IMPROVING DEFLECTION PREDICTION MODEL FROM ACI 318

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: IMPROVING DEFLECTION PREDICTION MODEL FROM ACI 318

Author(s): Viktor Gribniak and Gintaris Kaklauskas

Publication: Structural Journal

Volume: 111

Issue: 6

Appears on pages(s): 1491-1496

Keywords: accuracy; deflections; design code; reinforced concrete; shrinkage; test data

DOI: 10.14359/51687167

Date: 11/1/2014

Abstract:
This paper proposes a simple and mechanically sound modification of the deflection prediction model specified by the ACI 318 Building Code. The main idea of the proposal is that shrinkage effect should be taken into account in the assessment of the cracking resistance of bending members. This in turn will have influence on both short- and long-term deflection predictions. The proposed modification has been statistically validated using a database of more than 3500 measurements of short- and long-term deflections of 402 reinforced concrete members collected from 36 test programs.