Appears on pages(s): 85-94

Keywords: belite; bond valence; crystal stability; first principles study; hydraulic activity

DOI: 10.14359/51687128

Date: 1/1/2015

Abstract:
A first-principles study was carried out to investigate the stability of the crystal structure of beta-form belite (ß-C2S) substituted by Sr atoms as trace impurities for Ca atoms in CaOx polyhedra. The effect of the connection types of CaOx polyhedral, in the form of common-edge bond and common-face bond, upon the crystal stability is described. The Ca-Ca interatomic distance closely relates to the hydraulic activity of ß-C2S. The ß-C2S substituted by an Sr atom for Ca(1) atoms having seven Ca-O bonds is energetically more stable than that substituted by an Sr atom for Ca(2) atoms having eight Ca-O bonds. The Sr-doped ß-C2S having a common face bond with SrOx polyhedra is energetically more favorable and results in structural stability compared with that having a common edge bond with SrOx polyhedra.

Related References:

1. Jost, K. H.; Ziemer, B.; and Seydel, R., “Redetermination of the Structure of β-Dicalcium Silicate,” Acta Crystallographica, V. 33, No. 6, 1977, pp. 1696-1700. doi: 10.1107/S0567740877006918

2. Udagawa, S.; Urabe, K.; Natsume, M.; and Yano, T., “Refinement of the Crystal Structure of γ-Ca2SiO4,” Cement and Concrete Research, V. 10, No. 2, 1980, pp. 139-144. doi: 10.1016/0008-8846(80)90070-8

3. Czaya, R., “Refinement of the Structure of γ-Ca2SiO4,” Acta Crystallographica, V. 27, No. 4, 1971, pp. 848-849. doi: 10.1107/S0567740871003030

4. Xiuji, F.; Xinmin, M.; and Congxi, T., “Study on the Structure and Characteristic of Dicalcium Silicate with Quantum Chemistry Calculations,” Cement and Concrete Research, V. 24, No. 7, 1994, pp. 1311-1316. doi: 10.1016/0008-8846(94)90116-3

5. Atkins, P., and Friedman, R., Molecular Quantum Mechanics, Oxford University Press, 2005, 316 pp.

6. Singh, A. K., and Yakobson, B. I., “Electronics and Magnetism of Patterned Graphene Nanoroads,” Nano Letters, V. 9, No. 4, 2009, pp. 1540-1543. doi: 10.1021/nl803622c

7. Singh, A. K.; Janotti, A.; Scheffler, M.; and Van de Walle, C. G., “Sources of Electrical Conductivity in SnO2,” Physical Review Letters, V. 101, No. 5, 2008, 44 pp.

8. Singh, A. K.; Kumar, V.; and Kawazoe, Y., “Ferromagnetism and Piezomagnetic Behavior in Mn-doped Germanium Nanotubes,” Physical Review B, V. 69, No. 23, 2004, 4 pp.

9. Singh, A. K.; Kumar, V.; and Kawazoe, Y., “Metal Encapsulated Nanotubes of Silicon and Germanium,” Journal of Materials Chemistry, V. 14, No. 4, 2004, pp. 555-563. doi: 10.1039/b311850a

10. Singh, A. K.; Kumar, V.; Note, R.; and Kawazoe, Y., “Pristine Semiconducting [110] Silicon Nanowires,” Nano Letters, V. 5, No. 11, 2005, pp. 2302-2305. doi: 10.1021/nl051739f

11. Briere, T. M.; Sluiter, M. H. F.; Kumar, V.; and Kawazoe, Y., “Atomic Structures and Magnetic Behavior of Mn Clusters,” Physical Review B, V. 66, No. 6, 2002, 6 pp.

12. Laugesen, J. L., “Density Functional Calculation of Elastic Properties of Portlandite and Foshagite,” Nanotechnology in Construction, P. J. M. Bartos, J. J. Hughes, P. Trtik, and W. Zhu, eds., 2003, pp. 185-192.

13. Sakurada, R.; Singh, A. K.; Uzawa, M.; and Kawazoe, Y., “First Principles Calculation of Beta-Form Belite Substituted with Trace Impurity,” 34th Conference on Our World in Concrete and Structures, V. 28, 2009, pp. 297-304.

14. Sakurada, R.; Singh, A. K.; Uzawa, M.; and Kawazoe, Y., “First Principles Study on Crystal Structure of Beta-Form Belite,” The 4th Asian Particle Technology Symposium, 2009, pp. 691-696.

15. Uchikawa, H., “9th International Congress on the Chemistry of Cement/Special Lecture,” Cement & Concrete, No. 566, 1993, pp. 49-59.

16. Teoreanu, I., and Andronescu, E., “Orthosilicate Composition in CaO-SrO-BaO-SiO2 System and Their Water Reactivity,” 9th International Congress on the Chemistry of Cement, V. 2, 1992, pp. 107-113.

17. Benarchid, M. Y.; Diouri, A.; Boukhari, A.; Aride, J.; and Elkhadiri, I., “Hydration of Iron-Phosphorous Doped Dicalcium Silicate Phase,” Materials Chemistry and Physics, V. 94, No. 2-3, 2005, pp. 190-194. doi: 10.1016/j.matchemphys.2005.04.047

18. Fierens, P., and Tirlocq, J., “Nature and Concentration Effect of Stabilizing Elements of Beta-Dicalcium Silicate on Its Hydration Rate,” Cement and Concrete Research, V. 13, No. 2, 1983, pp. 267-276. doi: 10.1016/0008-8846(83)90110-2

19. Lai, G. C.; Nojiri, T.; and Nakao, K., “Studies of the Stability of β-Ca2SiO4 Doped by Minor Ions,” Cement and Concrete Research, V. 22, No. 5, 1992, pp. 743-754. doi: 10.1016/0008-8846(92)90097-F

20. Kresse, G., and Furthmüller, J., “Efficient Iterative Schemes for Ab initio Total-Energy Calculations Using a Plane-Wave Basis Set,” Physical Review B: Condensed Matter and Materials Physics, V. 54, No. 16, 1996, pp. 11169-11186. doi: 10.1103/PhysRevB.54.11169

21. Brown, I. D., and Altermatt, D., “Bond-Valence Parameters Obtained from a Systematic Analysis of the Inorganic Crystal Structure Database,” Acta Crystallographica, V. 41, No. 4, 1985, pp. 244-247. doi: 10.1107/S0108768185002063

22. Brese, N. E., and O’Keeffe, M., “Bond-Valence Parameters for Solids,” Acta Crystallographica, V. 47, No. 2, 1991, pp. 192-197. doi: 10.1107/S0108768190011041

23. Mori, K.; Kiyanagi, R.; Yoneyama, M.; Iwase, K.; Sato, T.; Itoh, K.; Sugiyama, M.; Kamiyama, T.; and Fukunaga, T., “Charge States of Ca Atoms in β-Dicalcium Silicate,” Journal of Solid State Chemistry, V. 179, No. 11, 2006, pp. 3286-3294. doi: 10.1016/j.jssc.2006.06.018


ALSO AVAILABLE IN:

Electronic Materials Journal