, pp. 609-613. doi: 10.1016/j.cemconres.2004.06.015

15. Alonso, C., and Fernandez, L., “Dehydration and Rehydration Process of Cement Paste Exposed to High Temperature Environments,” Journal of Materials Science, V. 39, No. 9, 2004, pp. 3015-3024. doi: 10.1023/B:JMSC.0000025827.65956.18

16. Castellote, M.; Alonso, C.; Andrade, C.; Turrillas, X.; and Campo, J., “Composition and Microstructural Changes of Cement Pastes upon Heating, as Studied by Neutron Diffraction,” Cement and Concrete Research, V. 34, No. 9, 2004, pp. 1633-1644. doi: 10.1016/S0008-8846(03)00229-1

17. Petzold, A., and Röhrs, M., Concrete for High Temperature, Maclaren and Sons Ltd, London, UK, 1970.

18. Taylor, H. F. W., “The Water Content of Calcium Silicate Hydrate (I),” Journal of the Chemical Society, 1953, pp. 163-171. doi: 10.1039/jr9530000163

19. Fordham, C. J., and Smalley, I. J., “A Simple Thermogravimetric Study of Hydrated Cement,” Cement and Concrete Research, V. 15, No. 1, 1985, pp. 141-144. doi: 10.1016/0008-8846(85)90019-5

20. Zhang, Q., and Ye, G., “Dehydration Kinetics of Portland Cement Paste at High Temperature,” Journal of Thermal Analysis and Calorimetry, V. 110, No. 1, 2012, pp. 153-158. doi: 10.1007/s10973-012-2303-9

21. Khoury, G. A.; Majorana, C. E.; Pesavento, F.; and Schrefler, B. A., “Modeling of Heated Concrete,” Magazine of Concrete Research, V. 54, No. 2, 2002, pp. 77-101. doi: 10.1680/macr.2002.54.2.77

22. Wang, H. Y., “The Effects of Elevated Temperature on Cement Paste Containing GGBFS,” Cement and Concrete Composites, V. 30, No. 10, 2008, pp. 992-999. doi: 10.1016/j.cemconcomp.2007.12.003

23. Ibrahim, R. K.; Hamid, R.; and Taha, M. R., “Fire Resistance of High-Volume Fly Ash Mortars with Nanosilica Addition,” Construction & Building Materials, V. 36, 2012, pp. 779-786. doi: 10.1016/j.conbuildmat.2012.05.028

24. Hertz, K. D., “Danish Investigations on Silica Fume Concretes at Elevated Temperatures,” ACI Materials Journal, V. 89, No. 4, July-Aug. 1992, pp. 345-347.

25. Kalifa, P.; Menneteau, F.-D.; and Quenard, D., “Spalling and Pore Pressure in HPC at High Temperatures,” Cement and Concrete Research, V. 30, No. 12, 2000, pp. 1915-1927. doi: 10.1016/S0008-8846(00)00384-7

26. Kalifa, P.; Chéné, G.; and Gallé, C., “High-Temperature Behaviour of HPC with Polypropylene Fibres: From Spalling to Microstructure,” Cement and Concrete Research, V. 31, No. 10, 2001, pp. 1487-1499. doi: 10.1016/S0008-8846(01)00596-8

27. Peng, G. F.; Yang, W. W.; Zhao, J.; Liu, Y. F.; Bian, S. H.; and Zhao, L. H., “Explosive Spalling and Residual Mechanical Properties of Fiber-Toughened High Performance Concrete Subjected to High Temperatures,” Cement and Concrete Research, V. 36, No. 4, 2006, pp. 723-727. doi: 10.1016/j.cemconres.2005.12.014

28. Dias, W. P. S.; Khoury, G. A.; and Sullivan, P. J. E., “Mechanical Properties of Hardened Cement Paste Exposed to Temperatures up to 700 C (1292 F),” ACI Materials Journal, V. 87, No. 2, Mar.-Apr. 1990, pp. 160-166.

29. Qing, Y.; Zenan, Z.; Deyu, K.; and Rongshen, C., “Influence of Nano-SiO2 Addition on Properties of Hardened Cement Paste as Compared with Silica Fume,” Construction & Building Materials, V. 21, No. 3, 2007, pp. 539-545. doi: 10.1016/j.conbuildmat.2005.09.001

30. Shih, J. Y.; Chang, T. P.; and Hsiao, T. C., “Effect of Nanosilica on Characterization of Portland Cement Composite,” Materials Science and Engineering A, V. 424, No. 1-2, 2006, pp. 266-274. doi: 10.1016/j.msea.2006.03.010

31. Gaitero, J. J.; Campillo, I.; and Guerrero, A., “Reduction of the Calcium Leaching Rate of Cement Paste by Addition of Silica Nanoparticles,” Cement and Concrete Research, V. 38, No. 8-9, 2008, pp. 1112-1118. doi: 10.1016/j.cemconres.2008.03.021

32. Jain, J. A., and Neithalath, N., “Beneficial Effects of Small Amount of Nano-silica on the Chemical Stability of Cement Pastes Exposed to Neutral pH Environments,” Nanotechnology of Concrete: The Next Big Thing is Small, SP-267, K. Sobolev and M. Reda Taha, eds., American Concrete Institute, Farmington Hills, MI, 2009, pp. 59-74.

33. Sáez del Bosque, I. F.; Martínez-Ramírez, S.; and Blanco-Varela, M. T., “FTIR Study of the Effect of Temperature and Nanosilica on the Nanostructure of C-S-H Gel Formed by Hydrating Tricalcium Silicate,” Construction & Building Materials, V. 52, 2014, pp. 314-323. doi: 10.1016/j.conbuildmat.2013.10.056

34. Mondal, P.; Shah, S. P.; Marks, L. D.; and Gaitero, J. J., “Comparative Study of the Effect of Microsilica and Nanosilica in Concrete,” Transportation Research Record: Journal of the Transport Research Board, V. 2141, 2010, pp. 6-9. doi: 10.3141/2141-02

35. DeJong, M. J., and Ulm, F. J., “The Nanogranular Behavior of C-S-H at Elevated Temperatures (up to 700 °C),” Cement and Concrete Research, V. 37, No. 1, 2007, pp. 1-12. doi: 10.1016/j.cemconres.2006.09.006

36. ASTM C305-06, “Standard Practice for Mechanical Mixing of Hydraulic Cement Pastes and Mortars of Plastic Consistency,” ASTM International, West Conshohocken, PA, 2006, 3 pp.

37. Senff, L.; Hotza, D.; Lucas, S.; Ferreira, V. M.; and Labrincha, J. A., “Effect of Nano-SiO2 and Nano-TiO2 Addition on the Rheological Behavior and the Hardened Properties of Cement Mortars,” Materials Science and Engineering A, V. 532, 2012, pp. 354-361. doi: 10.1016/j.msea.2011.10.102

38. Ji, T., “Preliminary Study on the Water Permeability and Microstructure of Concrete Incorporating Nano-SiO2,” Cement and Concrete Research, V. 35, No. 10, 2005, pp. 1943-1947. doi: 10.1016/j.cemconres.2005.07.004

39. Piasta, J.; Sawicz, Z.; and Rudzinski, L., “Changes in the Structure of Hardened Cement Paste due to High Temperature,” Matériaux et Constructions, V. 17, No. 4, 1984, pp. 291-296. doi: 10.1007/BF02479085

40. Famy, C.; Scrivener, K. L.; Atkinson, A.; and Brough, A. R., “Effect of an Early or a Late Heat Treatment on the Microstructure and Composition of Inner C-S-H Products of Portland Cement Mortars,” Cement and Concrete Research, V. 32, No. 2, 2002, pp. 269-278. doi: 10.1016/S0008-8846(01)00670-6

41. Dias, W. P. S.; Khoury, G. A.; and Sullivan, P. J. E., “Shrinkage of Hardened Cement Paste at Elevated Temperatures up to 670 C (1238 F),” ACI Materials Journal, V. 87, No. 3, May-June 1990, pp. 204-209.

42. Madani, H.; Bagheri, A.; and Parhizkar, T., “The Pozzolanic Reactivity of Monodispersed Nanosilica Hydrosols and their Influence on the Hydration Characteristics of Portland Cement,” Cement and Concrete Research, V. 42, No. 12, 2012, pp. 1563-1570. doi: 10.1016/j.cemconres.2012.09.004

43. Bukowski, J. M., and Berger, R. L., “Reactivity and Strength Development of CO2 Activated Non-hydraulic Calcium Silicates,” Cement and Concrete Research, V. 9, No. 1, 1979, pp. 57-68. doi: 10.1016/0008-8846(79)90095-4

44. Dunster, A. M., “An Investigation of the carbonation of Cement Paste using Trimethylsilylation,” Advances in Cement Research, V. 2, No. 7, 1989, pp. 99-106. doi: 10.1680/adcr.1989.2.7.99

45. Groves, G. W.; Rodway, D. K.; and Richardson, I. G., “The Carbonation of Hardened Cement Pastes,” Advances in Cement Research, V. 3, No. 11, 1990, pp. 117-125. doi: 10.1680/adcr.1990.3.11.117

46. Groves, G. W.; Brough, A. R.; Richardson, I. G.; and Dobson, C. M., “Progressive Changes in the Structure of Hardened C3S Cement Pastes due to Carbonation,” Journal of the American Ceramic Society, V. 74, No. 11, 1991, pp. 2891-2896. doi: 10.1111/j.1151-2916.1991.tb06859.x

47. Borges, P. H. R.; Costa, J. O.; Milestone, N. B.; Lynsdale, C. J.; and Streatfield, R. E., “Carbonation of CH and C-S-H in Composite Cement Pastes Containing High Amounts of BFS,” Cement and Concrete Research, V. 40, No. 2, 2010, pp. 284-292. doi: 10.1016/j.cemconres.2009.10.020

48. Black, L.; Breen, C.; Yarwood, J.; Garbev, K.; Stemmermann, P.; and Gasharova, B., “Structural Features of C-S-H(I) and its Carbonation in Air—A Raman Spectroscopic Study. Part II: Carbonated Phases,” Journal of the American Ceramic Society, V. 90, No. 3, 2007, pp. 908-917. doi: 10.1111/j.1551-2916.2006.01429.x


ALSO AVAILABLE IN: