Pressure of Internally Vibrated Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Pressure of Internally Vibrated Concrete

Author(s): Gardner, N.J.

Publication: Concrete International

Volume: 36

Issue: 6

Appears on pages(s): 33--37

Keywords: column, equation, hydrostatic, wall

DOI:

Date: 6/1/2014

Abstract:
Conventional concrete continues to comprise a large percentage of the concrete placed in vertical forms. Placement and consolidation methods thus remain the major determinants for the lateral pressures that will be experienced by the formwork. The author reviews current design equations and proposes an updated equation for calculating the pressures for concrete consolidated by internal vibration.