Photocatalytic Efficiency of Cement-Based Materials: Demonstration of Proposed Test Method

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Photocatalytic Efficiency of Cement-Based Materials: Demonstration of Proposed Test Method

Author(s): Amal R. Jayapalan, Bo Yeon Lee, Eva M. Land, Michael H. Bergin, and Kimberly E. Kurtis

Publication: Materials Journal

Volume: 112

Issue: 2

Appears on pages(s): 219-228

Keywords: characterization; photocatalysis; surface area; titania

DOI: 10.14359/51686985

Date: 3/1/2015

Abstract:
While there is an increasing interest in using photocatalytic cement-based materials, a lack of an appropriate standard procedure for testing the photocatalytic activity and efficiency of such materials makes comparisons among materials and data from different sources challenging. Current standard test methods are not appropriate for assessing photocatalytic nitrogen oxide conversion by cementitious materials because the standards do not consider surface properties of cementitious materials, nor are the test conditions appropriate for evaluation of cementitious materials. Therefore, the main objective is to propose a standard procedure for assessing the photocatalytic activity of cement mixtures with TiO2 additives and to define a parameter—the photocatalytic efficiency factor (PEF)—that could be used to compare the photocatalytic activity of different TiO2 cement mixtures, even for extended exposure conditions. The use of PEF is demonstrated, and values of PEF ranging from 8.40 to 51.55 μmol·h–1·m–2 (0.78 to 4.79 μmol·h–1·ft–2) was observed for mixtures with TiO2 up to 15% replacement.

Related References:

1. Environmental Protection Agency, “Primary National Ambient Air Quality Standards for Nitrogen Dioxide; Final Rule,” Federal Register, V. 75, No. 26, 2010, pp. 6473-6537.

2. Council Directive 1999/30/EC, “Relating to Limit Values for Sulphur Dioxide, Nitrogen Dioxide and Oxides of Nitrogen, Particulate Matter and Lead in Ambient Air,” Official Journal of the European Communities, V. 42, No. L 163, June 29, 1999, pp. 41-60.

3. Law 70 of 1992, “The Law Concerning Special Measures for Total Emission Reduction of Nitrogen Oxides from Automobiles in Specified Areas,” Ministry of the Environment, Government of Japan, Tokyo, Japan, 1992, 8 pp.

4. Carp, O.; Huisman, C. L.; and Reller, A., “Photoinduced Reactivity of Titanium Dioxide,” Progress in Solid State Chemistry, V. 32, No. 1-2, 2004, pp. 33-177.

5. Devahasdin, S.; Fan Jr., C.; Li, K.; and Chen, D. H., “TiO2 Photocatalytic Oxidation of Nitric Oxide: Transient Behavior and Reaction Kinetics,” Journal of Photochemistry and Photobiology A Chemistry, V. 156, No. 1-3, 2003, pp. 161-170.

6. Lackhoff, M.; Prieto, X.; Nestle, N.; Dehn, F.; and Niessner, R., “Photocatalytic Activity of Semiconductor-Modified Cement-Influence of Semiconductor Type and Cement Ageing,” Applied Catalysis B: Environmental, V. 43, No. 3, 2003, pp. 205-216.

7. Linkous, C. A.; Carter, G. J.; Locuson, D. B.; Ouellette, A. J.; Slattery, D. K.; and Smitha, L. A., “Photocatalytic Inhibition of Algae Growth Using TiO2, WO3, and Cocatalyst Modifications,” Environmental Science & Technology, V. 34, No. 22, 2000, pp. 4754-4758.

8. Maggos, T.; Plassais, A.; Bartzis, J. G.; Vasilakos, C.; Moussiopoulos, N.; and Bonafous, L., “Photocatalytic Degradation of NOx in a Pilot Street Canyon Configuration Using TiO2-Mortar Panels,” Environmental Monitoring and Assessment, V. 136, No. 1-3, 2008, pp. 35-44.

9. Allen, N. S.; Edge, M.; Verran, J.; Stratton, J.; Maltby, J.; and Bygott, C., “Photocatalytic Titania Based Surfaces: Environmental Benefits,” Polymer Degradation & Stability, V. 93, No. 9, 2008, pp. 1632-1646.

10. Husken, G.; Hunger, M.; and Brouwers, H. J. H., “Experimental Study of Photocatalytic Concrete Products for Air Purification,” Building and Environment, V. 44, No. 12, 2009, pp. 2463-2474.

11. Erickson, J., “Route 141 Testing Baffles Researchers,” Newsmagazine Network, April 1, 2013, http://www.newsmagazinenetwork.com/2013040132964/route-141-testing-baffles-researchers/.

12. Chen, J., and Poon, C.-S., “Photocatalytic Cementitious Materials: Influence of the Microstructure of Cement Paste on Photocatalytic Pollution Degradation,” Environmental Science & Technology, V. 43, No. 23, 2009, pp. 8948-8952.

13. Kawakami, M.; Furumura, T.; and Tokushige, H., “NOx Removal Effects and Physical Properties of Cement Mortar Incorporating Titanium Dioxide Powder,” International RILEM Symposium of Photocatalysis, Environment and Construction Materials, RILEM Publications S. A. R. L., Florence, Italy, 2007, pp. 163-170.

14. ISO 22197-1, “Fine Ceramics (Advanced Ceramics, Advanced Technical Ceramics)—Test Method for Air-Purification Performance of Semiconducting Photocatalytic Materials—Part 1: Removal of Nitric Oxide,” International Organization for Standardization, Geneva, Switzerland, 2007, 12 pp.

15. JIS R 1701-1, “Fine Ceramics (Advanced Ceramics, Advanced Technical Ceramics)—Test Method for Air Purification Performance of Photocatalytic Materials—Part 1: Removal of Nitric Oxide,” Japanese Standards Association, Tokyo, Japan, 2004, 24 pp.

16. UNI 11247, “Determination of the Degradation of Nitrogen Oxides in the Air by Inorganic Photocatalytic Materials: Continuous Flow Test Method,” Italian Organization of Standardization, Milan, Italy, 2010, 14 pp. (in Italian)

17. Hassan, M. M.; Dylla, H.; Mohammad, L. N.; and Rupnow, T., “Evaluation of the Durability of Titanium Dioxide Photocatalyst Coating for Concrete Pavement,” Construction and Building Materials, V. 24, No. 8, 2010, pp. 1456-1461.

18. Chen, J., and Poon, C.-S., “Photocatalytic Activity of Titanium Dioxide Modified Concrete Materials—Influence of Utilizing Recycled Glass Cullets as Aggregates,” Journal of Environmental Management, V. 90, No. 11, 2009, pp. 3436-3442.

19. Dylla, H.; Hassan, M. M.; Mohammad, L. N.; Rupnow, T.; and Wright, E., “Evaluation of Environmental Effectiveness of Titanium Dioxide Photocatalyst Coating for Concrete Pavement,” Transportation Research Record: Journal of the Transportation Research Board, V. 2164, No. 1, 2010, pp. 46-51.

20. Folli, A., and Macphee, D. E., “Thermodynamic and Kinetic Considerations of the Oxidation of Nitrogen Oxides on Photocatalytic Cementitious Materials,” Nanotechnology in Construction: 4th International Symposium (NICOM4), Crete, Greece, 2012.

21. Giannantonio, D. J.; Kurth, J. C.; Kurtis, K. E.; and Sobecky, P. A., “Effects of Concrete Properties and Nutrients on Fungal Colonization and Fouling,” International Biodeterioration & Biodegradation, V. 63, No. 3, 2009, pp. 252-259.

22. Lee, B. Y.; Jayapalan, A.; Bergin, M.; and Kurtis, K. E., “Photocatalytic Cement Exposed to Nitrogen Oxides: Effect of Oxidation and Binding,” Cement and Concrete Research, V. 60, 2014, pp. 30-36.

23. Folli, A.; Jakobsen, U. H.; Guerrini, G. L.; and Macphee, D. E., “Rhodamine B Discolouration on TiO2 in the Cement Environment: A Look at Fundamental Aspects of the Self-Cleaning Effect in Concretes,” Journal of Advanced Oxidation Technologies, V. 12, No. 1, 2009, pp. 126-133.

24. Ruot, B.; Plassais, A.; Olive, F.; Guillot, L.; and Bonafous, L., “TiO2-Containing Cement Pastes and Mortars: Measurements of the Photocatalytic Efficiency Using a Rhodamine B-Based Colourimetric Test,” Solar Energy, V. 83, No. 10, 2009, pp. 1794-1801.

25. Bianchi, C. L.; Ardizzone, S.; Cappelletti, G.; Pirola, C.; and Ragaini, V., “The Role of the Synthetic Procedure of Nano-Crystalline TiO2 on the Photodegradation of Toluene,” International RILEM Symposium on Photocatalysis, Environment, and Construction Materials—TDP 2007, RILEM Publications, Florence, Italy, 2007, pp. 17-24.

26. Maggos, T.; Bartzis, J. G.; Leva, P.; and Kotzias, D., “Application of Photocatalytic Technology for NOx Removal,” Applied Physics. A, Materials Science & Processing, V. 89, No. 1, 2007, pp. 81-84.

27. Linsebigler, A. L.; Lu, G. Q.; and Yates, J. T., “Photocatalysis on TiO2 Surfaces: Principles, Mechanisms, and Selected Results,” Chemical Reviews, V. 95, No. 3, 1995, pp. 735-758.

28. Bacsa, R. R., and Kiwi, J., “Effect of Rutile Phase on the Photocatalytic Properties of Nanocrystalline Titania during the Degradation of P-Coumaric Acid,” Applied Catalysis B: Environmental, V. 16, No. 1, 1998, pp. 19-29.

29. ASTM C305, “Standard Practice for Mechanical Mixing of Hydraulic Cement Pastes and Mortars of Plastic Consistency,” ASTM International, West Conshohocken, PA, 3 pp.

30. Jayapalan, A. R.; Lee, B. Y.; and Kurtis, K. E., “Can Nanotechnology Be ‘Green’? Comparing Efficacy of Nano and Microparticles in Cementitious Materials,” Cement and Concrete Composites, V. 36, 2013, pp. 16-24.

31. Kurtis, K. E.; El-Ashkar, N. H.; Collins, C. L.; and Naik, N. N., “Examining Cement-Based Materials by Laser Scanning Confocal Microscopy,” Cement and Concrete Composites, V. 25, No. 7, 2003, pp. 695-701.

32. Lee, B. Y., “Effect of Titanium Dioxide Nanoparticles on Early Age and Long Term Properties of Cementitious Materials,” PhD dissertation, Georgia Institute of Technology, Atlanta, GA, 2012, 227 pp.

33. Diamanti, M. V.; Ormellese, M.; and Pedeferri, M., “Characterization of Photocatalytic and Superhydrophilic Properties of Mortars Containing Titanium Dioxide,” Cement and Concrete Research, V. 38, No. 11, 2008, pp. 1349-1353.

34. Jayapalan, A. R., “Properties of Cement-Based Materials in the Presence of Nano and Microparticle Additives,” PhD dissertation, Georgia Institute of Technology, Atlanta, GA, 2013, 232 pp.

35. Hurum, D. C.; Agrios, A. G.; and Gray, K. A., “Explaining the Enhanced Photocatalytic Activity of Degussa P25 Mixed-Phase TiO2 Using EPR,” The Journal of Physical Chemistry B, V. 107, No. 19, 2003, pp. 4545-4549.


ALSO AVAILABLE IN:

Electronic Materials Journal