Characterization of Coal Fly Ash by the Absolute Foam Index

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Characterization of Coal Fly Ash by the Absolute Foam Index

Author(s): Melanie Kueber Watkins, Zeyad Ahmed, Lawrence Sutter, and David Hand

Publication: Materials Journal

Volume: 112

Issue: 3

Appears on pages(s): 393-398

Keywords: adsorption; air-entraining admixture; fly ash; foam index; slurry; supplementary cementitious material

DOI: 10.14359/51686792

Date: 5/1/2015

Abstract:
Long foam index test times and the inability to characterize different loss on ignition (LOI) in cementitious materials using the same solution concentrations prompted an examination of different test solution concentrations for various fly ash samples. A 15-minute duration forced the test into a number of cycles where air-entraining admixture (AEA) drops with sensitivity compatible to the fly ash allowed diffusion and reaction consistency throughout all the tests, allowing both low- and high-carbon fly ash to be characterized uniquely. The absolute foam index, defined as the amount of undiluted volume of AEA solution added to obtain a 15-minute endpoint (limits 12 to 18 minutes) signified by 15-second metastable foam, uniquely characterized 15 fly ash samples with LOI values that ranged from 0.17 to 23.3%. The absolute foam index strongly correlated to LOI values for fly ash samples greater than 5% LOI but variability was observed in samples less than 5% LOI.

Related References:

1. Harris, N. J.; Hover, K. C.; Folliard, K. J.; and Ley, M. T., “The Use of the Foam Index Test to Predict AEA Dosage in Concrete Containing Fly Ash: Part II—Development of a Standard Test Method: Apparatus and Procedure,” Journal of ASTM International, V. 5, No. 7, 2008, pp. 1-15.

2. Külaots, I.; Hsu, A.; Hurt, R. H.; and Suuberg, E. M., “Adsorption of Surfactants on Unburned Carbon in Fly Ash and Development of a Standardized Foam Index Test,” Cement and Concrete Research, V. 33, No. 12, 2003, pp. 2091-2099. doi: 10.1016/S0008-8846(03)00232-1

3. Baltrus, J. P., and LaCount, R. B., “Measurements of Adsorption of Air-Entraining Admixture on Fly Ash in Concrete and Cement,” Cement and Concrete Research, V. 31, No. 5, 2001, pp. 819-824. doi: 10.1016/S0008-8846(01)00494-X

4. Dodson, V. H., Concrete Admixtures, Van Nostrand Rienhold, New York, 1990, 208 pp.

5. Dodson, V.; LaCount, R. B.; and Kern, D. G., “Economical Treatment of High Carbon Fly Ash to Produce a Low Foam Index Product with Carbon Content Retained,” Waynesburg College, Waynesburg, PA, 2005, 28 pp.

6. American Coal Ash Association, “Fly Ash Facts for Engineers,” Report No. FHWA-IF-03-019, Federal Highway Administration, Washington, DC, 2003, 81 pp.

7. Taylor, P. C.; Johansen, V. C.; Graf, L. A.; Kozikowski, R. L.; Zemajtis, J. Z.; and Ferraris, C. F., “Identifying Incompatible Combinations of Concrete Materials: Volume II—Test Protocol,” Report No. FHWA-HRT-06-080, Federal Highway Administration, Washington, DC, 2006, 86 pp.

8. Freeman, E.; Gao, Y. M.; Hurt, R. H.; and Suuberg, E. M., “Interactions of Carbon-containing Fly Ash with Commercial Air-entraining Admixtures for Concrete,” Fuel, V. 76, No. 8, 1997, pp. 761-765. doi: 10.1016/S0016-2361(96)00193-7

9. Gebler, S., and Klieger, P., “Effect of Fly Ash on the Air-Void Stability of Concrete,” Fly Ash, Silica Fume, Slag and Other Mineral By-Products in Concrete, SP-79, American Concrete Institute, Farmington Hills, MI, 1983, pp. 103-142.

10. Grace Construction Products, “The Foam Index Test: A Rapid Indicator of Relative AEA Demand,” Technical Bulletin TB-0202, Columbia, MD, 2006, 2 pp.

11. Gurupira, T. Z.; Ochsenbein, M. P.; Stencel, J. M.; and Martinus, F., “Development of an Automated Foam Index Test,” 2005 World of Coal Ash Conference Proceedings, Lexington, KY, April 11-15, 2005, 5 pp.

12. Külaots, I.; Hurt, R. H.; and Suuberg, E. M., “Size Distribution of Unburned Carbon in Coal Fly Ash and its Implications,” Fuel, V. 83, No. 2, 2004, pp. 223-230. doi: 10.1016/S0016-2361(03)00255-2

13. Meininger, R. C., “Use of Fly Ash in Concrete—Report of Recent NSGA—NRMCA Research Laboratory Studies—Series J 153,” Technical Information Letter No. 381, National Ready Mixed Concrete Association, Silver Spring, MD, 1981.

14. Stencel, J. M.; Song, H.; and Cangialosi, F., “Automated Foam Index Test: Quantifying Air Entraining Agent Addition and Interactions with Fly Ash-Cement Admixtures,” Cement and Concrete Research, V. 39, No. 4, 2009, pp. 362-370. doi: 10.1016/j.cemconres.2009.01.010

15. Sutter, L.; Hooton, R. D.; and Schlorholtz, S., “Methods for Evaluating Fly Ash for Use in Highway Concrete,” NCHRP Report 749, National Cooperative Highway Research Program, Transportation Research Board, Washington, DC, 2013, 91 pp.

16. Kueber Watkins, M., “Characterization of a Coal Fly Ash-Cement Slurry by the Absolute Foam Index,” PhD dissertation, Michigan Technological University, Houghton, MI, 2013, 108 pp.

17. ASTM C311-11a, “Standard Test Methods for Sampling and Testing Fly Ash or Natural Pozzolans for Use in Portland-Cement Concrete,” ASTM International, West Conshohocken, PA, 2011, 10 pp.

18. Brown, R. C., and Dykstra, J., “Systematic Errors in the Use of Loss-on-Ignition to Measure Unburned Carbon in Fly Ash,” Fuel, V. 74, No. 4, 1995, pp. 570-574. doi: 10.1016/0016-2361(95)98360-Q

19. Pedersen, K. H.; Jensen, A. D.; Skjøth-Rasmussen, M. S.; and Dam-Johansen, K., “A Review of the Interference of Carbon Containing Fly Ash with Air Entrainment in Concrete,” Progress in Energy and Combustion Science, V. 34, No. 2, 2008, pp. 135-154. doi: 10.1016/j.pecs.2007.03.002


ALSO AVAILABLE IN:

Electronic Materials Journal