523.3R-14: Guide for Cellular Concretes above 50 lb/ft3 (800 kg/m3)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 523.3R-14: Guide for Cellular Concretes above 50 lb/ft3 (800 kg/m3)

Author(s): ACI Committee 523

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 17

Keywords: cellular concrete; compressive strength; fire resistance; insu-lating concrete; lightweight concrete; mixture proportioning; modulus of elasticity; precast concrete; recyclability; shear properties; splitting tensile strength; structural design.

DOI:

Date: 4/1/2014

Abstract:
This guide addresses the materials, properties, design, production, and placement of cellular concretes with as-cast densities greater than 50 lb/ft3 (800 kg/m3). The usual density range of cellular concrete is 20 to 120 lb/ft3 (320 to 1920 kg/m3). Cellular concretes in the lower portion of this range are used for many applications, such as roof thermal insulation and geotechnical fills. Cellular concretes in the higher density range are used for cast-in-place, precast applications and nonstructural floor fills.