Modeling Chloride Diffusion in Concrete with Linear Increase of Surface Chloride

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Modeling Chloride Diffusion in Concrete with Linear Increase of Surface Chloride

Author(s): Shengjun Zhou

Publication: Materials Journal

Volume: 111

Issue: 5

Appears on pages(s): 483-490

Keywords: chloride diffusion; modeling; surface chloride concentration

DOI: 10.14359/51686989

Date: 9/1/2014

Abstract:
Mathematical models are derived to predict chloride diffusion in concrete with an initial exposure period having a linear increase of surface chloride and decreasing diffusivity, and subsequent periods with a decreasing or constant diffusivity. A new method was developed to integrate the modeling results over these periods. Modeling examples indicated that chloride diffusion is slower in the short term with a slower linear buildup of surface chloride and in the long term with a longer period of decreasing diffusivity. In the aforementioned conditions, modeling by assuming a constant surface chloride predicts a faster diffusion with the average diffusivity and a slower diffusion with the minimum diffusivity. Modeling by assuming a constant surface chloride with a decreasing diffusivity for the entire exposure duration predicts faster diffusion within a period (75 years) and slightly slower diffusion after that.